CN102863236A CN2012103731616A CN201210373161A CN102863236A CN 102863236 A CN102863236 A CN 102863236A CN 2012103731616 A CN2012103731616 A CN 2012103731616A CN 201210373161 A CN201210373161 A CN 201210373161A CN 102863236 A CN102863236 A CN 102863236A
Authority
CN
China
Prior art keywords
attapulgite
raw material
material powder
volcanoclastic rock
powder
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Granted
Application number
CN2012103731616A
Other languages
English (en)
Other versions
CN102863236B (zh
Inventor
许庆华
李学东
许盛英
袁长兵
蒋文兰
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong twelfth Cotton Textile Co., Ltd.
Original Assignee
许庆华
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 许庆华 filed Critical 许庆华
Priority to CN 201210373161 priority Critical patent/CN102863236B/zh
Publication of CN102863236A publication Critical patent/CN102863236A/zh
Application granted granted Critical
Publication of CN102863236B publication Critical patent/CN102863236B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Links

Landscapes

  • Silicates, Zeolites, And Molecular Sieves (AREA)

Abstract

本发明公开了一种凹凸棒火山碎屑岩轻质生料粉,其技术方案的要点是,凹凸棒火山碎屑岩轻质生料粉由高粘凹凸棒石粘土粉、凹凸棒石粘土尾矿、火山碎屑岩混合物、硅藻土尾矿、膨胀蛭石和膨润土尾矿组成。将凹凸棒火山碎屑岩轻质生料粉的配料搅拌均匀进行粉碎,包装为凹凸棒火山碎屑岩轻质生料粉的成品。凹凸棒火山碎屑岩轻质生料粉具有气孔率高、体积密度小、高温下体积收缩较小和热导率低的优点。凹凸棒火山碎屑岩轻质生料粉的配料中大量采用各种废弃物,不仅有利于提高资源利用率,变废为宝,还能减少占用土地,保护和净化环境,节省能源,降低生产成本,提高经济效益,凹凸棒火山碎屑岩轻质生料粉适用于耐火保温工程。

