Prior art keywords
iron
ladle
spheroidizing
casting ladle
molten iron
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012105521627A
Other languages
English (en)
Inventor
李贵茂
王建立
李春荣
薄玉发
王恒
苗德壮
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHENYANG MACHINE TOOL YINFENG FOUNDRY CO Ltd
Original Assignee
SHENYANG MACHINE TOOL YINFENG FOUNDRY CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHENYANG MACHINE TOOL YINFENG FOUNDRY CO Ltd filed Critical SHENYANG MACHINE TOOL YINFENG FOUNDRY CO Ltd
Priority to CN2012105521627A priority Critical patent/CN102974777A/zh
Publication of CN102974777A publication Critical patent/CN102974777A/zh
Pending legal-status Critical Current

Links

Images

Classifications

    • YGENERAL TAGGING OF NEW TECHNOLOGICAL DEVELOPMENTS; GENERAL TAGGING OF CROSS-SECTIONAL TECHNOLOGIES SPANNING OVER SEVERAL SECTIONS OF THE IPC; TECHNICAL SUBJECTS COVERED BY FORMER USPC CROSS-REFERENCE ART COLLECTIONS [XRACs] AND DIGESTS
    • Y02TECHNOLOGIES OR APPLICATIONS FOR MITIGATION OR ADAPTATION AGAINST CLIMATE CHANGE
    • Y02PCLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
    • Y02P10/00Technologies related to metal processing
    • Y02P10/20Recycling

Landscapes

  • Refinement Of Pig-Iron, Manufacture Of Cast Iron, And Steel Manufacture Other Than In Revolving Furnaces (AREA)

Abstract

一种热浇包球化处理工艺,在出铁前用原铁水烫一遍浇包,使其在埋包之前达到红热状态;埋包处理时,操作者在浇包外部将球化剂、硅铁粒、钢铁屑按先后顺序倒入包内堤坝处,逐层摊平捣实;利用起吊设备将预制的原铁水铸铁盖板放在捣实层上;最后向包内冲入铁水,完成球化处理。该球化处理工艺可降低球化处理时铁水与浇包之间的温度差,避免铁水温度损失过大;球化处理后铁水温度可达1400℃~1480℃;埋包处理操作者无需进入包内,在包外利用起吊设备完成压盖操作,可降低高温操作的危险性;用原铁水铸铁盖板代替珍珠岩层,避免了使用珍珠岩产生的造渣问题;通过调整盖板厚度可延缓球化起爆时间,保证球化反应平稳。

Description

一种热浇包球化处理工艺
技术领域
本发明涉及铁水球化处理工艺,特别是一种利用原铁水预热浇包,然后进行浇包外埋包的球化处理工艺。
背景技术
目前,生产球铁铸件的企业大都采用浇包内修筑堤坝、用硅铁粒和珍珠岩等辅料覆盖球化剂,冲入法处理的球化工艺。在球化处理过程中,由于炉体不断转动,铁水落点不断变化,所覆盖的硅铁粒、钢铁屑和珍珠岩密度较小,极易漂浮及熔化过快,导致球化反应过早,球化不良等情况发生。另外,对较小铸件进行球化处理时,由于铁水包小,出铁量少,球化处理过程中铁水温度损失大,使处理后的铁水温度较低。
发明内容
本发明的目的是针对上述现有球化处理工艺存在的缺陷提供一种热浇包球化处理工艺。该球化处理工艺可降低铁水与浇包之间的温度差,从而减少球化处理时铁水的温度损失,提高球化处理后铁水温度,同时操作者埋包不需进入包内,降低高温操作的危险。
为实现上述目的,本发明提供的热浇包球化处理工艺按以下步骤进行:
(1)在出铁前30分钟内使用原铁水烫一遍浇包,使其在埋包之前达到红热状态;
(2)埋包处理时,操作者在浇包外部将球化剂、硅铁粒、钢铁屑按先后顺序倒入包内堤坝处,并逐层摊平捣实;
(3)利用起吊设备将预制的原铁水铸铁盖板吊起放在步骤(2)的捣实层上;
(4)向包内冲入铁水,完成热浇包球化处理,球化处理后铁水温度为1400℃~1480℃。
所述原铁水铸铁盖板的厚度根据浇包的大小在5—30mm范围内选取。
与现有技术相比,本发明球化处理工艺的有益效果是:
1、球化处理时铁水与浇包之间的温度差降低,避免球化处理时铁水温度损失过大;
2、埋包处理时,操作者无需进入包内;
3、在捣实包外利用起吊设备完成压盖操作,可降低高温操作的危险性;
4、用原铁水铸铁盖板代替珍珠岩层,避免了使用珍珠岩产生的造渣问题;
5、通过调整原铁水铸铁盖板厚度可延缓球化起爆时间,保证球化反应平稳进行;
6、球化反应在一次出铁完成时开始,球化处理后铁水温度可达到1400℃~1480℃。
附图说明
图1为本发明埋包后的球化包纵向剖视图;
图2为图1的俯视图。
图中:1-球化剂、2-硅铁粒、3-钢铁屑、4-原铁水铸铁盖板、5-吊钩、6-浇包、7-堤坝。
具体实施方式
以下结合附图对本发明作进一步说明。
结合图1和图2,本发明热浇包球化处理工艺,先在出铁前30分钟内使用原铁水烫一遍浇包6,使其在埋包之前达到红热状态;然后操作者在浇包外部将球化剂1、硅铁粒2、钢铁屑3按先后顺序倒入包内堤坝7的一侧,用工具逐层摊平捣实;再利用起吊设备将利用原铁水预制的上部带有吊钩5的原铁水铸铁盖板4吊起放在捣实层上,原铁水铸铁盖板的厚度可根据浇包的大小在5—30mm范围内选取;最后向包内冲入铁水,完成热浇包球化处理过程,球化处理后的铁水温度可达1400℃~1480℃。
本发明适用于各种出炉温度和不同成分铁水的球化处理。

