CN103551122A - 一种麦草粉改性活性炭吸附剂及其制备方法 - Google Patents

一种麦草粉改性活性炭吸附剂及其制备方法 Download PDF

Info

Publication number
CN103551122A
CN103551122A CN201310440346.9A CN201310440346A CN103551122A CN 103551122 A CN103551122 A CN 103551122A CN 201310440346 A CN201310440346 A CN 201310440346A CN 103551122 A CN103551122 A CN 103551122A
Authority
CN
China
Prior art keywords
parts
active carbon
powder
preparation
wheat straw
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201310440346.9A
Other languages
English (en)
Inventor
孙夕雨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Original Assignee
BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd filed Critical BENGBU DEMO FILTRATION TECHNOLOGY Co Ltd
Priority to CN201310440346.9A priority Critical patent/CN103551122A/zh
Publication of CN103551122A publication Critical patent/CN103551122A/zh
Pending legal-status Critical Current

Abstract

一种麦草粉改性活性炭吸附剂,由下列重量份的原料制成:麦草粉30-40、活性炭100-120、石英粉8-10、竹炭粉10-15、碳酸锂7-9、高岭土7-9、十二烷基二甲基氧化胺1-2、椰油酰二乙醇胺1-2、硅树脂聚醚乳液1-2、聚醚改性硅油1-2、改性硅藻土4-5、水适量。本发明使用麦草粉作为原料生产的活性炭质量轻、孔隙结构发达、比表面积大、吸附速度快、对各种溶质和游离气等有良好的吸附能力;本发明制备活性炭的亚甲蓝吸附值在1~7mg/0.1g;本发明制备活性炭过程中,无酸性废水、废气排放、成本低廉,实现农作物废物利用,减少环境污染,适合空气净化,有效去除甲醛、细菌、本分等有害物质。

Description

一种麦草粉改性活性炭吸附剂及其制备方法
技术领域
本发明涉及一种改性功能材料领域,尤其涉及一种麦草粉改性活性炭吸附剂及其制备方法。
背景技术
随着科技的发展,现代化工业的逐步建设,各种化学品被开发利用,给人们生活带来了便利,同时由于化学品产生了对环境和人体有害的物质,也成了人们不得不面对的问题。
目前空气中的污染物主要是工业燃料燃烧产生的气体、汽车尾气、生产中产生的有毒有害气体。水污染主要是工业生产排放的污水里含有大量有毒物质,还有人们生活中的污水产生很多有害物质。人们生活中也有很多时候需要脱除毒素,比如空调过滤网上有很多细菌、毒素,新装修的间有甲醛等有害物质,都需要脱除毒素。目前都脱除毒素经常用到吸附剂,主要有硅胶、活性氧化铝、活性炭、分子筛等,另外还有针对某种组分选择性吸附而研制的吸附材料。但是这些吸附剂大多吸附能力有限,需要针对不同的要求研究不同的吸附剂,发挥最好的作用。同时,寻找新的原料,以增强吸附效果,节约成本。
发明内容
本发明的目的在于提供一种麦草粉改性活性炭吸附剂及其制备方法。
本发明的技术方案如下:
一种麦草粉改性活性炭吸附剂,其特征在于由下列重量份的原料制成:麦草粉30-40、活性炭100-120、石英粉8-10、竹炭粉10-15、碳酸锂7-9、高岭土7-9、十二烷基二甲基氧化胺1-2、椰油酰二乙醇胺1-2、硅树脂聚醚乳液1-2、聚醚改性硅油1-2、改性硅藻土4-5、水适量;
所述改性硅藻土由下列重量份的原料制成:硅藻土100-110、麦饭石30-34、纳米碳1-2、抗坏血酸1-2、薏仁油1-2、十二烷基苯磺酸钠1-2、葡萄糖酸锌2-3、蒲公英粉2-3;制备方法是将硅藻土、麦饭石放入煅烧炉中在540-560℃下煅烧3-4小时,取出,放入12-15%的盐酸溶液中浸泡4-5小时,过滤取出,用清水反复洗涤,烘干,加入水中,同时,加入纳米碳、抗坏血酸、葡萄糖酸锌,研磨得到浆料,喷雾干燥,将其它剩余成分与干燥粉末混合,研磨分散均匀即得。
所述麦草粉改性活性炭吸附剂的制备方法,其特征在于包括以下步骤:将麦草粉、石英粉、高岭土一起送入炭化炉中,在600-720℃下炭化处理3-4小时,取出,与活性炭、竹炭粉、碳酸锂、十二烷基二甲基氧化胺、椰油酰二乙醇胺、硅树脂聚醚乳液、聚醚改性硅油一起加入适量水中调成泥状,加热至80-90℃,研磨2-3小时得200-300目浆料,用清水洗涤至PH值为中性,烘干;与其他剩余原料混合分散均匀即得。
本发明的有益效果
本发明使用麦草粉作为原料生产的活性炭质量轻、孔隙结构发达、比表面积大、吸附速度快、对各种溶质和游离气等有良好的吸附能力;本发明制备活性炭的亚甲蓝吸附值在1~7mg/0.1g;本发明制备活性炭过程中,无酸性废水、废气排放、成本低廉,实现农作物废物利用,减少环境污染,适合空气净化,有效去除甲醛、细菌、本分等有害物质。
具体实施方式
一种麦草粉改性活性炭吸附剂,其特征在于由下列重量份的原料制成:麦草粉34、活性炭110、石英粉9、竹炭粉14、碳酸锂7、高岭土8、十二烷基二甲基氧化胺1、椰油酰二乙醇胺2、硅树脂聚醚乳液1、聚醚改性硅油1、改性硅藻土4、水适量;
所述改性硅藻土由下列重量份(公斤)的原料制成:硅藻土106、麦饭石33、纳米碳1.4、抗坏血酸1.5、薏仁油1.6、十二烷基苯磺酸钠1.5、葡萄糖酸锌2.5、蒲公英粉2.4;制备方法是将硅藻土、麦饭石放入煅烧炉中在550℃下煅烧3.4小时,取出,放入15%的盐酸溶液中浸泡4小时,过滤取出,用清水反复洗涤,烘干,加入水中,同时,加入纳米碳、抗坏血酸、葡萄糖酸锌,研磨得到浆料,喷雾干燥,将其它剩余成分与干燥粉末混合,研磨分散均匀即得。
所述麦草粉改性活性炭吸附剂的制备方法,其特征在于包括以下步骤:将麦草粉、石英粉、高岭土一起送入炭化炉中,在660℃下炭化处理4小时,取出,与活性炭、竹炭粉、碳酸锂、十二烷基二甲基氧化胺、椰油酰二乙醇胺、硅树脂聚醚乳液、聚醚改性硅油一起加入适量水中调成泥状,加热至90℃,研磨3小时得300目浆料,用清水洗涤至PH值为中性,烘干;与其他剩余原料混合分散均匀即得。
经测定,其碘值1581mg/g,亚甲基蓝吸附值26.2mL/0.1g。

