CN103103745A - 新型节能、环保毛纺专用和毛油及其制备方法 - Google Patents
新型节能、环保毛纺专用和毛油及其制备方法 Download PDFInfo
- Publication number
- CN103103745A CN103103745A CN2011103543612A CN201110354361A CN103103745A CN 103103745 A CN103103745 A CN 103103745A CN 2011103543612 A CN2011103543612 A CN 2011103543612A CN 201110354361 A CN201110354361 A CN 201110354361A CN 103103745 A CN103103745 A CN 103103745A
- Authority
- CN
- China
- Prior art keywords
- oil
- crude oil
- minutes
- aeo
- fatty alcohol
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种以废生活用新型精炼的“地沟油”为基础原料代替5#或7#矿物油为和毛油的基础原料,配备脂肪醇类非离子表面活性剂制备新型节能、环保的和毛油。其组分为:地沟油:50~60份。脂肪醇非离子表面活性剂:40~50份。新型精炼“地沟油”为基础原料的和毛油,“地沟油”的精制方法为:取一份原油以1∶1.5的水,在50℃~60℃的温度下搅拌40~50分钟,静置30分钟,放出水与杂质。再进行同上方法水洗2次。脂肪醇非离子表面活性剂以AEO-3、AEO-9、AEO-7其中两种以上的组合。本和毛油采用精制地沟油与脂肪醇类助剂相结合制备而成,具有良好的平滑性,适用于生产,具备优于矿物油的特性。
Description
技术领域
本发明属于毛纺加工领域,是一种新型的地沟油代替润滑油为基础原料的毛纺加工必须使用的润滑剂——和毛油。
背景技术
羊毛在生产加工中纤维与纤维之间、纤维与机械之间摩擦产生大量的静电,就如同我们脱羊毛衫一样静电非常大。因此,在羊毛加工之前需要喷洒一定量的和毛油,起到消除静电减少摩擦力、增强纤维的抱合力的作用,以此减少断头率提高可纺性,使纺纱的质量和效率得以保证。现有的和毛油主要还是以5#或7#矿物白油为基础原料,再加上表面活性剂复配而成。随着石油资源越来越紧张且价格越来越高,给和毛油的生产带来一定的影响,必须用一种新型的既节能又环保市场上随处可见的其它原料代替。
发明内容
本发明的目的在于以废生活用地沟油代替5#或7#矿物油为和毛油的基础原料,制备新型节能、环保的和毛油。
具体实施方式
一种新型精炼的“地沟油”为基础原料,配备脂肪醇类非离子表面活性剂而合成的和毛油:
地沟油:50~60份。
脂肪醇非离子表面活性剂:40~50份。
脂肪醇非离子表面活性剂以AEO-3、AEO-9、AEO-7其中两种以上的组合。
新型精炼地沟油为合毛油基础原料的精制方法:
1、取一份原油以1∶1.5的水,在50℃~60℃的温度下搅拌40~50分钟,静置30分钟,放出水与杂质。
2、升温至230℃~260℃同时负压40~50分钟,抽出异味。
3、再以5%的硫酸水,以1∶1.5的比例在50℃~60℃条件下继续水洗30~40分钟,静置30分钟后放出水分和杂质。
4、再进行同上方法水洗2次。
5、过滤脱色。
6、进行检验,采用气相色谱法。其检验项目:水分≤0.1、酸价≤5、皂化价160~190、碘值80~120。
新型节能环保的合毛油制备方法:
在常温下将精炼地沟油与脂肪醇非离子表面活性剂按一定比例放在容器中,充分搅拌15~20分钟后得到新型节能环保的和毛油产品。
本发明的优点和积极效果是:
1、本和毛油采用精制地沟油与脂肪醇类助剂相结合制备而成,具有良好的平滑性,适用于生产,具备优于矿物油的特性。
2、本和毛油在常规条件下制备方法简单可靠,制备出的和毛油产品为淡黄色透明液体,易溶于水,PH值为7~7.5,常规条件下能够稳定,易于运输和储存。
