CN103334459A - Process for anti-skid treatment of cable trench - Google Patents
Process for anti-skid treatment of cable trench Download PDFInfo
- Publication number
- CN103334459A CN103334459A CN2013103034113A CN201310303411A CN103334459A CN 103334459 A CN103334459 A CN 103334459A CN 2013103034113 A CN2013103034113 A CN 2013103034113A CN 201310303411 A CN201310303411 A CN 201310303411A CN 103334459 A CN103334459 A CN 103334459A
- Authority
- CN
- China
- Prior art keywords
- cable trench
- paint
- technology
- skidding processing
- surface layer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
The invention relates to a process for anti-skid treatment of a cable trench. The process comprises the following steps: polishing an exposed metal part of a cable trench to remove rusty spots and remarkably improve the metal surface roughness; brushing away metal particles left on the surface; knocking to eliminate dirt on the surface of exposed concrete of the cable trench to remarkably improve the surface roughness; cleaning residual fragment dust; sequentially coating priming paint, middle-layer paint and surface-layer paint; achieving slinging treatment with quartz sand; curing 2 hours to complete the anti-skid treatment of the cable trench. Compared with the prior art, the process provided by the invention can improve corrosion resistance of the cable trench, performs slinging treatment on the surface to improve the integral roughness and further improves the safety performance.
Description
Technical field
The present invention relates to a kind of cable trench treatment process, especially relate to a kind of technology for the anti-skidding processing of cable trench.
Background technology
Reformed and opened up to the outside world since 30 years, the development in Shanghai is maked rapid progress, and the step of urban construction all never slowed down a moment.Originally be positioned at the unlimited well of sidewalk, residential quarter or factory, also along with the transformation in the widening of road, old district, progressively become the road surface of slow lane, roadway.In the face of like this abominable running environment, the unlimited well of building according to original design standard is down current wagon flow, exposes not shockproof defective and not anti-skidding potential safety hazard.Cable operation department of company all can be subjected to several every year about the complaint of non power driven vehicle slideway when opening wide the enforcement of well lid plate, all can handle a collection of unlimited well lid plate every year and ring the defective that influences resident's rest, and a lot of defective all is cureless repeated defective.In the face of like this passive situation, take long-term, stable measure and solution completely, become the task of top priority of unlimited well construction, operation and service work.
Summary of the invention
Purpose of the present invention is exactly to provide the technology that is used for the anti-skidding processing of cable trench that a kind of resistance to corrosion is strong, security performance is good for the defective that overcomes above-mentioned prior art existence.
Purpose of the present invention can be achieved through the following technical solutions:
A kind of technology for the anti-skidding processing of cable trench may further comprise the steps:
(1) bottom surface polishing: the cable trench exposed metal is partly polished, worn rust staining also obviously improves the metal surface roughness, brush the metal powder grain of remained on surface again, cable trench is exposed the concrete surface, knock and remove its surperficial dirt and obviously improve surface roughness, clear up the fragment dust of leaving over again;
(2) be coated with priming paint: with the whole bottom surface of epoxy mortar equating, and the embedding crack of squeegeeing, utilize the full width of cloth brushing of priming paint then, solidified again 1 hour;
(3) be coated with intermediate layer paint:, solidified again 1 hour in the full width of cloth brushing intermediate layer paint of priming paint face;
(4) be coated with the surface layer lacquer: at the full width of cloth brushing surface layer lacquer of middle level lacquer painting, use quartz sand to carry out ramming then and handle, handle the back and solidified 2 hours, namely finish the anti-skidding processing to cable trench.
Described priming paint is commercially available yanfloor3600 priming paint.
Described intermediate layer paint is commercially available yanfloorSL9u intermediate layer paint.
Described surface layer lacquer is commercially available yanfloorSL39u surface layer lacquer.
Ramming is handled and is adopted sand slinger that the surface layer lacquer is sprayed quartz sand formation sand face.
Ramming is handled and is adopted the hand mode of spreading that the surface layer lacquer is shed quartz sand, and every square metre of quartz sand that uses is 6kg.
Ramming is handled and is adopted rotary broom to paint the wire drawing of rolling at surface layer.
Compared with prior art, the present invention brushes different types of coating lacquer three times by cable trench is divided, and control hardening time, make priming paint, intermediate layer paint and finish paint merge mutually and realize separately function, improve the resistance to corrosion of cable trench, in addition ramming is carried out on the surface and handle feasible whole roughness raising, and then improved security performance.
The specific embodiment
The present invention is described in detail below in conjunction with specific embodiment.
