CN103495370B - 一种永固红2bp微胶囊的制备方法 - Google Patents

一种永固红2bp微胶囊的制备方法 Download PDF

Info

Publication number
CN103495370B
CN103495370B CN201310411008.2A CN201310411008A CN103495370B CN 103495370 B CN103495370 B CN 103495370B CN 201310411008 A CN201310411008 A CN 201310411008A CN 103495370 B CN103495370 B CN 103495370B
Authority
CN
China
Prior art keywords
permanent bordeaux
preparation
parts
weight
microcapsule
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201310411008.2A
Other languages
English (en)
Other versions
CN103495370A (zh
Inventor
党斌
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU XUANDE TEXTILE SCIENCE & TECHNOLOGY CO., LTD.
Original Assignee
Suzhou Chen Hao Textile Technology Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Suzhou Chen Hao Textile Technology Co Ltd filed Critical Suzhou Chen Hao Textile Technology Co Ltd
Priority to CN201310411008.2A priority Critical patent/CN103495370B/zh
Publication of CN103495370A publication Critical patent/CN103495370A/zh
Application granted granted Critical
Publication of CN103495370B publication Critical patent/CN103495370B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种永固红2BP微胶囊的制备方法,制备方法包括以下步骤:(1)将永固红2BP使用球磨机粉碎至目数为350目~400目;(2)取350目~400目的永固红2BP为8~11份,放入反应容器中,温度调节为35℃;(3)向容器中加入丙酮为70~80份,搅拌均匀;(4)向容器中缓慢加入聚氨酯为21~24份,聚乙烯醇为16~19份,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。本发明的制备方法方便简单,制备得到的永固红2BP微胶囊扩大了永固红2BP的应用范围,同时也增强了其稳定性。

Description

一种永固红2BP微胶囊的制备方法
技术领域
本发明涉及一种微胶囊的制备方法,特别是涉及一种永固红2BP微胶囊的制备方法。
背景技术
微胶囊技术在很多行业应用非常广泛,芯材通过使用壁材进行包裹后,可以增强芯材的稳定性,由于彼此多选用高分子材料等物质,可以进一步的拓展芯材的应用空间。在颜料领域,微胶囊技术应用较少,通过将一些应用范围较窄的颜料进行微胶囊化,制备得到的微胶囊体适应性较强,可以适用于多个分散体系中,此外,还可以增强颜料微胶囊的贮藏稳定性。
发明内容
要解决的技术问题:永固红2BP不溶于水的问题。
技术方案:本发明公开了一种永固红2BP微胶囊的制备方法,制备方法包括以下步骤:(1)将永固红2BP使用球磨机粉碎至目数为350目~400目;(2)取350目~400目的永固红2BP为8~11份,放入反应容器中,温度调节为35℃;(3)向容器中加入丙酮为70~80份,搅拌均匀;(4)向容器中缓慢加入聚氨酯为21~24份,聚乙烯醇为16~19份,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。优选将永固红2BP使用球磨机粉碎至目数为400目。永固红2BP优选为11份丙酮优选为80份。聚乙烯醇优选为19份。
有益效果:本发明的制备方法方便简单,制备得到的永固红2BP微胶囊扩大了永固红2BP的应用范围,同时制备得到的微胶囊在常温下放置1年后,性状没有发生变化。
具体实施方式
实施例1
(1)将永固红2BP使用球磨机粉碎至目数为400目;(2)取400目的永固红2BP为11kg,放入反应容器中,温度调节为35℃;(3)向容器中加入丙酮为80kg,搅拌均匀;(4)向容器中缓慢加入聚氨酯为21kg,聚乙烯醇为16kg,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。
实施例2
(1)将永固红2BP使用球磨机粉碎至目数为350目;(2)取350目的永固红2BP为10kg,放入反应容器中,温度调节为35℃;(3)向容器中加入丙酮为70kg,搅拌均匀;(4)向容器中缓慢加入聚氨酯为23kg,聚乙烯醇为17kg,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。
实施例3
(1)将永固红2BP使用球磨机粉碎至目数为400目;(2)取400目的永固红2BP为8kg,放入反应容器中,温度调节为35℃;(3)向容器中加入丙酮为75kg,搅拌均匀;(4)向容器中缓慢加入聚氨酯为24kg,聚乙烯醇为19kg,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。
将实施例1、实施例2、实施例3的产品投入水中,具有良好的分散性,拓展了永固红2BP的应用范围,同时实施例1、实施例2、实施例3的产品在常温下放置一年后没有发生变化,具有良好的稳定性。

Claims (5)

1.一种永固红2BP微胶囊的制备方法,其特征在于制备方法包括以下步骤:(1)将永固红2BP使用球磨机粉碎至目数为350目~400目;(2)按重量取350目~400目的永固红2BP为8~11份,放入反应容器中,温度调节为35℃;(3)按重量向容器中加入丙酮为70~80份,搅拌均匀;(4)按重量向容器中缓慢加入聚氨酯为21~24份,聚乙烯醇为16~19份,加入的同时进行搅拌;(5)搅拌均匀后温度调节为60℃,待丙酮挥发干后得到永固红2BP微胶囊。
2.根据权利要求1所述的一种永固红2BP微胶囊的制备方法,其特征在于将永固红2BP使用球磨机粉碎至目数为400目。
3.根据权利要求1所述的一种永固红2BP微胶囊的制备方法,其特征在于永固红2BP为11重量份
4.根据权利要求1所述的一种永固红2BP微胶囊的制备方法,其特征在于丙酮为80重量份。
5.根据权利要求1所述的一种永固红2BP微胶囊的制备方法,其特征在于聚乙烯醇为19重量份。
CN201310411008.2A 2013-09-11 2013-09-11 一种永固红2bp微胶囊的制备方法 Expired - Fee Related CN103495370B (zh)