3、本和毛油采用生物可降解且对环境友好的脂肪醇非离子助剂做为复配助剂,起到了环保作用(不含APEO)。
4、本和毛油以精制地沟油为基础原料替代矿物油是一项节约石油不可再生资源的重要举措,同时也给纺织助剂增添了一种新型更好的节能环保的新材料。
5、本和毛油的精制地沟油与矿物油价格相比要低于目前矿物油价格的10%左右,降低了生产成本,给生产厂家和用户带来了更好的经济效益。
6、本和毛油采用地沟油进行精制,达到了废物利用、物尽其用的效果。同时也开辟了废油利用的新途径,更有效地解决阻止地沟油回流餐桌一种新办法。
具体实施方式
以下结合实例对本发明做进一步描述:
一种新型节能环保和毛油,其原料组分及组分的重量份数分别为:
精制地沟油:60~50份。
脂肪醇非离子助剂:40~50份。
脂肪醇类非离子助剂为AEO-9、AEO-7、AEO-3的其中两种以上的组合。
地沟油的精炼制备方法包括如下步骤:
1、在50℃~60℃的水温进行清洗40~50分钟,静置30分钟后放出水和杂质。
2、蒸馏升温至230℃~260℃,同时负压抽40~50分钟,去除部分异味。
3、酸洗再以5%的硫酸水以1∶1.5的比例,在50℃~60℃条件下继续清洗30~40分钟,静置30分钟后放出水和杂质。
4、再进行水洗2次,然后静置30分钟后放出水分。
5、脱色处理后成为精制“地沟油”。
下面通过一些具体实施例对本合毛油产品制备方法进行说明
实施例:
1、将精制地沟油取50kg放在容器中,取AEO-320kg、AEO-920kg、AEO-75kg、离子水5kg,在常温下充分搅拌15~30分钟,静置取样,得到精纺和毛油产品。
2、将精制地沟油取60kg放在容器中,取AEO-3 15kg、AEO-9 15kg、离子水10kg,在常温下充分搅拌15~30分钟,静置取样,得到和毛油产品。
本新型节能环保和毛油的使用方法为:
将和毛油以羊毛的1.5%-5%的比例,再按与水的比1∶5~20的比例进行稀释充分搅拌,制成和毛油的稀释液,在和毛工序和纺纱并条工序中喷洒在羊毛上,达到毛纤维含有不超过1.5%的含油率,羊毛才具有平行顺滑的纺纱效果。保持6~8小时后再进行下工序的作业。
本新型节能环保和毛油的化学机理为:和毛油是将几种原料混合的品质较均匀的混合体。羊毛开松、除杂、梳理过程中要经过多次的拉伸。为减少纤维在梳理过程中的损伤,需要加入适量的和毛油,以增强纤维的润滑性,降低其摩擦系数。同时,纤维在后道加工过程中将会受到各种摩擦而产生静电,导致纤维扩散。加入和毛油后可消除或减少静电,增加纤维之间的抱合力,有利于后道各工序加工的正常进行,提高产品质量和制成率。
需要强调的是:本发明所述的实施例是说明性的,而不是限定性的。因此本发明并不是限于具体实施方式中所述的实施例。凡是由本领域技术人员根据本发明的技术方案得出的其他实施方式同样属于本发明保护的范围。
Claims (3)
1.一种以废生活用新型精炼“地沟油”为基础原料的和毛油,其特征在于:
地沟油:50~60份。
脂肪醇非离子表面活性剂:40~50份。
脂肪醇非离子表面活性剂以AEO-3、AEO-9、AEO-7其中两种以上的组合。
2.根据权利要求1所述的新型精炼“地沟油”为基础原料的和毛油,
其特征在于:所述的“地沟油”的精制方法为:
取一份原油以1∶1.5的水,在50℃~60℃的温度下搅拌40~50分钟,静置30分钟,放出水与杂质。
升温至230℃~260℃同时负压40~50分钟,抽出异味。
再以5%的硫酸水,以1∶1.5的比例在50℃~60℃条件下继续水洗30~40分钟,静置30分钟后放出水分和杂质。
再进行同上方法水洗2次。
过滤脱色。
进行检验,采用气相色谱法。其检验项目:水分≤0.1、酸价≤5、皂化价160~190、碘值80~120。
3.根据权利要求1所述的新型精炼“地沟油”为基础原料的和毛油,
其特征在于:所述新型节能环保的合毛油制备方法:
在常温下将精炼地沟油与脂肪醇非离子表面活性剂按一定比例放在容器中,充分搅拌15~20分钟后得到新型节能环保的和毛油产品。