CN103275574A - 一种木地板用聚醋酸乙烯耐磨涂料 - Google Patents
一种木地板用聚醋酸乙烯耐磨涂料 Download PDFInfo
- Publication number
- CN103275574A CN103275574A CN2013101966895A CN201310196689A CN103275574A CN 103275574 A CN103275574 A CN 103275574A CN 2013101966895 A CN2013101966895 A CN 2013101966895A CN 201310196689 A CN201310196689 A CN 201310196689A CN 103275574 A CN103275574 A CN 103275574A
- Authority
- CN
- China
- Prior art keywords
- parts
- wear
- resistant paint
- vinyl acetate
- acetate copolymer
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种木地板用聚醋酸乙烯耐磨涂料,它主要是由下列原料按照重量配比搅拌制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠和6-8份尿素。本发明制得的聚醋酸乙烯耐磨涂料可为木地板提供一种具有较高耐磨性、抗冲击、高附着力、坚韧的保护涂层。
Description
技术领域
本发明涉及一种木地板用聚醋酸乙烯耐磨涂料。
技术背景
尽管当今世界已发展生产了多种新型建筑结构材料和装饰材料,但由于木材具有其独特的优良特性,木质饰面给人以一种特殊的优美观感,这是其他装饰材料无法与之相比的。所以,木材在建筑工程尤其是装饰领域中,始终保持着重要的地位。随着建筑业的发展,室内装修业将有更大的发展,而木地板作为室内装修的重要材料之一也将随之发展。而现有的木地板上为了防止受潮变形,所以在其的表面上会涂覆具有防水功能的漆层,但是这类漆层并不耐磨,很容易被刮掉;同时当地板涂层磨损后,其表面光洁度也会变差,影响美观且会缩短地板的使用寿命。所以在其的表面还需要涂覆一层耐磨涂料,用来保护地板上的漆层,避免漆膜破损或剥离。
发明内容
本发明目的是为了克服现有技术的不足,提供一种的木地板用聚醋酸乙烯耐磨涂料。
为解决上述问题,本发明提供的技术方案是:一种木地板用聚醋酸乙烯耐磨涂料,它主要是由下列原料按照重量配比搅拌制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠和6-8份尿素。
还包括10-12份乙二醇丁醚。
还包括4-5份富马酸。
本发明的有益效果:本发明制得的聚醋酸乙烯耐磨涂料可为木地板提供一种具有较高耐磨性、抗冲击、高附着力、坚韧的保护涂层。粘涂工艺简单,一般只需按比例配好涂料,搅拌均匀涂敷于地板表面即可,对施工人员无较高的技术要求,施工方便,对场地要求低。
具体实施方式
实施例1
一种木地板用聚醋酸乙烯耐磨涂料按下列原料按照重量配比通过搅拌机高速分散搅拌均匀制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠和6-8份尿素。
实施例2
一种木地板用聚醋酸乙烯耐磨涂料按下列原料按照重量配比通过搅拌机高速分散搅拌均匀制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠,6-8份尿素和10-12份乙二醇丁醚。
实施例3
一种木地板用聚醋酸乙烯耐磨涂料按下列原料按照重量配比通过搅拌机高速分散搅拌均匀制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠,6-8份尿素,10-12份乙二醇丁醚和4-5份富马酸。
实施例4
本发明制备的产品的主要技术性能如表1:
表1
项目 | 技术指标 |
平均粒度,μm | 76-81 |
吸水量/(g/10mi n) | ≤1.54 |
耐碱性(48h) | 无异常 |
附着力 | 1 级 |
耐水性(96h) | 无异常 |
粘结强度/MPa | 标准状态 |
硬度 | 7H( 莫氏 ) |
粘度 | 3400-3600mPa.s |
表干时间 | 大于 30 分钟 |
耐磨损性 | 0.012 |
Claims (3)
1.一种木地板用聚醋酸乙烯耐磨涂料,其特征在于它主要是由下列原料按照重量配比搅拌制成:50-54份聚醋酸乙烯,10-15份蜜胺,25份异丙醇,10份二乙烯三胺,10-13份石英砂,5-6份醋酸铝,4-10份二氯二苯甲酮,6-8份三聚磷酸钠和6-8份尿素。
2.根据权利要求1所述的一种木地板用聚醋酸乙烯耐磨涂料,其特征在于:还包括10-12份乙二醇丁醚。
3.根据权利要求1或2所述的一种木地板用聚醋酸乙烯耐磨涂料,其特征在于:还包括4-5份富马酸。