Prior art keywords
thermal insulation
unburned attapulgite
insulating brick
unburned
silt
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2012104163846A
Other languages
English (en)
Inventor
许庆华
李学东
李文娟
周浩
许盛英
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
XUYI COUNTY DONGQIANG NEW BUILDING MATERIALS FACTORY
Original Assignee
XUYI COUNTY DONGQIANG NEW BUILDING MATERIALS FACTORY
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by XUYI COUNTY DONGQIANG NEW BUILDING MATERIALS FACTORY filed Critical XUYI COUNTY DONGQIANG NEW BUILDING MATERIALS FACTORY
Priority to CN2012104163846A priority Critical patent/CN102875097A/zh
Publication of CN102875097A publication Critical patent/CN102875097A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Curing Cements, Concrete, And Artificial Stone (AREA)

Abstract

本发明公开了一种免烧凹凸棒河底淤泥保温砖,其技术方案的要点是,免烧凹凸棒河底淤泥保温砖的配料由凹凸棒石粘土尾矿粉、河底淤泥、火山碎屑岩混合物、膨润土尾矿粉、粉煤灰、膨胀珍珠岩和水泥组成。将免烧凹凸棒河底淤泥保温砖的配料经过搅拌,压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,按照水泥制品的常规养护方法养护,28天后包装为免烧凹凸棒河底淤泥保温砖的成品。免烧凹凸棒河底淤泥保温砖具有强度好、保温节能、隔音隔热和防火阻燃的特点。本发明的配料中大量采用各种废弃物,不仅有利于提高资源利用率,变废为宝,还能减少占用土地,保护和净化环境,节省能源,免烧凹凸棒河底淤泥保温砖适用于各种建筑的墙体施工

