CN103230768B - 承压反应釜不锈钢耐蚀层制作工艺 - Google Patents
承压反应釜不锈钢耐蚀层制作工艺 Download PDFInfo
- Publication number
- CN103230768B CN103230768B CN201310145551.2A CN201310145551A CN103230768B CN 103230768 B CN103230768 B CN 103230768B CN 201310145551 A CN201310145551 A CN 201310145551A CN 103230768 B CN103230768 B CN 103230768B
- Authority
- CN
- China
- Prior art keywords
- stainless steel
- kettle
- hole
- pressure
- welding
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Active
Abstract
Description
Claims (4)