CN103334459B - A kind of technique for the anti-skidding process of cable trench - Google Patents

A kind of technique for the anti-skidding process of cable trench Download PDF

Info

Publication number
CN103334459B
CN103334459B CN201310303411.3A CN201310303411A CN103334459B CN 103334459 B CN103334459 B CN 103334459B CN 201310303411 A CN201310303411 A CN 201310303411A CN 103334459 B CN103334459 B CN 103334459B
Authority
CN
China
Prior art keywords
cable trench
paint
layer paint
technique
surface layer
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201310303411.3A
Other languages
Chinese (zh)
Other versions
CN103334459A (en
Inventor
王承
朱宇明
徐治
胡嘉骏
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
State Grid Corp of China SGCC
Shanghai Municipal Electric Power Co
Original Assignee
State Grid Corp of China SGCC
Shanghai Municipal Electric Power Co
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by State Grid Corp of China SGCC, Shanghai Municipal Electric Power Co filed Critical State Grid Corp of China SGCC
Priority to CN201310303411.3A priority Critical patent/CN103334459B/en
Publication of CN103334459A publication Critical patent/CN103334459A/en
Application granted granted Critical
Publication of CN103334459B publication Critical patent/CN103334459B/en
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The present invention relates to a kind of technique for the anti-skidding process of cable trench, cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, clear up the fragment dust left over again, be coated with priming paint, intermediate layer paint, surface layer paint more successively, then use quartz sand to carry out ramming process, solidify the anti-skidding process namely completed for 2 hours cable trench.Compared with prior art, the present invention improves the resistance to corrosion of cable trench, and effects on surface carries out the roughness raising that ramming process makes entirety in addition, and then improves security performance.

Description

A kind of technique for the anti-skidding process of cable trench
Technical field
The present invention relates to a kind of cable trench treatment process, especially relate to a kind of technique for the anti-skidding process of cable trench.
Background technology
Reformed and opened up to the outside world since 30 years, the development in Shanghai is maked rapid progress, and the step of urban construction all never slowed down a moment.Originally be positioned at the unlimited well of sidewalk, community or factory, also along with the transformation in the widening of road, old district, progressively become the road surface of slow lane, roadway.In the face of so severe running environment, the unlimited well built according to original design standard wagon flow current under, expose not shockproof defect and not anti-skidding potential safety hazard.Company cable runs the complaint that department all can be subject to several slideways when exercising on unlimited manhole cover plate about non power driven vehicle every year, all can process a collection of unlimited manhole cover plate every year and ring the defect affecting resident and have a rest, and a lot of defect is all cureless repeated defect.In the face of so passive situation, take long-term, stable measure and solution thoroughly, become the task of top priority of unlimited well construction, operation and service work.
Summary of the invention
Object of the present invention be exactly in order to overcome above-mentioned prior art exist defect and the technique for the anti-skidding process of cable trench that a kind of resistance to corrosion is strong, security performance is good is provided.
Object of the present invention can be achieved through the following technical solutions:
For a technique for the anti-skidding process of cable trench, comprise the following steps:
(1) bottom surface polishing: cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, then clearing up the fragment dust left over;
(2) priming paint is coated with: repair flat bottom surface with epoxy mortar, and embedding gap of squeegeeing, then utilize the full width brushing of priming paint, then solidify 1 hour;
(3) be coated with intermediate layer paint: full width brushing intermediate layer paint on priming paint face, then solidify 1 hour;
(4) be coated with surface layer paint: full width brushing surface layer paint on the lacquer painting of middle level, then use quartz sand to carry out ramming process, process Post RDBMS 2 hours, namely complete the anti-skidding process to cable trench.
Described priming paint is commercially available yanfloor3600 priming paint.
Described intermediate layer paint is commercially available yanfloorSL9u intermediate layer paint.
Described surface layer paint is commercially available yanfloorSL39u surface layer paint.
Ramming process adopts sand slinger to spray quartz sand to surface layer paint and forms sand face.
Ramming process adopts hand mode of spreading to shed quartz sand to surface layer paint, and every square metre of quartz sand used is 6kg.
Ramming process employing rotary broom is painted at surface layer and is carried out rolling wire drawing.
Compared with prior art, the present invention brushes different types of coating lacquer three times by dividing cable trench, and control hardening time, priming paint, intermediate layer paint and finish paint are merged mutually and realizes respective function, improve the resistance to corrosion of cable trench, effects on surface carries out the roughness raising that ramming process makes entirety in addition, and then improves security performance.
Detailed description of the invention
Below in conjunction with specific embodiment, the present invention is described in detail.
Embodiment 1
For a technique for the anti-skidding process of cable trench, comprise the following steps:
(1) bottom surface polishing: cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, then clearing up the fragment dust left over;
(2) priming paint is coated with: repair flat bottom surface with epoxy mortar, and embedding gap of squeegeeing, then utilize the full width brushing of commercially available yanfloor3600 priming paint, then solidify 1 hour;
(3) be coated with intermediate layer paint: the yanfloorSL9u intermediate layer paint that full width brushing is commercially available on priming paint face, then solidify 1 hour;
(4) surface layer paint is coated with: the yanfloorSL39u surface layer paint that full width brushing is commercially available on the lacquer painting of middle level, then quartz sand is used to carry out ramming process, mechanical ramming process is adopted in the present embodiment, utilize sand slinger to spray quartz sand to surface layer paint and form sand face, process Post RDBMS 2 hours, namely complete the anti-skidding process to cable trench.
Embodiment 2
For a technique for the anti-skidding process of cable trench, comprise the following steps:
(1) bottom surface polishing: cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, then clearing up the fragment dust left over;
(2) priming paint is coated with: repair flat bottom surface with epoxy mortar, and embedding gap of squeegeeing, then utilize the full width brushing of commercially available yanfloor3600 priming paint, then solidify 1 hour;
(3) be coated with intermediate layer paint: the yanfloorSL9u intermediate layer paint that full width brushing is commercially available on priming paint face, then solidify 1 hour;
(4) surface layer paint is coated with: the yanfloorSL39u surface layer paint that full width brushing is commercially available on the lacquer painting of middle level, then quartz sand is used to carry out ramming process, hand mode of spreading is adopted to shed quartz sand to surface layer paint in the present embodiment, every square metre of quartz sand used is 6kg, process Post RDBMS 2 hours, namely complete the anti-skidding process to cable trench.
Embodiment 3
For a technique for the anti-skidding process of cable trench, comprise the following steps:
(1) bottom surface polishing: cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, then clearing up the fragment dust left over;
(2) priming paint is coated with; Flat bottom surface is repaiied with epoxy mortar, and embedding gap of squeegeeing, then utilize the full width brushing of commercially available yanfloor3600 priming paint, then solidify 1 hour;
(3) be coated with intermediate layer paint: the yanfloorSL9u intermediate layer paint that full width brushing is commercially available on priming paint face, then solidify 1 hour;
(4) surface layer paint is coated with: the yanfloorSL39u surface layer paint that full width brushing is commercially available on the lacquer painting of middle level, then quartz sand is used to carry out ramming process, adopt rotary broom to paint at surface layer in the present embodiment and carry out rolling wire drawing, process Post RDBMS 2 hours, namely complete the anti-skidding process to cable trench.

