CN103173188A - 一种大豆蛋白/微晶纤维素胶粘剂的制备方法 - Google Patents

一种大豆蛋白/微晶纤维素胶粘剂的制备方法 Download PDF

Info

Publication number
CN103173188A
CN103173188A CN2012105404430A CN201210540443A CN103173188A CN 103173188 A CN103173188 A CN 103173188A CN 2012105404430 A CN2012105404430 A CN 2012105404430A CN 201210540443 A CN201210540443 A CN 201210540443A CN 103173188 A CN103173188 A CN 103173188A
Authority
CN
China
Prior art keywords
microcrystalline cellulose
soybean protein
soybean
silane coupling
coupling agent
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012105404430A
Other languages
English (en)
Other versions
CN103173188B (zh
Inventor
白绘宇
丁玥
刘晓亚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Liao Fuhua
Original Assignee
Jiangnan University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Jiangnan University filed Critical Jiangnan University
Priority to CN201210540443.0A priority Critical patent/CN103173188B/zh
Publication of CN103173188A publication Critical patent/CN103173188A/zh
Application granted granted Critical
Publication of CN103173188B publication Critical patent/CN103173188B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种大豆蛋白/微晶纤维素胶粘剂的制备方法。本发明的大豆蛋白/微晶纤维素胶粘剂,包括以下重量份的成分:大豆蛋白100份,水2000~3000份,微晶纤维素0.5~1.5份,硅烷偶联剂0.5~1份。并且由下述方法制得:将大豆蛋白与水混合均匀,然后加入微晶纤维素和硅烷偶联剂进行联合改性后,即得到所述的大豆蛋白/微晶纤维素胶粘剂。本发明所述方法工艺简便,生产成本低,无污染,而且施用方便,粘合性能好,适用于工业化生产。该胶粘剂可用于粘合木材、纸张等纤维材料。并且大豆来源广泛,该胶粘剂具有很好的推广应用价值。

