Prior art keywords
flange
red copper
brass
copper spinning
processing technology
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN 201210045203
Other languages
English (en)
Inventor
张道勇
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
JIANGSU YONGLONG ELECTRICAL CO Ltd
Original Assignee
JIANGSU YONGLONG ELECTRICAL CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by JIANGSU YONGLONG ELECTRICAL CO Ltd filed Critical JIANGSU YONGLONG ELECTRICAL CO Ltd
Priority to CN 201210045203 priority Critical patent/CN103292091A/zh
Publication of CN103292091A publication Critical patent/CN103292091A/zh
Pending legal-status Critical Current

Links

Images

Abstract

本发明涉及到一种在高电压环境中应用的电极法兰及其加工工艺。本发明包括通过螺纹连接的紫铜旋压管和黄铜法兰,两者螺纹连接处设有焊接坡口并通过银焊将两者固定;并按以下步骤进行:1)首先在紫铜旋压管和黄铜法兰对应的部位预制对应的螺纹,然后将两者螺纹连接,并在两者连接的上方预留焊接坡口;2)在焊接坡口处通过银焊将紫铜旋压管和黄铜法兰焊接成一体。依据本发明生产出的电极法兰避免了气孔的产生,提高了电极法兰的性能。

Description

一种超高压电极法兰及其加工工艺
技术领域
本发明涉及到一种在高电压环境中应用的电极法兰及其加工工艺,属于一种电气连接件。
背景技术
现有的超高压电极法兰由紫铜旋压管和黄铜法兰直接焊接在一起,在焊接的过程中需要加温进行焊接,其焊接处往往存在气孔,导致电极法兰在使用过程中易发电,影响设备的安全性和操作人员的安全性,需进一步改进。
发明内容
本发明针对上述缺陷,目的在于提供一种避免气孔产生的一种超高压电极法兰及其加工工艺。
为此本发明采用的技术方案是:本发明包括通过螺纹连接的紫铜旋压管和黄铜法兰,两者螺纹连接处设有焊接坡口并通过银焊将两者固定。
本发明所述的紫铜旋压管和黄铜法兰通过锥螺纹连接。
本发明所述两者的螺纹连接处涂钎焊料。
本发明的电极法兰按以下步骤进行:
1)首先在紫铜旋压管和黄铜法兰对应的部位预制对应的螺纹,然后将两者螺纹连接,并在两者连接的上方预留焊接坡口;
2)在焊接坡口处通过银焊将紫铜旋压管和黄铜法兰焊接成一体。
本发明可在1)步骤中,在将紫铜旋压管和黄铜法兰连接之前先在两者的螺纹处涂钎焊料,然后在通过螺纹将两者连接。
本发明所述螺纹连接为锥螺纹连接。
本发明的优点是:1)本发明通过螺纹将紫铜旋压管和黄铜法兰连接进行固定,然后通过银焊将两者固定,本发明利用银焊低熔点、良好润湿性和填满间隙的能力,使焊接处形成无气孔、高强度、良好塑性和良好导电性能的电极法兰;2)本发明在紫铜旋压管和黄铜法兰的螺纹连接处涂钎焊料,进一步避免了气孔的产生;3)本发明进一步的优先采用锥螺纹,这样在银焊前,紫铜旋压管和黄铜法兰两者的定位更加可靠,更有利于银焊的操作,从而进一步保证了电极法兰的焊接质量,提高的电极法兰的性能。
附图说明
图1为传统电极法兰的结构示意图。
图2为本发明的结构示意图。
图3为图2A部的结构示意图。
图4为本发明的另一种结构示意图。
图5为图4B部的结构示意图。
图中1为紫铜旋压管、2为黄铜法兰、3为螺纹、4为焊接坡口、5为锥螺纹。
具体实施方式
本发明包括通过螺纹3连接的紫铜旋压管1和黄铜法兰2,两者螺纹3连接处设有焊接坡口4并通过银焊将两者固定。
本发明所述的紫铜旋压管1和黄铜法兰2通过锥螺纹5连接。
本发明所述两者的螺纹3连接处涂钎焊料。
本发明的电极法兰按以下步骤进行:
1)首先在紫铜旋压管1和黄铜法兰2对应的部位预制对应的螺纹3,然后将两者螺纹3连接,并在两者连接的上方预留焊接坡口4;
2)在焊接坡口4处通过银焊将紫铜旋压管1和黄铜法兰2焊接成一体。
本发明可在1)步骤中,在将紫铜旋压管1和黄铜法兰2连接之前先在两者的螺纹3处涂钎焊料,然后在通过螺纹3将两者连接。
本发明所述螺纹3连接优先的为锥螺纹5连接。

Claims (6)