Claims (4)

1. for a technique for the anti-skidding process of cable trench, it is characterized in that, this technique comprises the following steps:
(1) bottom surface polishing: cable trench exposed metal portions is polished, worn rust staining also significantly improves Metal Surface Roughness, brush the metal powder grain of remained on surface again, concrete surface is exposed to cable trench, knock the dirt on its surface of removal and significantly improve surface roughness, then clearing up the fragment dust left over;
(2) priming paint is coated with: repair flat bottom surface with epoxy mortar, and embedding gap of squeegeeing, then utilize the full width brushing of priming paint, then solidify 1 hour;
(3) be coated with intermediate layer paint: full width brushing intermediate layer paint on priming paint face, then solidify 1 hour;
(4) be coated with surface layer paint: full width brushing surface layer paint on the lacquer painting of middle level, then use quartz sand to carry out ramming process, process Post RDBMS 2 hours, namely complete the anti-skidding process to cable trench;
Ramming process adopts sand slinger to spray quartz sand to surface layer paint and forms sand face, or adopts hand mode of spreading to shed quartz sand to surface layer paint, and every square metre of quartz sand used is 6kg, or adopts rotary broom to paint at surface layer to carry out rolling wire drawing.
2. a kind of technique for the anti-skidding process of cable trench according to claim 1, is characterized in that, described priming paint is commercially available yanfloor3600 priming paint.
3. a kind of technique for the anti-skidding process of cable trench according to claim 1, is characterized in that, described intermediate layer paint is commercially available yanfloorSL9u intermediate layer paint.
4. a kind of technique for the anti-skidding process of cable trench according to claim 1, is characterized in that, described surface layer paint is commercially available yanfloorSL39u surface layer paint.
CN201310303411.3A 2013-07-18 2013-07-18 A kind of technique for the anti-skidding process of cable trench Active CN103334459B (en)