Claims (2)

1.一种热浇包球化处理工艺,其特征是按以下步骤进行:
(1)在出铁前30分钟内使用原铁水烫一遍浇包,使其在埋包之前达到红热状态;
(2)埋包处理时,操作者在浇包外部将球化剂、硅铁粒、钢铁屑按先后顺序倒入包内堤坝处,并逐层摊平捣实;
(3)利用起吊设备将预制的原铁水铸铁盖板吊起放在步骤(2)的捣实层上;
(4)向包内冲入铁水,完成热浇包球化处理,球化处理后铁水温度为1400℃~1480℃。
2.根据权利要求1所述的热浇包球化处理工艺,其特征是,所述原铁水铸铁盖板的厚度根据浇包的大小在5—30mm范围内选取。
CN2012105521627A 2012-12-17 2012-12-17 一种热浇包球化处理工艺 Pending CN102974777A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2012105521627A CN102974777A (zh) 2012-12-17 2012-12-17 一种热浇包球化处理工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2012105521627A CN102974777A (zh) 2012-12-17 2012-12-17 一种热浇包球化处理工艺

Publications (1)

Publication Number Publication Date
CN102974777A true CN102974777A (zh) 2013-03-20

Family

ID=47849287

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2012105521627A Pending CN102974777A (zh) 2012-12-17 2012-12-17 一种热浇包球化处理工艺

Country Status (1)

Country Link
CN (1) CN102974777A (zh)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104624986A (zh) * 2015-01-16 2015-05-20 遵义拓特铸锻有限公司 一种平底塞杆式底注钢水包球化处理的工艺方法
CN106367672A (zh) * 2016-08-31 2017-02-01 云南德胜钢铁有限公司 一种球墨铸铁及其加工工艺
CN106467949A (zh) * 2016-08-31 2017-03-01 云南德胜钢铁有限公司 一种挡矿板及其加工工艺
CN108746572A (zh) * 2018-07-02 2018-11-06 西峡县众德汽车部件有限公司 球化浇注包及球化浇注方法

Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002275575A (ja) * 2001-03-21 2002-09-25 Aisin Seiki Co Ltd 高強度球状黒鉛鋳鉄及びその製造方法
CN101029367A (zh) * 2007-04-17 2007-09-05 刘年路 球化处理装置及球化处理工艺
CN101519708A (zh) * 2009-04-20 2009-09-02 芜湖市金贸流体科技股份有限公司 高韧性、高耐蚀球墨铸铁的生产方法
CN102000785A (zh) * 2010-11-30 2011-04-06 刘之增 冲入法球化包内球化剂的覆盖工艺
CN102071353A (zh) * 2010-12-10 2011-05-25 四川海科机械制造有限公司 一种耐低温高韧性铸态球铁、生产方法及其应用
CN201940591U (zh) * 2010-11-30 2011-08-24 刘之增 冲入法球化包
CN102220540A (zh) * 2011-06-13 2011-10-19 江铃汽车股份有限公司 一种冲入法球化处理工艺
CN102337446A (zh) * 2011-11-03 2012-02-01 广西玉林玉柴机器配件制造有限公司 球化处理的装包工艺

