CN103046331B - 一种高效低泡环保型精练剂及其制备方法 - Google Patents

一种高效低泡环保型精练剂及其制备方法 Download PDF

Info

Publication number
CN103046331B
CN103046331B CN201210536924.4A CN201210536924A CN103046331B CN 103046331 B CN103046331 B CN 103046331B CN 201210536924 A CN201210536924 A CN 201210536924A CN 103046331 B CN103046331 B CN 103046331B
Authority
CN
China
Prior art keywords
scouring agent
weight
isomeric alcohol
preparation
polyethenoxy ether
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201210536924.4A
Other languages
English (en)
Other versions
CN103046331A (zh
Inventor
秦勇
储富强
陶永新
孔泳
黎珊
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Huayu Fastener Co., Ltd
Original Assignee
Changzhou University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Changzhou University filed Critical Changzhou University
Priority to CN201210536924.4A priority Critical patent/CN103046331B/zh
Publication of CN103046331A publication Critical patent/CN103046331A/zh
Application granted granted Critical
Publication of CN103046331B publication Critical patent/CN103046331B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明提供了一种高效低泡环保型精练剂及其制备方法,该精练剂按照重量百分比包括:15~25%的十二烷基二苯醚二磺酸钠、5~15%C12~16仲烷基磺酸钠、15~25%烷基糖苷、10~15%异构醇聚氧乙烯醚,余量为水。制备该精练剂的具体步骤为:(1)将十二烷基二苯醚二磺酸钠和C12~16仲烷基磺酸钠加水搅拌溶解;(2)将烷基糖苷和异构醇聚氧乙烯醚加入步骤(1)的混合液中,搅拌混合均匀。本发明工艺简单、配方环保,产品的性能优异,是一种绿色环保印染助剂。

