CN103305035A - 绿色环保型纳米水性陶瓷硅酸盐无机涂料 - Google Patents
绿色环保型纳米水性陶瓷硅酸盐无机涂料 Download PDFInfo
- Publication number
- CN103305035A CN103305035A CN2013101710747A CN201310171074A CN103305035A CN 103305035 A CN103305035 A CN 103305035A CN 2013101710747 A CN2013101710747 A CN 2013101710747A CN 201310171074 A CN201310171074 A CN 201310171074A CN 103305035 A CN103305035 A CN 103305035A
- Authority
- CN
- China
- Prior art keywords
- parts
- resistance
- water
- filler
- silicate
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,所述绿色环保型纳米水性陶瓷硅酸盐无机涂料是由基料、填料和水组成的,所述基料为硅酸盐纳米陶瓷,其含量为每100份水中含有所述硅酸盐纳米陶瓷65-70份,所述填料的含量为每100份水中含有30-35份,其中,所述填料包括按重量份比组成的下列成分:20-25份钛白粉,25-30份滑石粉,25-30份碳酸钙,20-25份石墨。通过上述方式,本发明的涂料既具有优越的耐高温、耐酸碱、耐油性、耐溶剂性、抗静电、耐污染、防毒性、防水性等,更具备阻燃性、抗辐射性、自修复性、超耐磨性、抗冲击性等特殊性能,且其可直接搅拌均匀后使用,无风险。
Description
技术领域
本发明涉及建筑装饰材料领域,特别是涉及一种绿色环保型纳米水性陶瓷硅酸盐无机涂料。
背景技术
当前,随着国内、外建筑装饰行业、工业船舶、钢铁等行业的发展,涂料市场的需求越来越大,质量要求也越来越高。
但是,现在普遍使用的普通乳胶漆,其属于有机涂料,它的构成成分主要是合成树脂+胶黏剂(含有:甲醛、重金属等)+其他填料,挥发性有机化合物的释放,使其在打开盖子时有刺鼻气味,为了掩盖这一刺鼻气味,需在乳胶漆中添加香料,这就使技术工人在施工时需要佩戴口罩;而且工人在使用时,需要添加稀释剂,稀释剂的比例需要严格控制,其风险高;由于含有胶黏剂,容易粘结灰尘,造成污染。
发明内容
本发明主要解决的技术问题是:针对现有技术的不足,提供一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,既具有优越的耐高温、耐酸碱、耐油性、耐溶剂性、抗静电、耐污染、防毒性、防水性等,更具备阻燃性、抗辐射性、自修复性、超耐磨性、抗冲击性等特殊性能,且其可直接搅拌均匀后使用,无风险。
为解决上述技术问题,本发明采用的一个技术方案是:提供一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,所述绿色环保型纳米水性陶瓷硅酸盐无机涂料是由基料、填料和水组成的,所述基料为硅酸盐纳米陶瓷,其含量为每100份水中含有所述硅酸盐纳米陶瓷65-70份,所述填料的含量为每100份水中含有30-35份,其中,所述填料包括按重量份比组成的下列成分:20-25份钛白粉,25-30份滑石粉,25-30份碳酸钙,20-25份石墨。
在本发明一个较佳实施例中,所述硅酸盐纳米陶瓷的粒径为10-20nm。
在本发明一个较佳实施例中,所述滑石粉的细度为1250-1500目。
在本发明一个较佳实施例中,所述碳酸钙为胶体碳酸钙。
本发明的有益效果是:采用硅酸盐纳米陶瓷最为基料,通过各填料的作用,使其无毒无味,既具有优越的耐高温(600℃)、耐酸碱、耐油性、耐溶剂性、抗静电、耐污染、防毒性、防水性等,更具备阻燃性、抗辐射性、自修复性、超耐磨性、抗冲击性等特殊性能,且其属于水性涂料,使用时无需添加稀释剂,可直接搅拌均匀后使用,无风险。
具体实施方式
下面对本发明的较佳实施例进行详细阐述,以使本发明的优点和特征能更易于被本领域技术人员理解,从而对本发明的保护范围做出更为清楚明确的界定。
本发明实施例包括:
一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,所述绿色环保型纳米水性陶瓷硅酸盐无机涂料是由基料、填料和水组成的,所述基料为硅酸盐纳米陶瓷,其含量为每100份水中含有所述硅酸盐纳米陶瓷65-70份,优选为65份,所述填料的含量为每100份水中含有30-35份,优选为35份,其中,所述填料包括按重量份比组成的下列成分:20-25份钛白粉,25-30份滑石粉,25-30份碳酸钙,20-25份石墨,优选为:20份钛白粉,30份滑石粉,25份碳酸钙,25份石墨。
其中,所述硅酸盐纳米陶瓷的粒径为10-20nm,具有很高的力学性能,包括硬度,断裂韧度和低温延展性等,可耐高温、耐酸碱,且具有自清洁和防雾功能。
所述滑石粉的细度为1250-1500目,具有润滑性、抗黏、助流、耐火性、抗酸性、绝缘性、柔软、光泽好、吸附力强等优良的物理、化学特性。
所述碳酸钙为胶体碳酸钙,是一种具有活性的白色细腻、轻质粉末,其具有补强性。易分解于涂料之中,可使涂料具有一定的抗张强度及光滑细腻的外观。
由此得到的绿色环保型纳米水性陶瓷硅酸盐无机涂料,完全不含有机溶剂,无毒、不含有机挥发物、对人体和环境不会造成影响和危害,是完全具备绿色环保的高性能创新涂料。
本发明揭示了一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,采用硅酸盐纳米陶瓷最为基料,通过各填料的作用,使其无毒无味,既具有优越的耐高温(600℃)、耐酸碱、耐油性、耐溶剂性、抗静电、耐污染、防毒性、防水性等,更具备阻燃性、抗辐射性、自修复性、超耐磨性、抗冲击性等特殊性能,且其属于水性涂料,使用时无需添加稀释剂,可直接搅拌均匀后使用,无风险。
以上所述仅为本发明的实施例,并非因此限制本发明的专利范围,凡是利用本发明说明书内容所作的等效结构或等效流程变换,或直接或间接运用在其他相关的技术领域,均同理包括在本发明的专利保护范围内。
Claims (4)
1.一种绿色环保型纳米水性陶瓷硅酸盐无机涂料,其特征在于,所述绿色环保型纳米水性陶瓷硅酸盐无机涂料是由基料、填料和水组成的,所述基料为硅酸盐纳米陶瓷,其含量为每100份水中含有所述硅酸盐纳米陶瓷65-70份,所述填料的含量为每100份水中含有30-35份,其中,所述填料包括按重量份比组成的下列成分:20-25份钛白粉,25-30份滑石粉,25-30份碳酸钙,20-25份石墨。
2.根据权利要求1所述的绿色环保型纳米水性陶瓷硅酸盐无机涂料,其特征在于,所述硅酸盐纳米陶瓷的粒径为10-20nm。
3.根据权利要求1所述的绿色环保型纳米水性陶瓷硅酸盐无机涂料,其特征在于,所述滑石粉的细度为1250-1500目。
4.根据权利要求1所述的绿色环保型纳米水性陶瓷硅酸盐无机涂料,其特征在于,所述碳酸钙为胶体碳酸钙。