CN103172034A - 一种利用高频振动器对硫酸进行脱色的方法 - Google Patents
一种利用高频振动器对硫酸进行脱色的方法 Download PDFInfo
- Publication number
- CN103172034A CN103172034A CN2013101016229A CN201310101622A CN103172034A CN 103172034 A CN103172034 A CN 103172034A CN 2013101016229 A CN2013101016229 A CN 2013101016229A CN 201310101622 A CN201310101622 A CN 201310101622A CN 103172034 A CN103172034 A CN 103172034A
- Authority
- CN
- China
- Prior art keywords
- sulfuric acid
- dither
- frequency
- impurity
- purity
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
一种利用高频振动器对硫酸进行脱色的方法,包括以下步骤:(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释;(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为120-200Hz,每次激振40-60s,激振力为6-10KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将上层液体送入离心机中,在转速800-1500r/min下离心处理2-5min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%;(3)将离心处理后所得液体在温度140-160℃下恒温加热15-30min,使水分挥发,即成。利用本发明对硫酸进行脱色不影响硫酸成品的使用性能,所得硫酸成品的纯度和透明度高。
Description
技术领域
本发明涉及一种硫酸脱色的方法,尤其是涉及一种利用高频振动器对硫酸进行脱色的方法。
背景技术
目前,工业上普遍应用的硫酸制备方法受制备过程中反应物未反应完全,有中间产物生成,制备原料中的杂质等多方面因素影响,导致生产出的硫酸纯度不够,颜色浑浊,严重影响硫酸的使用性能,给工业的发展带来不便。
CN102757021A于2012年10月31日公开了一种使用过氧化氢对硫酸进行脱色的方法,该方法将过氧化氢溶液以6-18L/min·t的速度注入到密闭硫酸脱色槽的硫酸中,硫酸与过氧化氢溶液的体积比为100:6-22;同时不断搅拌,搅拌速度为8-15转/分钟,得成品硫酸。其存在的缺陷是,硫酸在纯度和透明度方面得以改善后,伴随有过氧化氢溶液,可能在一定程度上影响其使用性能;此外,在改善硫酸纯度和透明度方面还尚欠理想。
发明内容
本发明所要解决的技术问题是,提供一种不影响其使用性能,能更好地改善硫酸纯度和透明度的利用高频振动器对硫酸进行脱色的方法。
本发明解决其技术问题采用的技术方案是:一种利用高频振动器对硫酸进行脱色的方法,包括以下步骤:
(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为15-25wt%(优选18-22wt%);
(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为120-200Hz,每次激振40-60s,激振力为6-10KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将分层所得上层液体送入与振动器有导管连接的离心机中,在转速800-1500r/min下离心处理2-5min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%,关闭高频振动器;
(3)将离心处理后所得液体在温度140-160℃下恒温加热15-30min,使水分挥发,即成。
本发明首先对硫酸进行稀释,然后通过高频振动使稀释后的硫酸中的有色粒子、杂质在震动作用下与硫酸分离,再经离心处理分离出硫酸,最后对分离出的硫酸进行加热提纯,得到高纯度硫酸。
与现有技术相比,利用本发明对硫酸进行脱色不影响硫酸成品的使用性能,所得硫酸成品的纯度和透明度更高;此外,本发明操作简便,成本低廉,可大大降低工业用硫酸的生产成本。
具体实施方式
以下结合实施例对本发明作进一步说明。
实施例1
本实施例包括以下步骤:
(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为18wt%;
(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为120Hz,每次激振45s,激振力为7KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将分层所得上层液体送入与振动器有导管连接的离心机中,在转速1000r/min下离心处理3min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%,关闭高频振动器;
(3)将离心处理后所得液体在温度140℃下恒温加热30min,使水分挥发,得高纯度硫酸。
本实施例采用高频振动器处理硫酸,使硫酸脱色,所得成品酸分析结果见表1。
由表1可知,本实施例所得成品酸中硫酸的质量分数≥99.5%,杂质灰分、铁、砷、汞、铅的含量低,纯度高,透明度高(透明度≥190mm)。
实施例2
本实施例包括以下步骤:
(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为20wt%;
(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为150Hz,每次激振50s,激振力为8KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将分层所得上层液体送入与振动器有导管连接的离心机中,在转速1000r/min下离心处理3min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%,关闭高频振动器;
(3)将离心处理后所得液体在温度150℃下恒温加热25min,使水分挥发,得高纯度硫酸。
本实施例采用高频振动器处理硫酸,使硫酸脱色,所得成品酸分析结果见表2。
由表2可知,本实施例所得成品酸中硫酸的质量分数≥99.6%,杂质灰分、铁、砷、汞、铅的含量低,纯度高,透明度高(透明度≥200mm)。
实施例3
本实施例包括以下步骤:
(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为22wt%;
(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为180Hz,每次激振55s,激振力为9KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将分层所得上层液体送入与振动器有导管连接的离心机中,在转速1000r/min下离心处理4min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%,关闭高频振动器;
(3)将离心处理后所得液体在温度160℃下恒温加热20min,使水分挥发,得高纯度硫酸。
本实施例采用高频振动器处理硫酸,使硫酸脱色,所得成品酸分析结果见表3。
由表3可知,本实施例所得成品酸中硫酸的质量分数≥99.4%,杂质灰分、铁、砷、汞、铅的含量低,纯度高,透明度高(透明度≥195mm)。
Claims (2)
1. 一种利用高频振动器对硫酸进行脱色的方法,其特征在于:包括以下步骤:
(1)将含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为15-25wt%;
(2)将稀释后的硫酸盛入装有高频振动器的容器中,启动高频振动器,振动频率为120-200Hz,每次激振40-60s,激振力为6-10KN,在高频振动作用下硫酸中的有色粒子、杂质与硫酸分层,将分层所得上层液体送入与振动器有导管连接的离心机中,在转速800-1500r/min下离心处理2-5min,直至容器的硫酸的体积分数≤稀释后的硫酸体积的5%,关闭高频振动器;
(3)将离心处理后所得液体在温度140-160℃下恒温加热15-30min,使水分挥发,即成。
2.根据权利要求1所述的利用高频振动器对硫酸进行脱色的方法,其特征在于:步骤(1)中,含有杂质、颜色浑浊的硫酸用蒸馏水稀释至浓度为18-22wt%。