Prior art keywords
cart
silicon rod
glue
rod
sticky stick
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012101877308A
Other languages
English (en)
Other versions
CN102921616B (zh
Inventor
胥大鹏
陈新军
何江涛
李晓建
陆建虎
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Longi Green Energy Technology Co Ltd
Original Assignee
Ningxia Longi Silicon Materials Co Ltd
Yinchuan Longi Silicon Materials Co Ltd
Xian Longi Silicon Materials Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Ningxia Longi Silicon Materials Co Ltd, Yinchuan Longi Silicon Materials Co Ltd, Xian Longi Silicon Materials Corp filed Critical Ningxia Longi Silicon Materials Co Ltd
Priority to CN201210187730.8A priority Critical patent/CN102921616B/zh
Publication of CN102921616A publication Critical patent/CN102921616A/zh
Application granted granted Critical
Publication of CN102921616B publication Critical patent/CN102921616B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Images

Landscapes

  • Crystals, And After-Treatments Of Crystals (AREA)
  • Joining Of Glass To Other Materials (AREA)

Abstract

本发明公布了一种加速硅棒胶水硬化的方法,包括下述步骤:(1)将晶托冶具、玻璃基板、硅棒依次定位在粘棒推车上,用胶水将各部件粘结在一起;(2)将粘结好的各个部件连同粘棒推车推入硅棒加热器,对粘结好的各个部件进行加热;(3)设定烘箱温度50-60度,加热20-40分钟后,将粘棒推车拉出,更换另外的粘棒推车,进行加热硬化;(4)将加热后拉出的粘棒推车上的硅棒自然冷却至室温,完成胶水的硬化。本发明方法,大大缩短的胶水硬化的时间,含加热时间只需2.5小时,提高了工作效率,加快的硅棒粘结场地硅棒的周转速度。同时通过合理的温度和时间的控制,利用特制的加热器,使得加热所需电能消耗也较少,达到了能源消耗和工作效率提高的平衡点。

Description

一种加速硅棒胶水硬化的方法
技术领域
本发明属于硅切割技术领域,特别是涉及一种加速硅棒胶水硬化的方法。
背景技术
现有的硅切割加工时,需要将晶托冶具、玻璃基板、硅棒粘结在一起安装到切割机上进行切割。而粘结胶水的硬化常采用的方法就是常温硬化,这种方式硬化时间较长,时间大约4小时,胶水硬化过程中硅棒占地较多,影响工作效率。也有希望通过加热加速胶水的硬化,但是往往由于硅棒体积较大,所需的加热器的体积和功率也要较大,这样就大大增加了成本,因此很少采用加热器硬化胶水的方法。
发明内容
本发明目的在于针对现有技术的缺陷提供一种节约能源,工作效率高,硬化时间短的加速硅棒胶水硬化的方法。
本发明为实现上述目的,采用如下技术方案:
一种加速硅棒胶水硬化的方法,包括下述步骤:
(1)将晶托冶具、玻璃基板、硅棒依次定位在粘棒推车上,用胶水将各部件粘结在一起;
(2)将粘结好的各个部件连同粘棒推车推入硅棒加热器,所述加热箱加热部件位于箱体周边,底部悬空,底部两侧设置有轨道,所述粘棒推车可以推入轨道,粘棒推车和所述加热箱配合形成一个仅可容纳粘结好的硅棒、玻璃基板和晶托冶具的密闭加热空间,对粘结好的各个部件进行加热;
(3)设定烘箱温度50-60度,加热20-40分钟后,将粘棒推车拉出,更换另外的粘棒推车,进行加热硬化;
(4)将加热后拉出的粘棒推车上的硅棒自然冷却至室温,完成胶水的硬化。
本发明方法,大大缩短的胶水硬化的时间,含加热时间只需2.5小时,提高了工作效率,加快的硅棒粘结场地硅棒的周转速度。同时通过合理的温度和时间的控制,利用特制的加热器,使得加热所需电能消耗也较少,达到了能源消耗和工作效率提高的平衡点。
附图说明
图 1 为本发明硅棒加热器和粘棒推车配合示意图;
图中,1、硅棒加热器;2、粘棒推车;3、轨道。
具体实施方式
所示一种加速硅棒胶水硬化的方法,包括下述步骤:
(1)将晶托冶具、玻璃基板、硅棒依次定位在粘棒推车2上,用胶水将各部件粘结在一起;
(2)如图1所示将粘结好的各个部件连同粘棒推车2推入硅棒加热器1,所述加热箱加热部件位于箱体周边,底部悬空,底部两侧设置有轨道3,所述粘棒推车2可以推入轨道3,粘棒推车2和所述加热箱配合形成一个仅可容纳粘结好的硅棒、玻璃基板和晶托冶具的密闭加热空间,对粘结好的各个部件进行加热;
(3)设定烘箱温度50-60度,加热20-40分钟后,将粘棒推车拉出,更换另外的粘棒推车2,进行加热硬化;
(4)将加热后拉出的粘棒推车2上的硅棒自然冷却至室温,完成胶水的硬化。