Description

一种大豆蛋白/微晶纤维素胶粘剂的制备方法
技术领域
本发明属于高分子材料与胶粘剂领域,具体涉及一种大豆蛋白/微晶纤维素胶粘剂的制备方法。
背景技术
目前木材胶粘剂中主要是甲醛系胶粘剂,而甲醛系胶粘剂挥发出的甲醛污染环境并且危害健康,长期吸入少量甲醛就会引起慢性中毒。并且许多甲醛系胶粘剂的原料是石化产品,随着石油、煤、天然气等不可再生资源的日趋枯竭严重制约了其发展,人们迫切需要可再生的天然胶粘剂。大豆蛋白作为其中之一,由各种氨基酸经肽键相连而成,具有可生物降解,资源极其丰富,再生速度快,价格便宜等优点,因此人们对大豆蛋白的改性制备大豆蛋白胶粘剂研究也日益增多。微晶纤维素是一种新型的纤维素功能材料,具有较强的刚性、结晶度和力学性能等特点,并且因能提高复合材料的强度和阻湿性能。因此,用微晶纤维素改性大豆蛋白制备大豆蛋白/微晶纤维素胶粘剂,具有较好的粘合性能。
本专利发明了一种大豆蛋白/微晶纤维素胶粘剂的制备方法,包括大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕、豆饼、微晶纤维素、硅烷偶联剂,其特征是,以大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕和豆饼中的任何一种为原料,微晶纤维素和硅烷偶联剂为改性剂,将大豆蛋白原料与水和微晶纤维素及硅烷偶联剂混合,得到大豆蛋白/微晶纤维素胶粘剂。这种胶粘剂在木材,纸张粘结领域具有很好的应用前景。
发明内容
本发明的目的就是为了克服现有技术的不足,提供一种大豆蛋白/微晶纤维素胶粘剂的制备方法,包括大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕、豆饼、微晶纤维素、硅烷偶联剂,其特征是,以大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕和豆饼中的任何一种为原料,微晶纤维素和硅烷偶联剂为改性剂,将大豆蛋白原料与水和微晶纤维素及硅烷偶联剂混合,得到大豆蛋白/微晶纤维素胶粘剂。操作流程简单,制备出的大豆蛋白/微晶纤维素胶粘剂具有较好的粘结强度。
实现本发明目的采用的技术方案是:一种大豆蛋白/微晶纤维素胶粘剂的制备方法,包括以下步骤:先将大豆蛋白和水在85℃水浴中反应1h后,再加入微晶纤维素和硅烷偶联剂在65℃水浴中继续搅拌1h,得到微晶纤维素改性的大豆蛋白胶粘剂。
所述微晶纤维素的用量为大豆蛋白的0.5~1.5wt%。
所述硅烷偶联剂的用量为大豆蛋白的0.5~1wt%。
制得的大豆蛋白/微晶纤维素胶粘剂可以用作粘结木材和纸张等。
与现有技术相比较,本发明的创新如下:
本发明通过在大豆蛋白中填加微晶纤维素进行改性,改善了大豆蛋白的粘结性能,得到粘结强度好的大豆蛋白/微晶纤维素胶粘剂。本发明充分利用了来源丰富的大豆蛋白和微晶纤维素,节能环保,这样的蛋白质材料实用性更强。
具体实施方式
以下利用实施例进一步详细说明本发明,但不能认为是限定发明的范围。
实施例1大豆蛋白溶液的制备
先量取50ml的去离子水倒入三口烧瓶中,再称取2g的大豆分离蛋白倒入三口烧瓶中,于85℃水浴搅拌1h,得到大豆蛋白溶液。
实施例2大豆蛋白/微晶纤维素胶粘剂的制备
在上述大豆蛋白溶液中加入3mL甲基丙烯酰氧基官能团硅烷和0.5g的微晶纤维素,在65℃水浴中继续搅拌1h,得到大豆蛋白/微晶纤维素胶粘剂。
实施例3大豆蛋白/微晶纤维素胶粘剂胶液粘度的测定
将以上实例制得的大豆蛋白/微晶纤维素胶粘剂胶液,按照GB/T 2794-1995,采用旋转粘度计法测其粘度。所测得的粘度是0.24~12.62Pa.s。
实施例4胶粘强度的测试
将以上实例制得的大豆蛋白/微晶纤维素胶粘剂胶液均匀地涂在木板上,在120℃、1MPa热压条件下热压10min。用拉力试验机所测得的剪切强度即为胶粘强度。耐水强度的测定方法:将粘结后的木材放入自来水中24h,取出后放置于通风橱中干燥24h,测量剪切强度。所测得的剪切粘度可以达到2.5MPa,耐水强度可以达到1.3MPa。

Claims (1)

1.一种大豆蛋白/微晶纤维素胶粘剂的制备方法,包括大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕、豆饼、微晶纤维素、硅烷偶联剂,其特征是,以大豆浓缩蛋白、大豆分离蛋白、脱脂大豆粉、大豆粕和豆饼中的任何一种为原料,微晶纤维素和硅烷偶联剂为改性剂,将大豆蛋白原料与水和微晶纤维素及硅烷偶联剂混合,其中改性条件为:温度60~90℃,时间为1h~2h,大豆蛋白/微晶纤维素/硅烷偶联剂的质量比为:100/(0.5~1.5)/(0.5~1),具体工艺是,量取40~60mL的去离子水,称取2g的大豆蛋白倒入三口烧瓶中于85℃水浴中搅拌1h,再按照比例把微晶纤维素和硅烷偶联剂加到烧杯中,在65℃水浴中继续搅拌1h,得到微晶纤维素改性的大豆蛋白胶粘剂。
CN201210540443.0A 2012-12-14 2012-12-14 一种大豆蛋白/微晶纤维素胶粘剂的制备方法 Active CN103173188B (zh)