Prior art keywords
improvement
crepe
elastin
reed
satin
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012104611556A
Other languages
English (en)
Inventor
周丰林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2012104611556A priority Critical patent/CN103103688A/zh
Publication of CN103103688A publication Critical patent/CN103103688A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Looms (AREA)

Abstract

本发明提供了一种弹力素绉缎生产工艺的改进,采用19号钢筘。本发明的改进工艺在保持面料设计姆米(厚度)不变的情况下,将筘号由21.5号减小至19号,并保持成品门幅为140CM。通过减少筘号,以增加筘齿间的间隙,有效地提高弹力缎经向密度和纬向密度,实质性地解决成品弹性差的问题,确保成品质量。

Description

一种弹力素绉缎生产工艺的改进
技术领域
本发明涉及一种丝绸工艺,具体涉及一种弹力素绉缎生产工艺的改进。
背景技术
弹力素绉缎,具备了优良的弹性、手感柔软、轻盈秀气、穿着舒适、缩水率较小的优势。常规的弹力缎,其产品成品门幅为140CM,传统的生产工艺是采用21.5号钢筘,每筘穿入数为4。采用以上工艺加工织造弹力缎,由于所采用的筘号对其筘齿间隙的影响,导致产品的经向密度和纬向密度都不高,成品的弹性差,严重影响产品质量。
发明内容
针对以上现有技术中存在的问题,本发明提供了一种有效解决成品弹性差的弹力缎改进工艺。
本发明是通过以下技术方案实现的:
一种弹力素绉缎生产工艺的改进,所述工艺采用19号钢筘,成品门幅为140CM。
本发明的有益效果为:本发明的改进工艺在保持面料设计姆米(厚度)不变的情况下,将筘号由21.5号减小至19号,利于提高弹力缎经向密度和纬向密度,实质性地解决成品弹性差的问题,确保成品质量。
具体实施方式
本发明提供了弹力缎的改进工艺,工艺中保持了面料设计姆米(厚度)不变,保持了成品门幅为140CM。改进的部分为:摒弃了现有技术中采用的21.5号钢筘的设置,采用了较少的19号钢筘。
基于筘号与经向密度成正比的设计原理,通过减少筘号,以增加筘齿间的间隙,同时配合有效门幅的增加,以及纬线用量的增加,能有效地提高弹力缎经向密度和纬向密度,实质性地解决成品弹性差的问题,确保成品质量。

Claims (1)

1.一种弹力素绉缎生产工艺的改进,其特征在于所述工艺采用19号钢筘,成品门幅为140CM。
CN2012104611556A 2012-11-16 2012-11-16 一种弹力素绉缎生产工艺的改进 Pending CN103103688A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2012104611556A CN103103688A (zh) 2012-11-16 2012-11-16 一种弹力素绉缎生产工艺的改进

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2012104611556A CN103103688A (zh) 2012-11-16 2012-11-16 一种弹力素绉缎生产工艺的改进

Publications (1)

Publication Number Publication Date
CN103103688A true CN103103688A (zh) 2013-05-15

Family

ID=48311866

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2012104611556A Pending CN103103688A (zh) 2012-11-16 2012-11-16 一种弹力素绉缎生产工艺的改进

Country Status (1)

Country Link
CN (1) CN103103688A (zh)

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105040229A (zh) * 2015-09-14 2015-11-11 广西华虹绸缎有限责任公司 一种240素绉缎的织造方法

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH1037040A (ja) * 1996-07-17 1998-02-10 Tajima Kinuorimono Kyodo Kumiai 絹綿複合織りゆかた地及びその製造方法
CN101255626A (zh) * 2008-04-14 2008-09-03 江苏华佳丝绸有限公司 一种立体弹力真丝美缎
CN102051729A (zh) * 2010-12-28 2011-05-11 达利丝绸(浙江)有限公司 真丝印经织造工艺及其应用

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH1037040A (ja) * 1996-07-17 1998-02-10 Tajima Kinuorimono Kyodo Kumiai 絹綿複合織りゆかた地及びその製造方法
CN101255626A (zh) * 2008-04-14 2008-09-03 江苏华佳丝绸有限公司 一种立体弹力真丝美缎
CN102051729A (zh) * 2010-12-28 2011-05-11 达利丝绸(浙江)有限公司 真丝印经织造工艺及其应用

Non-Patent Citations (5)

* Cited by examiner, † Cited by third party
Title
冯岑等: "全真丝纬向弹力机织物的设计与分析", 《丝绸》 *
唐虹: "弹力素绉缎缝缩的方向性研究", 《丝绸》 *
对外经济贸易部: "《中国对外经济贸易年鉴 1991》", 31 December 1988, 中国社会出版社 *
朱俊芳,左葆齐,饶纲强,周立平: "蚕丝/氨纶弹力织物机织工艺研究", 《丝绸》 *
陈文娟等: "开发新产品准确选择筘号的生产研究", 《江苏纺织》 *

Cited By (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105040229A (zh) * 2015-09-14 2015-11-11 广西华虹绸缎有限责任公司 一种240素绉缎的织造方法

Similar Documents

Publication Publication Date Title
CN103103688A (zh) 一种弹力素绉缎生产工艺的改进
CN103276497A (zh) 一种含有桑蚕丝、丝光棉和胶原蛋白纤维的复合丝织物
CN102851831A (zh) 弹力缎的改进工艺
CN103103691A (zh) 一种宽幅素绉缎生产工艺的改进
CN102877184A (zh) 14548素绉缎的改进工艺
MX360007B (es) Tela industrial bicapa.
CN203373504U (zh) 一种双芯牛仔面料
CN204936358U (zh) 一种具有弹力且能定型的皮革
CN204280829U (zh) 一种人丝织造压辊牵应力卷取装置
CN102922831A (zh) 一种冰爽弹性面料
CN204589474U (zh) 拉链织带机的压带板装置
CN202891334U (zh) 一种双层一体式毛毯
CN202559008U (zh) 双斜服装布料
CN201567416U (zh) 一体编织防滑织带
CN103498257A (zh) 一种防尘牛仔布
CN103103689A (zh) 一种宽幅双宫绸生产工艺的改进
CN202786633U (zh) 棉涤弹力牛仔布
CN202744728U (zh) 全棉薄型牛仔布
CN103103690A (zh) 一种中幅斜纹绸生产工艺的改进
CN203846209U (zh) 喷水织机的纬纱筒座板
CN102851838A (zh) 19015斜纹绸的改进工艺
CN203136034U (zh) 一种平板电视
CN206495019U (zh) 用于剑杆织机的齿条
CN102864553A (zh) 19006斜纹绸的改进工艺
CN201473687U (zh) 剑杆织机的送纬剑杆头壳体

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130515