Claims (1)

1.一种加速硅棒胶水硬化的方法,包括下述步骤:
(1)将晶托冶具、玻璃基板、硅棒依次定位在粘棒推车上,用胶水将各部件粘结在一起;
(2)将粘结好的各个部件连同粘棒推车推入硅棒加热器,所述加热箱加热部件位于箱体周边,底部悬空,底部两侧设置有轨道,所述粘棒推车可以推入轨道,粘棒推车和所述加热箱配合形成一个仅可容纳粘结好的硅棒、玻璃基板和晶托冶具的密闭加热空间,对粘结好的各个部件进行加热;
(3)设定烘箱温度50-60度,加热20-40分钟后,将粘棒推车拉出,更换另外的粘棒推车,进行加热硬化;
(4)将加热后拉出的粘棒推车上的硅棒自然冷却至室温,完成胶水的硬化。
CN201210187730.8A 2012-06-07 2012-06-07 一种加速硅棒胶水硬化的方法 Active CN102921616B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201210187730.8A CN102921616B (zh) 2012-06-07 2012-06-07 一种加速硅棒胶水硬化的方法

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201210187730.8A CN102921616B (zh) 2012-06-07 2012-06-07 一种加速硅棒胶水硬化的方法

Publications (2)

Publication Number Publication Date
CN102921616A true CN102921616A (zh) 2013-02-13
CN102921616B CN102921616B (zh) 2015-01-28

Family

ID=47636623

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201210187730.8A Active CN102921616B (zh) 2012-06-07 2012-06-07 一种加速硅棒胶水硬化的方法

Country Status (1)

Country Link
CN (1) CN102921616B (zh)

Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN2061678U (zh) * 1989-12-29 1990-09-05 北京重型电机厂 带有密封炉门的新型箱式电阻炉
CN101632978A (zh) * 2009-08-09 2010-01-27 江苏新源动力有限公司 双极板涂胶方法
CN101788713A (zh) * 2010-01-19 2010-07-28 武汉凌云光电科技有限责任公司 半导体激光胶水固化装置及应用方法

Patent Citations (3)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN2061678U (zh) * 1989-12-29 1990-09-05 北京重型电机厂 带有密封炉门的新型箱式电阻炉
CN101632978A (zh) * 2009-08-09 2010-01-27 江苏新源动力有限公司 双极板涂胶方法
CN101788713A (zh) * 2010-01-19 2010-07-28 武汉凌云光电科技有限责任公司 半导体激光胶水固化装置及应用方法