Description

免烧凹凸棒河底淤泥保温砖
技术领域
本发明涉及建筑材料领域,具体涉及一种免烧凹凸棒河底淤泥保温砖。
背景技术
我国矿产资源80%为共伴生矿,大量有价值资源存留于尾矿之中,尾矿堆存需要占用大量土地。很多尾矿库超期或超负荷使用,甚至违规操作,使尾矿库存在极大的安全隐患,对周边地区的人民财产和生命安全造成严重威胁。
凹凸棒石粘土除含凹凸棒石外,常含有蒙脱石、高岭石、水云母、海泡石、石英、蛋白石及碳酸盐等矿物。
我国为治理港口、航道、湖泊及河流水体的水质恶化,大多是采取疏浚工程,疏浚工程所产生的河底淤泥量日益增加,组成成分复杂,容易产生二次污染,处理不当将对环境造成极为不利的影响,因而对疏浚河底淤泥的处理就成了人们普遍关注的问题。
与凹凸棒石粘土矿共生的还有火山碎屑岩,火山碎屑岩大多在凹凸棒石粘土矿的上层,有的凹凸棒石粘土矿区上层的火山碎屑岩矿层的厚度高达数十米,凹凸棒石粘土在开采过程中,凹凸棒石粘土矿区上层的火山碎屑岩作为废弃物抛弃,据实地考察,每开采1吨凹凸棒石粘土产生的火山碎屑岩有30吨以上,按年产15万吨的产量计算,产生的火山碎屑岩高达450万吨,多年来都没有能得到利用,整个矿区到处是重新堆积的火山碎屑岩混合物,造成严重的资源浪费和经济损失。
粉煤灰是从煤燃烧后的烟气中收捕下来的细灰,粉煤灰也是燃煤电厂排出的主要固体废物,是我国当前排量较大的工业废渣之一,随着电力工业的发展,燃煤电厂的粉煤灰排放量逐年增加。大量的粉煤灰不加处理,就会产生扬尘,污染大气;若排入水系会造成河流淤塞,其中的有毒化学物质还会对人体和生物造成危害。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种免烧凹凸棒河底淤泥保温砖。
免烧凹凸棒河底淤泥保温砖的配料由凹凸棒石粘土尾矿粉、河底淤泥、火山碎屑岩混合物、膨润土尾矿粉、粉煤灰、膨胀珍珠岩和水泥组成。免烧凹凸棒河底淤泥保温砖的生产方法:将免烧凹凸棒河底淤泥保温砖的配料经过搅拌,压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,按照水泥制品的常规养护方法养护,28天后包装为免烧凹凸棒河底淤泥保温砖的成品。
凹凸棒石粘土是一种层链状结构的含水富镁铝硅酸盐粘土矿物,凹凸棒石粘土土质细腻,吸水性强,湿时具粘性和可塑性,有利于原料之间的粘结,并能提高免烧凹凸棒河底淤泥保温砖的强度和孔隙率。
凹凸棒石粘土在开采过程中会混杂有一定量的碎石和泥土,无法进行筛分,作为一种尾矿抛弃,造成大量的资源浪费,本发明选用粉碎后的凹凸棒石粘土尾矿粉,颗粒细度≤0.149毫米。
河底淤泥是疏浚港口、航道、湖泊及河流等工程中已经抛弃或集中堆放的淤泥,本发明选用的河底淤泥含水率小于20%,颗粒细度≤5.0毫米。
火山碎屑岩是介于岩浆熔岩和沉积岩之间的过渡类型的岩石,其中50%以上的成分是由火山碎屑流喷出的物质组成,这些火山碎屑主要是火山上早期凝固的熔岩、通道周围在火山喷发时被炸裂的岩石形成的。火山碎屑岩混合物包括岩屑、晶屑、玻璃质屑、浆屑、火山块、火山砾和火山灰,火山碎屑岩能增加免烧凹凸棒河底淤泥保温砖的强度,本发明选用粉碎后的火山碎屑岩混合物,颗粒细度≤3.0毫米。
膨润土具有可塑性和黏结性,本发明选用的膨润土尾矿大多分布在凹凸棒石粘土矿的下层,很难进行独立开采,质量也较差,大部分被抛弃于尾矿区,本发明选用粉碎后的膨润土尾矿粉,颗粒细度≤0.25毫米。
粉煤灰能增加免烧凹凸棒河底淤泥保温砖的孔隙率,本发明选用粉碎后的粉煤灰,颗粒细度≤0.25毫米。
膨胀珍珠岩是珍珠岩矿砂经预热,瞬时高温焙烧膨胀后制成的一种内部为蜂窝状结构的白色颗粒状的材料。膨胀珍珠岩具有表观密度轻、导热系数低、化学稳定性好、使用温度范围广、吸湿能力小、无毒、无味、防火和吸音等特点,本发明选用粉碎后膨胀珍珠岩的颗粒细度≤0.25毫米。
水泥选用硅酸盐水泥。
本发明通过下述技术方案予以实现:
1、免烧凹凸棒河底淤泥保温砖的配料按重量百分比由下列组分组成:凹凸棒石粘土尾矿粉2~20%、河底淤泥15~35%、火山碎屑岩混合物5~20%、膨润土尾矿粉5~15%、粉煤灰2~15%、膨胀珍珠岩1~15%、水泥5~15%和水10~30%; 
所述免烧凹凸棒河底淤泥保温砖的生产方法:将免烧凹凸棒河底淤泥保温砖的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输送到全自动砌块成型机中,压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,按照水泥制品的常规养护方法进行养护,28天后包装为免烧凹凸棒河底淤泥保温砖的成品;
所述压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,是指根据设计需要,压制成正方形、长方形、三角形、椭圆形、梯形、梅花形、菱形的免烧凹凸棒河底淤泥保温砖半成品。
免烧凹凸棒河底淤泥保温砖具有强度好、保温节能、隔音隔热和防火阻燃的特点。
免烧凹凸棒河底淤泥保温砖的配料中大量采用各种废弃物,不仅有利于提高资源利用率,变废为宝,还能减少占用土地,保护和净化环境,节省能源,降低生产成本,提高经济效益。
免烧凹凸棒河底淤泥保温砖适用于各种建筑的墙体施工
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、免烧凹凸棒河底淤泥保温砖的配料按重量百分比由下列组分组成:凹凸棒石粘土尾矿粉12%、河底淤泥28%、火山碎屑岩混合物10%、膨润土尾矿粉8%、粉煤灰5%、膨胀珍珠岩3%、水泥9%和水25%; 
所述免烧凹凸棒河底淤泥保温砖的生产方法:将免烧凹凸棒河底淤泥保温砖的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输送到全自动砌块成型机中,压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,按照水泥制品的常规养护方法进行养护,28天后包装为免烧凹凸棒河底淤泥保温砖的成品;
所述压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,是指根据设计需要,压制成长方形的免烧凹凸棒河底淤泥保温砖半成品。

Claims (1)

1.一种免烧凹凸棒河底淤泥保温砖,其特征在于,免烧凹凸棒河底淤泥保温砖的配料按重量百分比由下列组分组成:凹凸棒石粘土尾矿粉2~20%、河底淤泥15~35%、火山碎屑岩混合物5~20%、膨润土尾矿粉5~15%、粉煤灰2~15%、膨胀珍珠岩1~15%、水泥5~15%和水10~30%; 
所述免烧凹凸棒河底淤泥保温砖的生产方法:将免烧凹凸棒河底淤泥保温砖的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输送到全自动砌块成型机中,压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,按照水泥制品的常规养护方法进行养护,28天后包装为免烧凹凸棒河底淤泥保温砖的成品;
所述压制成不同形状的免烧凹凸棒河底淤泥保温砖半成品,是指根据设计需要,压制成正方形、长方形、三角形、椭圆形、梯形、梅花形、菱形的免烧凹凸棒河底淤泥保温砖半成品。
CN2012104163846A 2012-10-27 2012-10-27 免烧凹凸棒河底淤泥保温砖 Pending CN102875097A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN2012104163846A CN102875097A (zh) 2012-10-27 2012-10-27 免烧凹凸棒河底淤泥保温砖