Patent Citations (8)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JP2002275575A (ja) * 2001-03-21 2002-09-25 Aisin Seiki Co Ltd 高強度球状黒鉛鋳鉄及びその製造方法
CN101029367A (zh) * 2007-04-17 2007-09-05 刘年路 球化处理装置及球化处理工艺
CN101519708A (zh) * 2009-04-20 2009-09-02 芜湖市金贸流体科技股份有限公司 高韧性、高耐蚀球墨铸铁的生产方法
CN102000785A (zh) * 2010-11-30 2011-04-06 刘之增 冲入法球化包内球化剂的覆盖工艺
CN201940591U (zh) * 2010-11-30 2011-08-24 刘之增 冲入法球化包
CN102071353A (zh) * 2010-12-10 2011-05-25 四川海科机械制造有限公司 一种耐低温高韧性铸态球铁、生产方法及其应用
CN102220540A (zh) * 2011-06-13 2011-10-19 江铃汽车股份有限公司 一种冲入法球化处理工艺
CN102337446A (zh) * 2011-11-03 2012-02-01 广西玉林玉柴机器配件制造有限公司 球化处理的装包工艺

Non-Patent Citations (4)

* Cited by examiner, † Cited by third party
Title
天津市机械工业管理局: "《铸造工必读》", 31 January 1991, article "球化处理" *
机械工业部: "《化铁工操作技能与考核》", 31 January 1997, article "球化处理" *
陈琦等: "《铸造循环利用技术》", 31 July 2009, article "钢铁屑" *
骆莉等: "《工程材料及机械制造基础》", 29 February 2012, article "球化处理" *

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN104624986A (zh) * 2015-01-16 2015-05-20 遵义拓特铸锻有限公司 一种平底塞杆式底注钢水包球化处理的工艺方法
CN106367672A (zh) * 2016-08-31 2017-02-01 云南德胜钢铁有限公司 一种球墨铸铁及其加工工艺
CN106467949A (zh) * 2016-08-31 2017-03-01 云南德胜钢铁有限公司 一种挡矿板及其加工工艺
CN108746572A (zh) * 2018-07-02 2018-11-06 西峡县众德汽车部件有限公司 球化浇注包及球化浇注方法

Similar Documents

Publication Publication Date Title
CN106811676A (zh) 一种高强度高韧性铸态qt700‑10及其生产方法
RU2018141749A (ru) Способ производства чугуна, устройство для его производства и чугун, полученный указанным способом
CN102974777A (zh) 一种热浇包球化处理工艺
CN105364028B (zh) 一种球墨铸铁球化处理包堤坝的砌筑方法
CN105200305B (zh) 一种灰铸铁及其制备方法
CN103849710A (zh) 一种电炉全铁水冶炼工艺生产高碳铬轴承钢的方法
CN105154623A (zh) 一种熔炼38CrMoAl钢的高效合金化方法
CN105420592A (zh) 耐低温球墨铸铁件及其制备方法
CN109338026A (zh) 高温球墨铸铁的制造工艺
CN102703809A (zh) 一种热轧钢及其制造方法
CN104084770A (zh) 一种42CrMo轴承套圈毛坯的铸辗复合工艺
IN2015KN00602A (zh)
CN108193019A (zh) 一种精密铸造熔炼浇注工艺
CN114905033B (zh) 一种带加热功能的铁水罐结构
CN105132626A (zh) 注余钢渣回收利用方法
CN104561409A (zh) 一种亚共晶铸造生铁的生产方法
CN103045931B (zh) 一种低温无镍情况下获得合格机械性能的熔炼方法
CN105316566A (zh) 一种矿山专用耐磨球及其制造方法
CN105290345A (zh) 一种钢包铸余钢水的处理方法
CN105039834A (zh) 一种耐低温球墨铸铁熔炼工艺
CN105344949B (zh) 一种钢铁熔炼‑模铸新工艺
CN103874771B (zh) 球墨铸铁的球化处理方法
CN103992125B (zh) 一种陶瓷流槽的制备方法
CN104624986A (zh) 一种平底塞杆式底注钢水包球化处理的工艺方法
CN103740946B (zh) 一种用于铝熔体在线精炼的设备及方法

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C53 Correction of patent of invention or patent application
CB03 Change of inventor or designer information

Inventor after: Zhao Shouguo

Inventor after: Wang Lianshuang

Inventor after: Li Guimao

Inventor after: Bao Yufa

Inventor after: Miao Dezhuang

Inventor after: Liu Yan

Inventor after: Zhang Jibo

Inventor before: Li Guimao

Inventor before: Wang Jianli

Inventor before: Li Chunrong

Inventor before: Bao Yufa

Inventor before: Wang Heng

Inventor before: Miao Dezhuang

COR Change of bibliographic data

Free format text: CORRECT: INVENTOR; FROM: LI GUIMAO WANG JIANLI LI CHUNRONG BAO YUFA WANG HENG MIAO DEZHUANG TO: ZHAO SHOUGUO WANG LIANSHUANG LI GUIMAO BAO YUFA MIAO DEZHUANG LIU YAN ZHANG JIBO

C12 Rejection of a patent application after its publication
RJ01 Rejection of invention patent application after publication

Application publication date: 20130320