Also Published As

Publication number Publication date
CN102921616B (zh) 2015-01-28

Similar Documents

Publication Publication Date Title
CN103668025A (zh) 钛合金高温状态消除应力校正变形热处理工装及工艺
CN102325429B (zh) 一种粘结模块电源的上、下磁芯方法
CN102921616B (zh) 一种加速硅棒胶水硬化的方法
CN102589282B (zh) 磁性材料的烧结装置
CN106984369B (zh) 一种微流控芯片用键合装置
CN104734431A (zh) 一种电机铁芯的制造方法
CN106601987B (zh) 锂离子电池极片的冷却方法及锂离子电池极片冷却装置
CN105225729B (zh) 各向异性导电膜、及覆晶薄膜与柔性电路板的邦定方法
CN206663019U (zh) 一种超硬材料磨具高效粘接装置
CN102886281A (zh) 一种基于pmma及其它聚合物材质的微流控芯片的键合装置
CN104184269B (zh) 电机转子自动装配机的工作方法
CN103583716A (zh) 一种茶叶提香方法
CN108215358A (zh) 一种太阳能电池背板及其制备方法
CN205346279U (zh) 一种便于调节的自动夹装装置
CN204882213U (zh) 一种用于动态加载过程前样品升温的加载结构
CN103158255A (zh) 塑胶件与金属件的装配方法及其装配设备
CN205038540U (zh) 一种制冷片可自动分离复合式控温装置
CN104400452A (zh) 一种高温合金蜂窝零件铣加工夹持方法
CN203457895U (zh) 鞋底烘干机
CN102124358B (zh) 设备测试系统和方法
CN202308011U (zh) 太阳能电池板压合装置
CN103882196A (zh) 对ZG35Mn钢进行正火回火的热处理工艺
CN104465880A (zh) 太阳能电池组件返修装置
KR101116411B1 (ko) 산업용 다공성 수지필터의 전자파 박막 소결방법
CN211599194U (zh) 碳纤维件粘接工装

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
CP01 Change in the name or title of a patent holder

Address after: The new Ximeilu 214000 Jiangsu city of Wuxi province 111-1

Patentee after: WUXI LONGI SILICON MATERIALS Corp.

Address before: The new Ximeilu 214000 Jiangsu city of Wuxi province 111-1

Co-patentee before: LONGI GREEN ENERGY TECHNOLOGY Co.,Ltd.

Patentee before: Wuxi LONGi Silicon Materials Corp.

Co-patentee before: NINGXIA LONGI SILICON MATERIALS Co.,Ltd.

Co-patentee before: YINCHUAN LONGI SILICON MATERIALS Co.,Ltd.

Address after: The new Ximeilu 214000 Jiangsu city of Wuxi province 111-1

Co-patentee after: LONGI GREEN ENERGY TECHNOLOGY Co.,Ltd.

Patentee after: WUXI LONGI SILICON MATERIALS Corp.

Co-patentee after: NINGXIA LONGI SILICON MATERIALS Co.,Ltd.

Co-patentee after: YINCHUAN LONGI SILICON MATERIALS Co.,Ltd.

Address before: The new Ximeilu 214000 Jiangsu city of Wuxi province 111-1

Co-patentee before: XI'AN LONGI SILICON MATERIALS Corp.

Patentee before: Wuxi LONGi Silicon Materials Corp.

Co-patentee before: NINGXIA LONGI SILICON MATERIALS Co.,Ltd.

Co-patentee before: YINCHUAN LONGI SILICON MATERIALS Co.,Ltd.

CP01 Change in the name or title of a patent holder
TR01 Transfer of patent right

Effective date of registration: 20211026

Address after: 710199 no.388 Hangtian Middle Road, Chang'an District, Xi'an City, Shaanxi Province

Patentee after: LONGI GREEN ENERGY TECHNOLOGY Co.,Ltd.

Address before: No. 111-1, Ximei Road, New District, Wuxi City, Jiangsu Province, 214000

Patentee before: WUXI LONGI SILICON MATERIALS Corp.

TR01 Transfer of patent right