CN103275479A - Frp预浸带及其制备工艺 - Google Patents

Frp预浸带及其制备工艺 Download PDF

Info

Publication number
CN103275479A
CN103275479A CN2013102239328A CN201310223932A CN103275479A CN 103275479 A CN103275479 A CN 103275479A CN 2013102239328 A CN2013102239328 A CN 2013102239328A CN 201310223932 A CN201310223932 A CN 201310223932A CN 103275479 A CN103275479 A CN 103275479A
Authority
CN
China
Prior art keywords
curing
yarn
glass fibre
heating
glass fiber
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2013102239328A
Other languages
English (en)
Inventor
陆志强
仇宝鑫
赵荣兵
陆卫强
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Hetai Communication Equipment Co., Ltd.
Sichuan Jiusheng Communications Technology Co., Ltd.
Original Assignee
NANTONG HETAI COMMUNICATION EQUIPMENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG HETAI COMMUNICATION EQUIPMENT CO Ltd filed Critical NANTONG HETAI COMMUNICATION EQUIPMENT CO Ltd
Priority to CN2013102239328A priority Critical patent/CN103275479A/zh
Publication of CN103275479A publication Critical patent/CN103275479A/zh
Pending legal-status Critical Current

Abstract

本发明公开了FRP预浸带,包括以下质量百分含量的原料:玻璃纤维75-85%;水性聚氨酯15-25%。本发明还公开了一种FRP预浸带的制备工艺,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱、导纱后进行浸料步骤,将玻璃纤维浸入水性聚氨酯中,再将浸料好的玻璃纤维进入定型模冷却定型,保持3-5m/min的速度进入加热固化烘箱中进行加热固化,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。本发明优点:将增强材料玻璃纤维和水性聚氨酯结合,使得两者柔韧性和拉伸强度有机结合,具有抗张、耐冲压性好,防潮、防鼠的功能。

Description

FRP预浸带及其制备工艺
技术领域
本发明涉及一种FRP预浸带,属于通信线缆领域。
本发明还涉及一种FRP预浸带的制备工艺。
背景技术
一般情况下,光缆加强芯都是一种圆棒结构,但是有些特殊的光缆,要求加强件能阻水、抗压、防鼠,但是一般的光缆其抗张、抗侧压、抗回缩、耐冲压性能差。因此,需要提供一种新的技术方案来解决上述问题。
发明内容
本发明的目的是提供一种抗张、抗侧压性能强的FRP预浸带。
本发明的另一个目的是提供一种FRP预浸带的制备工艺。
为实现上述目的,本发明采用的技术方案是:
FRP预浸带,包括以下质量百分含量的原料:
玻璃纤维      75-85%;    
水性聚氨酯    15-25%。      
一种FRP预浸带的制备工艺,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱,再用导纱板进行导纱,多股纱线并为一股纱,然后进入浸槽进行浸料,将玻璃纤维浸入水性聚氨酯中,按质量百分含量75-85%的玻璃纤维和质量百分含量的15-25%的水性聚氨酯进行浸料过程,再将浸料好的玻璃纤维进入定型模冷却定型,冷却温度为50-70℃,保持3-5m/min的速度进入加热固化烘箱中进行加热固化,加热温度180-220℃,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。
本发明的优点:将增强材料玻璃纤维和水性聚氨酯结合,使得两者柔韧性和拉伸强度有机结合,连续生产稳定性,具有抗张、抗侧压、高低温性能优异,抗回缩、耐冲压性好,防潮、防鼠的功能。
具体实施方式
以下实施例旨在说明本发明而不是对本方明的进一步限定。
实施例1
FRP预浸带,包括以下原料:
玻璃纤维      75㎏;    
水性聚氨酯    25㎏。      
一种FRP预浸带的制备工艺,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱,再用导纱板进行导纱,多股纱线并为一股纱,然后进入浸槽进行浸料,将玻璃纤维浸入水性聚氨酯中,按75㎏的玻璃纤维和25㎏的水性聚氨酯进行浸料过程,再将浸料好的玻璃纤维进入定型模冷却定型,冷却温度为50℃,保持3m/min的速度进入加热固化烘箱中进行加热固化,加热温度180℃,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。
实施例2
FRP预浸带,包括以下原料:
玻璃纤维      80㎏;    
水性聚氨酯    20㎏。      
一种FRP预浸带的制备工艺,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱,再用导纱板进行导纱,多股纱线并为一股纱,然后进入浸槽进行浸料,将玻璃纤维浸入水性聚氨酯中,按80㎏的玻璃纤维和20㎏的水性聚氨酯进行浸料过程,再将浸料好的玻璃纤维进入定型模冷却定型,冷却温度为60℃,保持4m/min的速度进入加热固化烘箱中进行加热固化,加热温度200℃,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。
实施例3
FRP预浸带,包括以下原料:
玻璃纤维      85㎏;    
水性聚氨酯    15㎏。      
一种FRP预浸带的制备工艺,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱,再用导纱板进行导纱,多股纱线并为一股纱,然后进入浸槽进行浸料,将玻璃纤维浸入水性聚氨酯中,按85㎏的玻璃纤维和15㎏的水性聚氨酯进行浸料过程,再将浸料好的玻璃纤维进入定型模冷却定型,冷却温度为60℃,保持5m/min的速度进入加热固化烘箱中进行加热固化,加热温度220℃,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。
将增强材料玻璃纤维和水性聚氨酯结合,使得两者柔韧性和拉伸强度有机结合,连续生产稳定性,具有抗张、抗侧压、高低温性能优异,抗回缩、耐冲压性好,防潮、防鼠的功能。

Claims (2)

1.FRP预浸带,其特征在于:包括以下质量百分含量的原料:
玻璃纤维      75-85%;    
水性聚氨酯    15-25%。
2.一种如权利要求1所述的FRP预浸带的制备工艺,其特征在于,依次包括放纱、导纱、浸料、定型模、加热固化烘箱、双轮压辊定型和收卷步骤,玻璃纤维经放纱,再用导纱板进行导纱,多股纱线并为一股纱,然后进入浸槽进行浸料,将玻璃纤维浸入水性聚氨酯中,按质量百分含量75-85%的玻璃纤维和质量百分含量的15-25%的水性聚氨酯进行浸料过程,再将浸料好的玻璃纤维进入定型模冷却定型,冷却温度为50-70℃,保持3-5m/min的速度进入加热固化烘箱中进行加热固化,加热温度180-220℃,最后将加热固化后的玻璃纤维进行双轮压辊定型,最后成品收卷。
CN2013102239328A 2013-06-07 2013-06-07 Frp预浸带及其制备工艺 Pending CN103275479A (zh)