一种挤塑泡沫保温板及其制备方法 Download PDFInfo
- Publication number
- CN103450558A CN103450558A CN2013102973720A CN201310297372A CN103450558A CN 103450558 A CN103450558 A CN 103450558A CN 2013102973720 A CN2013102973720 A CN 2013102973720A CN 201310297372 A CN201310297372 A CN 201310297372A CN 103450558 A CN103450558 A CN 103450558A
- Authority
- CN
- China
- Prior art keywords
- parts
- powder
- loess
- used oil
- preparation
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
一种挤塑泡沫保温板及其制备方法,其特征在于由下列重量份的原料制成:聚丙烯腈20-30、等规聚丙烯100-120、纳米砖渣粉末50-60、秸秆粉末20-23、粉煤灰10-15、废机油2-3、改性黄土粉12-14、烯基丁二酸酯1-2、二烷基二硫代磷酸锌1-2、铝粉0.2-0.3、十二烷基苯磺酸钠2-3、氟利昂3-4。本发明具有强度高,质量轻,导热系数低的特点,且成本低,配制简单,施工方便,能代替聚苯乙烯泡沫板、挤塑板和保温体系浆料颗粒保温板等,适于工业化批量生产。
Description
技术领域
本发明涉及一种墙板,更具体地说,是一种挤塑泡沫保温板及其制备方法。
背景技术
房屋建筑,特别是高寒地区的房屋建筑,建筑屋中的大量热量是通过屋顶和墙体散失的。因此,需要在屋顶和外墙铺砌保温板,起到保温隔热和节约能源的作用。现有的挤塑保温板,具有强度低、抗压低、密度低、抗老化性弱、成本高的缺点,需要有新的产品面世,参与竞争。
发明内容
本发明的目的是提供一种挤塑泡沫保温板及其制备方法。
本发明所采用的技术方案是:
一种挤塑泡沫保温板,其特征在于由下列重量份的原料制成:
聚丙烯腈20-30、等规聚丙烯100-120、纳米砖渣粉末50-60、秸秆粉末20-23、粉煤灰10-15、废机油2-3、改性黄土粉12-14、烯基丁二酸酯1-2、二烷基二硫代磷酸锌1-2、铝粉0.2-0.3、十二烷基苯磺酸钠2-3、氟利昂3-4。
所述的改性黄土粉由以下重量份的原料制得:黄土100-120、草木灰30-40、废机油10-12、淀粉10-12、十二烷基苯磺酸钠1-2、铝粉0.2-0.3、水适量;
制备方法是:将黄土在460-480℃下煅烧2-3小时,研成粉末;将淀粉、十二烷基苯磺酸钠加入到适量水中,加热成糊状;向糊中加入所述的煅烧黄土粉、草木灰、铝粉、废机油,混合搅拌40-50分钟,送入60-70℃烘房中烘干,打碎成粗颗粒,筛出1-3mm的粗颗粒即可。
所述的挤塑泡沫保温板的制备方法,其特征在于包括以下步骤:
(1)将纳米砖渣粉末、秸秆粉末、粉煤灰、废机油、改性黄土粉、烯基丁二酸酯、二烷基二硫代磷酸锌、铝粉、十二烷基苯磺酸钠混合,搅拌均匀;
(2)然后将聚丙烯腈、等规聚丙烯加热至150-175℃后,与步骤(1)物料混合,使各物料熔融和混合,形成聚合物熔体;然后加入氟利昂搅拌混合;将熔体降温至100-135℃,然后,送入挤塑机,挤出成型。
本发明具有强度高,质量轻,导热系数低的特点,原料为工矿废料和价廉材料,成本低,配制简单,施工方便,能代替聚苯乙烯泡沫板、挤塑板和保温体系浆料颗粒保温板等,适于工业化批量生产。
具体实施方式
一种挤塑泡沫保温板,由下列重量份(公斤)的原料制成:
聚丙烯腈20、等规聚丙烯120、纳米砖渣粉末60、秸秆粉末23、粉煤灰10、废机油2、改性黄土粉14、烯基丁二酸酯2、二烷基二硫代磷酸锌2、铝粉0.2、十二烷基苯磺酸钠2、氟利昂4。
所述的改性黄土粉由以下重量份(公斤)的原料制得:黄土120、草木灰30、废机油10、淀粉12、十二烷基苯磺酸钠2、铝粉0.3、水适量;
制备方法是:将黄土在460-480℃下煅烧2-3小时,研成粉末;将淀粉、十二烷基苯磺酸钠加入到适量水中,加热成糊状;向糊中加入所述的煅烧黄土粉、草木灰、铝粉、废机油,混合搅拌40-50分钟,送入60-70℃烘房中烘干,打碎成粗颗粒,筛出1-3mm的粗颗粒即可。
挤塑泡沫保温板的制备方法,包括以下步骤:
(1)将纳米砖渣粉末、秸秆粉末、粉煤灰、废机油、改性黄土粉、烯基丁二酸酯、二烷基二硫代磷酸锌、铝粉、十二烷基苯磺酸钠混合,搅拌均匀;
(2)然后将聚丙烯腈、等规聚丙烯加热至150-175℃后,与步骤(1)物料混合,使各物料熔融和混合,形成聚合物熔体;然后加入氟利昂搅拌混合;将熔体降温至100-135℃,然后,送入挤塑机,挤出成型。
本发明经检测,抗压强度≥ 280kPa,导热系数≤ 0.03W/mk,吸水率≤ 1% (V/V),水气透湿系数≤ 3ng/m.s.Pa。
Claims (2)
1.一种挤塑泡沫保温板,其特征在于由下列重量份的原料制成:
聚丙烯腈20-30、等规聚丙烯100-120、纳米砖渣粉末50-60、秸秆粉末20-23、粉煤灰10-15、废机油2-3、改性黄土粉12-14、烯基丁二酸酯1-2、二烷基二硫代磷酸锌1-2、铝粉0.2-0.3、十二烷基苯磺酸钠2-3、氟利昂3-4;
所述的改性黄土粉由以下重量份的原料制得:黄土100-120、草木灰30-40、废机油10-12、淀粉10-12、十二烷基苯磺酸钠1-2、铝粉0.2-0.3、水适量;
制备方法是:将黄土在460-480℃下煅烧2-3小时,研成粉末;将淀粉、十二烷基苯磺酸钠加入到适量水中,加热成糊状;向糊中加入所述的煅烧黄土粉、草木灰、铝粉、废机油,混合搅拌40-50分钟,送入60-70℃烘房中烘干,打碎成粗颗粒,筛出1-3mm的粗颗粒即可。
2.根据权利要求1所述的挤塑泡沫保温板的制备方法,其特征在于包括以下步骤:
(1)将纳米砖渣粉末、秸秆粉末、粉煤灰、废机油、改性黄土粉、烯基丁二酸酯、二烷基二硫代磷酸锌、铝粉、十二烷基苯磺酸钠混合,搅拌均匀;
(2)然后将聚丙烯腈、等规聚丙烯加热至150-175℃后,与步骤(1)物料混合,使各物料熔融和混合,形成聚合物熔体;然后加入氟利昂搅拌混合;将熔体降温至100-135℃,然后,送入挤塑机,挤出成型。