CN103352551B - 一种立体墙面的涂覆方法 - Google Patents

一种立体墙面的涂覆方法 Download PDF

Info

Publication number
CN103352551B
CN103352551B CN201310292471.XA CN201310292471A CN103352551B CN 103352551 B CN103352551 B CN 103352551B CN 201310292471 A CN201310292471 A CN 201310292471A CN 103352551 B CN103352551 B CN 103352551B
Authority
CN
China
Prior art keywords
putty
fine particle
layer
floor
wall
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310292471.XA
Other languages
English (en)
Other versions
CN103352551A (zh
Inventor
王和山
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Anhui Kailin New Material Co Ltd
Original Assignee
Anhui Kailin New Material Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Anhui Kailin New Material Co Ltd filed Critical Anhui Kailin New Material Co Ltd
Priority to CN201310292471.XA priority Critical patent/CN103352551B/zh
Publication of CN103352551A publication Critical patent/CN103352551A/zh
Application granted granted Critical
Publication of CN103352551B publication Critical patent/CN103352551B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种立体墙面的涂覆方法,包括以下步骤:将待涂覆墙面打磨平整;在所述墙面上打第一层腻子;在所述第一层腻子上粘合防裂网;待所述第一层腻子晾干后,在所述防裂网上打第二层腻子;在所述第二层腻子上粘合细小颗粒;待所述第二层腻子晾干后,在第二层腻子和细小颗粒涂覆涂料。本发明中,在用涂料涂覆墙壁之前,在墙壁上粘合细小颗粒,这样涂覆后的墙壁不是光滑的,而是凹凸不平,具有立体感和层次感。

Description

一种立体墙面的涂覆方法
技术领域
本发明涉及墙面涂覆技术领域,尤其涉及一种立体墙面的涂覆方法。
背景技术
墙壁涂料作为室内装修必不可少的材料已被广泛应用,其可以将室内墙壁染成自己喜欢的图案。墙壁涂料的评价标准主要包括耐用、环保等,因此大多数公司的改进方向也是如何提高墙壁涂料的寿命和减少污染,很少有人想到如何进行墙壁的立体涂覆,以增加墙壁的立体感和层次感,亟待改进。
发明内容
针对现有技术存在的问题,本发明的目的在于提出一种立体墙面的涂覆方法,在墙壁上粘合细小颗粒,涂覆后的墙壁具有立体感和层次感。
一种立体墙面的涂覆方法,包括以下步骤:
将待涂覆墙面打磨平整;
在所述墙面上打第一层腻子;
在所述第一层腻子上粘合防裂网;
待所述第一层腻子晾干后,在所述防裂网上打第二层腻子;
在所述第二层腻子上粘合细小颗粒;
待所述第二层腻子晾干后,在第二层腻子和细小颗粒涂覆涂料。
优选地,所述细小颗粒为细小石粒或木屑。
优选地,所述细小颗粒在所述第二层腻子上形成图形或图案。
本发明中,在用涂料涂覆墙壁之前,在墙壁上粘合细小颗粒,这样涂覆后的墙壁不是光滑的,而是凹凸不平,具有立体感和层次感。
说明书附图
图1是本发明提供的一种立体墙面的涂覆方法的流程图。
具体实施方式
如图1所示,图1是本发明提供的一种立体墙面的涂覆方法的流程图。
参照图1,本发明实施例提供了一种立体墙面的涂覆方法,包括以下步骤:
步骤S1,将待涂覆墙面打磨平整;
步骤S2,在所述墙面上打第一层腻子;
步骤S3,在所述第一层腻子上粘合防裂网;
步骤S4,待所述第一层腻子晾干后,在所述防裂网上打第二层腻子;
步骤S5,在所述第二层腻子上粘合细小颗粒;所述细小颗粒可以为细小石粒或木屑,也可以为其他材料。所述细小颗粒在所述第二层腻子上形成图形或图案,也可以不规则分布。
步骤S6,待所述第二层腻子晾干后,在第二层腻子和细小颗粒涂覆涂料。
以上所述,仅为本发明较佳的具体实施方式,但本发明的保护范围并不局限于此,任何熟悉本技术领域的技术人员在本发明揭露的技术范围内,根据本发明的技术方案及其发明构思加以等同替换或改变,都应涵盖在本发明的保护范围之内。

Claims (1)

1.一种立体墙面的涂覆方法,其特征在于,包括以下步骤:
将待涂覆墙面打磨平整;
在所述墙面上打第一层腻子;
在所述第一层腻子上粘合防裂网;
待所述第一层腻子晾干后,在所述防裂网上打第二层腻子;
在所述第二层腻子上粘合细小颗粒;
待所述第二层腻子晾干后,在第二层腻子和细小颗粒涂覆涂料;
所述细小颗粒为细小石粒和/或木屑;
所述细小颗粒在所述第二层腻子上形成图形或图案。
CN201310292471.XA 2013-07-11 2013-07-11 一种立体墙面的涂覆方法 Active CN103352551B (zh)