Description

一种高效低泡环保型精练剂及其制备方法
技术领域
本发明涉及一种纺织印染前处理助剂,特别涉及一种高效低泡环保型精练剂。 
背景技术
精练剂是经过一定的配比的方法得到的,一种以洗涤作用为主的、兼有渗透、乳化、分散、络合等协同作用的复配物,包括表面活性剂以及适当的添加剂。精练剂在退、煮、漂工序中起着非常重要的作用。大部分精练剂的耐碱浓度一般在100g/L以下,而退、煮、漂补充碱的浓度在200g/L以上,烧碱和精练剂,只能分开配料。这样虽然碱浓度可控制,但精练剂浓度无法准确控制,导致半制品毛效差异,若将精练剂和烧碱配在一起,便能彻底解决这个问题,故需要能耐200g/L烧碱,在浓碱条件下有强耐碱性,不能出现漂油、沉析等不良现象的精炼剂,而且渗透性要好。 
目前,我国能耐200g/L烧碱的精练剂不仅品种少,而且质量不稳定,特别是环保型产品的开发和发展缓慢,充斥市场的都是含烷基磷酸酯盐和烷基酚聚氧乙烯醚等表面活性剂的产品。烷基磷酸酯虽然具有很好的耐碱性和渗透性,但会导致水体的富营养化;而烷基酚聚氧乙烯醚因为具有致癌性、致畸性及耐生物降解而被禁用。因此目前的精练剂均因为环保问题面临被淘汰的局面。国外已经有替代烷基磷酸酯和烷基酚聚氧乙烯醚活性组分的精练剂出现,国内虽然也开发了一些产品,但效果仍不理想,每年我国仍需从国外大量进口环保型精练剂。 
发明内容
本发明所要解决的技术问题是:现有技术中,能耐高浓度碱的精练剂品种少,而且质量不稳定,使用过程中还会带来环境污染问题。 
为解决这一技术问题,本发明提供的技术方案是: 
本发明提供了一种高效低泡环保型精练剂,该精练剂的组成,按照重量百分比包括:15~25%的十二烷基二苯醚二磺酸钠、5~15%C12~16仲烷基磺酸钠、15~25%烷基糖苷、10~15%异构醇聚氧乙烯醚和20~55%的水, 
该精炼剂的配方包括两种性质的组分,一组为阴离子表面活性剂,一组为非离子表面活性剂, 
具体地说,该精练剂中的阴离子表面活性剂为十二烷基二苯醚二磺酸钠和C12~16仲烷基 磺酸钠,十二烷基二苯醚二磺酸钠能耐>400g/L强碱,而C12~16仲烷基磺酸钠只能耐<80g/L的碱,但仲烷基磺酸钠具有更好的渗透性和乳化性; 
非离子表面活性剂为烷基糖苷和异构醇醚聚氧乙烯醚,烷基糖苷能耐>400g/L的强碱,异构醇聚氧乙烯醚则只能耐<60g/L的碱,烷基糖苷的乳化性差,但醇醚具有更优异的洗涤性,通过这种阴非离子复配技术实现本发明, 
作为优选:烷基糖苷的烷基链长为8~14, 
作为优选:异构醇聚氧乙烯醚的烷基链长为10~13, 
作为优选:异构醇聚氧乙烯醚的EO链长为5~12。 
本发明还提供了一种上述精练剂的制备方法,按重量百分比,具体步骤为, 
(1)将十二烷基二苯醚二磺酸钠和C12~16仲烷基磺酸钠加水搅拌溶解; 
(2)将烷基糖苷和异构醇聚氧乙烯醚加入步骤(1)的混合液中,搅拌混合均匀, 
作为优选:重量百分比为,15~25%的十二烷基二苯醚二磺酸钠、5~15%的C12~16仲烷基磺酸钠、15~25%的烷基糖苷、10~15%的异构醇聚氧乙烯醚,20~55%的水。 
本发明的有益效果是:本发明采用十二烷基二苯醚二磺酸钠取代烷基磷酸酯盐;窄分布的异构醇聚氧乙烯醚和烷基糖苷复配取代烷基酚聚氧乙烯醚,实现产品的绿色化。异构醇聚氧乙烯醚具有优异的乳化性和洗涤性,烷基糖苷具有优异的渗透性,是烷基酚聚氧乙烯醚的理想替代品;耐强碱、低泡、高螯合能力的十二烷基二苯醚二磺酸钠是烷基磷酸酯的理想替代品。本发明中提到的十二烷基二苯醚二磺酸钠、C12~16仲烷基磺酸钠、烷基糖苷、异构醇聚氧乙烯醚市场上都有商品出售,产品制备工艺简单。制备出的产品耐碱性高,渗透快,起泡性低,稳定性好,使用过程中,不易引起环境污染。 
具体实施方式
实施例(一) 
按以下步骤制备高效低泡环保型精练剂,具体操作为: 
(1)在反应釜中,将15kg十二烷基二苯醚二磺酸钠和5kg C12~16仲烷基磺酸钠(SAS60),加50kg水搅拌,充分溶解; 
(2)将20kg C10烷基糖苷和10kg C13异构醇聚氧乙烯醚(EO=7-10)加入步骤(1)的反应釜中,充分搅拌溶解,出料。 
制得的高效低泡环保型精炼剂的主要技术性能指标如下 
外观:黄色透明水溶液 
比重:1.0kg/L 
固含量:35% 
耐碱性:210g/L(用浓度为210g/L的NaOH溶液配制精炼剂溶液,不分层、无沉析) 
渗透性:<15s(帆布沉降法) 
起泡性:<30cm(量筒震荡法) 
实施例(二) 
按以下步骤制备高效低泡环保型精练剂,具体操作为: 
(1)在反应釜中,将20kg十二烷基二苯醚二磺酸钠和10kg C12~16仲烷基磺酸钠(SAS60)加40kg水搅拌,充分溶解; 
(2)将15kg C8烷基糖苷和15kg C13异构醇聚氧乙烯醚(EO=5~8)加入步骤(1)的反应釜中,充分搅拌溶解,出料。 
制得的高效低泡环保型精炼剂的主要技术性能指标如下 
外观:黄色透明水溶液 
比重:1.0kg/L 
固含量:38% 
耐碱性:280g/L(用浓度为280g/L的NaOH溶液配制精炼剂溶液,不分层、无沉析) 
渗透性:<10s(帆布沉降法) 
起泡性:<30cm(量筒震荡法) 
实施例(三) 
按以下步骤制备高效低泡环保型精练剂,具体操作为: 
(1)在反应釜中,将25kg十二烷基二苯醚二磺酸钠和15kg C12~16仲烷基磺酸钠(SAS60)加25kg水搅拌,充分溶解; 
(2)将25kg C8烷基糖苷和10kg C13异构醇聚氧乙烯醚(EO=5~8)加入步骤(1)的反应釜中,充分搅拌溶解,出料。 
制得的高效低泡环保型精炼剂的主要技术性能指标如下 
外观:黄色透明水溶液 
比重:1.0kg/L 
固含量:42% 
耐碱性:290g/L(用浓度为290g/L的NaOH溶液配制精炼剂溶液,不分层、无沉析) 
渗透性:<15s(帆布沉降法) 
起泡性:<30cm(量筒震荡法)。 

Claims (6)

1.一种高效低泡环保型精练剂,其特征在于:所述的精练剂按照重量百分比包括:15~25%的十二烷基二苯醚二磺酸钠、5~15%C12~16仲烷基磺酸钠、15~25%烷基糖苷、10~15%异构醇聚氧乙烯醚和20~55%的水。
2.如权利要求1所述的精练剂,其特征在于:所述的烷基糖苷的烷基链长为8~14。
3.如权利要求1所述的精练剂,其特征在于:所述的异构醇聚氧乙烯醚的烷基链长为10~13。
4.如权利要求1所述的精练剂,其特征在于:所述的异构醇聚氧乙烯醚的EO链长为5~12。
5.如权利要求1至4任一项所述的精练剂的制备方法,其特征在于:所述的制备方法为,按重量百分比,由以下步骤实现,
(1)将十二烷基二苯醚二磺酸钠和C12~16仲烷基磺酸钠加水搅拌溶解;
(2)将烷基糖苷和异构醇聚氧乙烯醚加入步骤(1)的混合液中,搅拌混合均匀。
6.如权利要求5所述的精练剂的制备方法,其特征在于:所述的重量百分比为,15~25%的十二烷基二苯醚二磺酸钠、5~15%的C12~16仲烷基磺酸钠、15~25%的烷基糖苷、10~15%的异构醇聚氧乙烯醚,20~55%的水。
CN201210536924.4A 2012-12-12 2012-12-12 一种高效低泡环保型精练剂及其制备方法 Active CN103046331B (zh)