Claims (2)

1.一种麦草粉改性活性炭吸附剂,其特征在于由下列重量份的原料制成:麦草粉30-40、活性炭100-120、石英粉8-10、竹炭粉10-15、碳酸锂7-9、高岭土7-9、十二烷基二甲基氧化胺1-2、椰油酰二乙醇胺1-2、硅树脂聚醚乳液1-2、聚醚改性硅油1-2、改性硅藻土4-5、水适量;
所述改性硅藻土由下列重量份的原料制成:硅藻土100-110、麦饭石30-34、纳米碳1-2、抗坏血酸1-2、薏仁油1-2、十二烷基苯磺酸钠1-2、葡萄糖酸锌2-3、蒲公英粉2-3;制备方法是将硅藻土、麦饭石放入煅烧炉中在540-560℃下煅烧3-4小时,取出,放入12-15%的盐酸溶液中浸泡4-5小时,过滤取出,用清水反复洗涤,烘干,加入水中,同时,加入纳米碳、抗坏血酸、葡萄糖酸锌,研磨得到浆料,喷雾干燥,将其它剩余成分与干燥粉末混合,研磨分散均匀即得。
2.根据权利要求1所述麦草粉改性活性炭吸附剂的制备方法,其特征在于包括以下步骤:将麦草粉、石英粉、高岭土一起送入炭化炉中,在600-720℃下炭化处理3-4小时,取出,与活性炭、竹炭粉、碳酸锂、十二烷基二甲基氧化胺、椰油酰二乙醇胺、硅树脂聚醚乳液、聚醚改性硅油一起加入适量水中调成泥状,加热至80-90℃,研磨2-3小时得200-300目浆料,用清水洗涤至PH值为中性,烘干;与其他剩余原料混合分散均匀即得。
CN201310440346.9A 2013-09-25 2013-09-25 一种麦草粉改性活性炭吸附剂及其制备方法 Pending CN103551122A (zh)