Embodiment 1
A kind of technology for the anti-skidding processing of cable trench may further comprise the steps:
(1) bottom surface polishing: the cable trench exposed metal is partly polished, worn rust staining also obviously improves the metal surface roughness, brush the metal powder grain of remained on surface again, cable trench is exposed the concrete surface, knock and remove its surperficial dirt and obviously improve surface roughness, clear up the fragment dust of leaving over again;
(2) be coated with priming paint: with the whole bottom surface of epoxy mortar equating, and the embedding crack of squeegeeing, utilize the full width of cloth brushing of commercially available yanfloor3600 priming paint then, solidified again 1 hour;
(3) be coated with intermediate layer paint:, solidified again 1 hour in the full commercially available yanfloorSL9u intermediate layer paint of width of cloth brushing of priming paint face;
(4) be coated with the surface layer lacquer: at the commercially available yanfloorSL39u surface layer lacquer of the full width of cloth brushing of middle level lacquer painting, using quartz sand to carry out ramming then handles, adopt mechanical ramming to handle in the present embodiment, utilize sand slinger that the surface layer lacquer is sprayed quartz sand and form the sand face, handle the back and solidified 2 hours, namely finish the anti-skidding processing to cable trench.
Embodiment 2
A kind of technology for the anti-skidding processing of cable trench may further comprise the steps:
(1) bottom surface polishing: the cable trench exposed metal is partly polished, worn rust staining also obviously improves the metal surface roughness, brush the metal powder grain of remained on surface again, cable trench is exposed the concrete surface, knock and remove its surperficial dirt and obviously improve surface roughness, clear up the fragment dust of leaving over again;
(2) be coated with priming paint: with the whole bottom surface of epoxy mortar equating, and the embedding crack of squeegeeing, utilize the full width of cloth brushing of commercially available yanfloor3600 priming paint then, solidified again 1 hour;
(3) be coated with intermediate layer paint:, solidified again 1 hour in the full commercially available yanfloorSL9u intermediate layer paint of width of cloth brushing of priming paint face;
(4) be coated with the surface layer lacquer: at the commercially available yanfloorSL39u surface layer lacquer of the full width of cloth brushing of middle level lacquer painting, using quartz sand to carry out ramming then handles, adopt the hand mode of spreading that the surface layer lacquer is shed quartz sand in the present embodiment, every square metre of quartz sand that uses is 6kg, handle the back and solidified 2 hours, namely finish the anti-skidding processing to cable trench.
Embodiment 3
A kind of technology for the anti-skidding processing of cable trench may further comprise the steps:
(1) bottom surface polishing: the cable trench exposed metal is partly polished, worn rust staining also obviously improves the metal surface roughness, brush the metal powder grain of remained on surface again, cable trench is exposed the concrete surface, knock and remove its surperficial dirt and obviously improve surface roughness, clear up the fragment dust of leaving over again;
(2) be coated with priming paint; With the whole bottom surface of epoxy mortar equating, and the embedding crack of squeegeeing, utilize the full width of cloth brushing of commercially available yanfloor3600 priming paint then, solidified again 1 hour;
(3) be coated with intermediate layer paint:, solidified again 1 hour in the full commercially available yanfloorSL9u intermediate layer paint of width of cloth brushing of priming paint face;
(4) be coated with the surface layer lacquer: at the commercially available yanfloorSL39u surface layer lacquer of the full width of cloth brushing of middle level lacquer painting, using quartz sand to carry out ramming then handles, adopt rotary broom to paint the wire drawing of rolling at surface layer in the present embodiment, handle the back and solidified 2 hours, namely finish the anti-skidding processing to cable trench.
Claims (7)
1. technology that is used for the anti-skidding processing of cable trench is characterized in that this technology may further comprise the steps:
(1) bottom surface polishing: the cable trench exposed metal is partly polished, worn rust staining also obviously improves the metal surface roughness, brush the metal powder grain of remained on surface again, cable trench is exposed the concrete surface, knock and remove its surperficial dirt and obviously improve surface roughness, clear up the fragment dust of leaving over again;
(2) be coated with priming paint: with the whole bottom surface of epoxy mortar equating, and the embedding crack of squeegeeing, utilize the full width of cloth brushing of priming paint then, solidified again 1 hour;
(3) be coated with intermediate layer paint:, solidified again 1 hour in the full width of cloth brushing intermediate layer paint of priming paint face;
(4) be coated with the surface layer lacquer: at the full width of cloth brushing surface layer lacquer of middle level lacquer painting, use quartz sand to carry out ramming then and handle, handle the back and solidified 2 hours, namely finish the anti-skidding processing to cable trench.
2. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, described priming paint is commercially available yanfloor3600 priming paint.
3. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, described intermediate layer paint is commercially available yanfloorSL9u intermediate layer paint.
4. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, described surface layer lacquer is commercially available yanfloorSL39u surface layer lacquer.
5. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, ramming is handled and adopted sand slinger that the surface layer lacquer is sprayed quartz sand formation sand face.
6. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, ramming is handled and adopted the hand mode of spreading that the surface layer lacquer is shed quartz sand, and every square metre of quartz sand that uses is 6kg.
7. a kind of technology for the anti-skidding processing of cable trench according to claim 1 is characterized in that, ramming is handled and adopted rotary broom to paint the wire drawing of rolling at surface layer.