1.一种超高压电极法兰,其特征在于,包括通过螺纹连接的紫铜旋压管和黄铜法兰,两者螺纹连接处设有焊接坡口并通过银焊将两者固定。
2.根据权利要求1所述的一种超高压电极法兰,其特征在于,所述的紫铜旋压管和黄铜法兰通过锥螺纹连接。
3.根据权利要求1或2所述的一种超高压电极法兰,其特征在于,所述两者的螺纹连接处涂钎焊料。
4.一种超高压电极法兰的加工工艺,其特征在于,按以下步骤进行:
1)首先在紫铜旋压管和黄铜法兰对应的部位预制对应的螺纹,然后将两者螺纹连接,并在两者连接的上方预留焊接坡口;
2)在焊接坡口处通过银焊将紫铜旋压管和黄铜法兰焊接成一体。
5.根据权利要求4所述的一种超高压电极法兰的加工工艺,其特征在于,在1)步骤中,在将紫铜旋压管和黄铜法兰连接之前先在两者的螺纹处涂钎焊料,然后在通过螺纹将两者连接。
6.根据权利要求4或5所述的一种超高压电极法兰的加工工艺,其特征在于,所述螺纹连接为锥螺纹连接。
CN 201210045203 2012-02-27 2012-02-27 一种超高压电极法兰及其加工工艺 Pending CN103292091A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201210045203 CN103292091A (zh) 2012-02-27 2012-02-27 一种超高压电极法兰及其加工工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201210045203 CN103292091A (zh) 2012-02-27 2012-02-27 一种超高压电极法兰及其加工工艺

Publications (1)

Publication Number Publication Date
CN103292091A true CN103292091A (zh) 2013-09-11

Family

ID=49093426

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201210045203 Pending CN103292091A (zh) 2012-02-27 2012-02-27 一种超高压电极法兰及其加工工艺

Country Status (1)

Country Link
CN (1) CN103292091A (zh)

Cited By (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103667050A (zh) * 2013-12-03 2014-03-26 青岛天人环境股份有限公司 一种生物原料高压破壁装置
CN103753021A (zh) * 2014-01-17 2014-04-30 中国科学院半导体研究所 紫铜与黄铜的激光焊接方法
CN107939499A (zh) * 2017-11-22 2018-04-20 浙江邝记汽车零部件有限公司 一种汽车排气管
CN112621017A (zh) * 2020-12-09 2021-04-09 广东澳森热交换系统有限公司 一种黄铜焊料及利用该焊料焊接碳钢与紫铜的纤焊工艺
CN114160931A (zh) * 2021-12-30 2022-03-11 武昌船舶重工集团有限公司 紫铜管与黄铜法兰的焊接方法

Cited By (6)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN103667050A (zh) * 2013-12-03 2014-03-26 青岛天人环境股份有限公司 一种生物原料高压破壁装置
CN103753021A (zh) * 2014-01-17 2014-04-30 中国科学院半导体研究所 紫铜与黄铜的激光焊接方法
CN103753021B (zh) * 2014-01-17 2016-03-30 中国科学院半导体研究所 紫铜与黄铜的激光焊接方法
CN107939499A (zh) * 2017-11-22 2018-04-20 浙江邝记汽车零部件有限公司 一种汽车排气管
CN112621017A (zh) * 2020-12-09 2021-04-09 广东澳森热交换系统有限公司 一种黄铜焊料及利用该焊料焊接碳钢与紫铜的纤焊工艺
CN114160931A (zh) * 2021-12-30 2022-03-11 武昌船舶重工集团有限公司 紫铜管与黄铜法兰的焊接方法

Similar Documents

Publication Publication Date Title
CN103292091A (zh) 一种超高压电极法兰及其加工工艺
CN103033002B (zh) 一种储液器进出气管及其应用
CN204179789U (zh) 一种电机线圈引线与电缆连接件
CN103474857B (zh) 电连接器电缆焊接用固定夹具
CN104841786B (zh) 一种胀管机及其扩口套筒
CN202469299U (zh) 一种超高压电极法兰
CN204167506U (zh) 一种电焊把接线用绝缘套管
CN203147094U (zh) 铜铝管电阻焊接头
CN105478943A (zh) 一种用于电容器引线的焊接工艺
CN202721273U (zh) 一种压接式连接器
CN201663055U (zh) 高强度易焊环保型电容器引线
CN202905959U (zh) 电焊接地夹钳紧固装置
CN106057286A (zh) 高性能导电杆
CN102886613B (zh) 气化炉炉盖上接管的焊接方法
CN203437792U (zh) 气体保护焊机的气体流量监测装置
CN209389277U (zh) 一种高电压测试转接线
CN203670140U (zh) 压缩机
CN204167242U (zh) 一种方形贴装保险丝
CN203202465U (zh) 排气管法兰
CN104551429A (zh) 一种固态电容器专用导针焊接装置及导针焊接的方法
CN206210608U (zh) 一种线圈出头处引线连接结构
CN203690088U (zh) 一种高压互感器用接线端子
CN202405732U (zh) 连接插拔式电缆终端和套管的连接装置
CN201853934U (zh) Co2激光管电极用螺旋式锁紧连接器
CN202028865U (zh) 一种气体保护焊焊枪接头

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130911