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN2012104163846A CN102875097A (zh) 2012-10-27 2012-10-27 免烧凹凸棒河底淤泥保温砖

Publications (1)

Publication Number Publication Date
CN102875097A true CN102875097A (zh) 2013-01-16

Family

ID=47476661

Family Applications (1)

Application Number Title Priority Date Filing Date
CN2012104163846A Pending CN102875097A (zh) 2012-10-27 2012-10-27 免烧凹凸棒河底淤泥保温砖

Country Status (1)

Country Link
CN (1) CN102875097A (zh)

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107032683A (zh) * 2017-06-05 2017-08-11 合肥永泰新型建材有限公司 一种节能环保砖及制备方法
CN107226666A (zh) * 2017-06-06 2017-10-03 肥西县碧涛建材有限公司 一种高强度保温墙砖及其制备方法
CN108218315A (zh) * 2018-01-10 2018-06-29 和县明生环保材料有限责任公司 一种墙体自保温砖的制备方法
CN109293313A (zh) * 2018-11-24 2019-02-01 深圳市深广通环保建材有限公司 一种淤泥砖及其制备工艺

Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102503516A (zh) * 2011-11-10 2012-06-20 许庆华 免烧碎石形凹凸棒河底淤泥陶粒

Patent Citations (1)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102503516A (zh) * 2011-11-10 2012-06-20 许庆华 免烧碎石形凹凸棒河底淤泥陶粒

Cited By (4)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN107032683A (zh) * 2017-06-05 2017-08-11 合肥永泰新型建材有限公司 一种节能环保砖及制备方法
CN107226666A (zh) * 2017-06-06 2017-10-03 肥西县碧涛建材有限公司 一种高强度保温墙砖及其制备方法
CN108218315A (zh) * 2018-01-10 2018-06-29 和县明生环保材料有限责任公司 一种墙体自保温砖的制备方法
CN109293313A (zh) * 2018-11-24 2019-02-01 深圳市深广通环保建材有限公司 一种淤泥砖及其制备工艺

Similar Documents

Publication Publication Date Title
CN102875097A (zh) 免烧凹凸棒河底淤泥保温砖
CN102887684B (zh) 免烧凹凸棒粉煤灰陶粒保温砖
CN102863204A (zh) 凹凸棒粉煤灰陶粒保温砖
CN102875125B (zh) 凹凸棒河底淤泥保温砖
CN102910877A (zh) 凹凸棒页岩粉煤灰空心砌块
CN102910895B (zh) 凹凸棒页岩河底淤泥烧结保温砖
CN102887687B (zh) 免烧凹凸棒粉煤灰保温砖
CN102887688B (zh) 免烧凹凸棒粉煤灰保温板的生产方法
CN102875080B (zh) 免烧凹凸棒河底淤泥保温板的生产方法
CN102924016B (zh) 凹凸棒页岩河底淤泥空心砌块
CN102875079B (zh) 免烧凹凸棒粉煤灰陶粒保温板的生产方法
CN102863196B (zh) 免烧凹凸棒耐火陶粒保温砖
CN102887685B (zh) 免烧凹凸棒河底淤泥陶粒保温砖
CN102924055B (zh) 凹凸棒页岩河底淤泥烧结多孔砖
CN102875098B (zh) 免烧凹凸棒河底淤泥陶粒保温板的生产方法
CN102992706B (zh) 免烧凹凸棒建筑垃圾保温板
CN102887686B (zh) 免烧凹凸棒建筑垃圾陶粒保温砖
CN102898122B (zh) 凹凸棒页岩河底淤泥陶粒空心砌块
CN102910925B (zh) 凹凸棒页岩耐火空心砌块
CN102924056B (zh) 凹凸棒页岩河底淤泥陶粒烧结多孔砌块
CN102924008B (zh) 凹凸棒页岩粉煤灰陶粒空心砌块
CN102910876B (zh) 凹凸棒页岩建筑垃圾空心砌块
CN102875102B (zh) 免烧凹凸棒耐火陶粒保温板的生产方法
CN102875194B (zh) 凹凸棒河底淤泥保温板的生产方法
CN102924051B (zh) 凹凸棒页岩河底淤泥烧结保温砌块

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20130116