Description

凹凸棒火山碎屑岩轻质生料粉
技术领域
本发明涉及耐火材料,具体涉及一种凹凸棒火山碎屑岩轻质生料粉。
背景技术
轻质耐火材料是一种气孔率高、体积密度小、热导率低的耐火材料,在工业窑炉和其他热工设备上用作隔热材料;与一般耐火砖比较,轻质耐火材料抗渣蚀性、力学强度、耐磨损性较差,高温下体积收缩较大。
我国矿产资源80%为共伴生矿,大量有价值资源存留于尾矿之中,尾矿堆存需要占用大量土地。很多尾矿库超期或超负荷使用,甚至违规操作,使尾矿库存在极大的安全隐患,对周边地区的人民财产和生命安全造成严重威胁。
凹凸棒石粘土除含凹凸棒石外,常含有膨润土、高岭石、水云母、海泡石、石英、蛋白石及碳酸盐等矿物。
与凹凸棒石粘土矿共生的还有火山碎屑岩,火山碎屑岩大多在凹凸棒石粘土矿的上层,有的凹凸棒石粘土矿区上层的火山碎屑岩矿层厚度高达数十米,在凹凸棒石粘土在开采过程中,凹凸棒石粘土矿区上层的火山碎屑岩作为废弃物抛弃,据实地考察,每开采1吨凹凸棒石粘土,产生的火山碎屑岩有30吨以上,按年产15万吨的产量计算,产生的火山碎屑岩高达450万吨,多年来都没有能得到利用,整个矿区到处是重新堆积的火山碎屑岩混合物,造成严重的资源浪费和经济损失。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种凹凸棒火山碎屑岩轻质生料粉。
凹凸棒火山碎屑岩轻质生料粉由高粘凹凸棒石粘土粉、凹凸棒石粘土尾矿、火山碎屑岩混合物、硅藻土尾矿、膨胀蛭石和膨润土尾矿组成。
凹凸棒火山碎屑岩轻质生料粉的生产方法:将凹凸棒火山碎屑岩轻质生料粉的配料搅拌均匀进行粉碎,包装为凹凸棒火山碎屑岩轻质生料粉的成品。
凹凸棒石粘土是一种层链状结构的含水富镁铝硅酸盐粘土矿物,凹凸棒石粘土土质细腻,吸水性强,湿时具粘性和可塑性,有利于原料之间的粘结,能提高凹凸棒火山碎屑岩轻质生料粉的附着力。
高粘凹凸棒石粘土粉是指取28.0g凹凸棒石粘土粉试样,加入高速搅拌机的悬浮液杯中,再加入372g水,将悬浮液杯置于高速搅拌机上,在11000转/分钟的转速下搅拌20分钟,再将经过高速搅拌试样悬浮液倒入250ml的烧杯中,使用NDJ-1型旋转粘度计进行测试其悬浮液的粘度,测试粘度值≥2200 mPa·s的凹凸棒石粘土粉为高粘凹凸棒石粘土粉,本发明选用高粘凹凸棒石粘土粉的颗粒细度≤0.074毫米。
凹凸棒石粘土在开采过程中会混杂有一定量的碎石和泥土,作为一种凹凸棒石粘土尾矿抛弃,造成大量的资源浪费,本发明选用凹凸棒石粘土尾矿的颗粒细度≤2.0毫米。
火山碎屑岩是介于岩浆熔岩和沉积岩之间的过渡类型的岩石,其中50%以上的成分是由火山碎屑流喷出的物质组成,这些火山碎屑主要是火山上早期凝固的熔岩、通道周围在火山喷发时被炸裂的岩石形成的。火山碎屑岩混合物包括岩屑、晶屑、玻璃质屑、浆屑、火山块(直径大于100毫米)、火山砾(直径大于2毫米)和火山灰(直径小于2毫米),火山碎屑岩主要化学成分是二氧化硅和氧化铝,具有较好的耐火性能和增加凹凸棒火山碎屑岩轻质生料粉的强度,本发明选用火山碎屑岩混合物的颗粒细度≤5.0毫米。
硅藻土细腻、松散、质轻、多孔,比表面积大,空隙呈有规律分布,化学性质稳定,是一种天然纳米孔径无定形硅质材料,但是硅藻土综合利用率低,多数企业的产品出自于一级土,而二、三级土被大量废弃,造成了资源浪费严重,还污染了环境,本发明选用硅藻土尾矿的颗粒细度≤2.0毫米。
生蛭石片经过高温焙烧后,其体积能迅速膨胀数倍至数十倍,体积膨胀后的蛭石就叫膨胀蛭石,具有很强的保温隔热性能,本发明选用膨胀蛭石的颗粒细度≤2.0毫米。
膨润土主要是由膨润土组成的岩石,是冶金领域重要的矿物原料,本发明选用的膨润土尾矿大多分布在凹凸棒石粘土矿的下层,很难进行独立开采,但是膨润土尾矿中氧化铝的含量≥16%,并具有可塑性和黏结性,本发明选用膨润土尾矿的颗粒细度≤2.0毫米。
本发明通过下述技术方案予以实现:
1、凹凸棒火山碎屑岩轻质生料粉的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉2~12%、凹凸棒石粘土尾矿5~25%、火山碎屑岩混合物15~40%、硅藻土尾矿5~35%、膨胀蛭石2~20%和膨润土尾矿2~15%;
所述凹凸棒火山碎屑岩轻质生料粉的生产方法:将凹凸棒火山碎屑岩轻质生料粉的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输入粉碎机中粉碎为凹凸棒火山碎屑岩轻质生料粉的半成品,凹凸棒火山碎屑岩轻质生料粉半成品的颗粒细度≤0.15毫米,包装为凹凸棒火山碎屑岩轻质生料粉的成品。
凹凸棒火山碎屑岩轻质生料粉具有气孔率高、体积密度小、高温下体积收缩较小和热导率低的优点。
凹凸棒火山碎屑岩轻质生料粉的配料中大量采用各种废弃物,不仅有利于提高资源利用率,变废为宝,还能减少占用土地,保护和净化环境,节省能源,降低生产成本,提高经济效益。
凹凸棒火山碎屑岩轻质生料粉适用于耐火保温工程。
具体实施方式
下面结合实施例对本发明作进一步的描述: 
1、凹凸棒火山碎屑岩轻质生料粉的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉8%、凹凸棒石粘土尾矿14%、火山碎屑岩混合物30%、硅藻土尾矿26%、膨胀蛭石16%和膨润土尾矿6%;
所述凹凸棒火山碎屑岩轻质生料粉的生产方法:将凹凸棒火山碎屑岩轻质生料粉的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输入粉碎机中粉碎为凹凸棒火山碎屑岩轻质生料粉的半成品,凹凸棒火山碎屑岩轻质生料粉半成品的颗粒细度≤0.105毫米,包装为凹凸棒火山碎屑岩轻质生料粉的成品。

Claims (1)

1.一种凹凸棒火山碎屑岩轻质生料粉,其特征在于,凹凸棒火山碎屑岩轻质生料粉的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉2~12%、凹凸棒石粘土尾矿5~25%、火山碎屑岩混合物15~40%、硅藻土尾矿5~35%、膨胀蛭石2~20%和膨润土尾矿2~15%;
所述凹凸棒火山碎屑岩轻质生料粉的生产方法:将凹凸棒火山碎屑岩轻质生料粉的配料加入已经运行的双卧轴强制式搅拌机中搅拌,搅拌均匀后输入粉碎机中粉碎为凹凸棒火山碎屑岩轻质生料粉的半成品,凹凸棒火山碎屑岩轻质生料粉半成品的颗粒细度≤0.15毫米,包装为凹凸棒火山碎屑岩轻质生料粉的成品;
高粘凹凸棒石粘土粉是指取28.0g凹凸棒石粘土粉试样,加入高速搅拌机的悬浮液杯中,再加入372g水,将悬浮液杯置于高速搅拌机上,在11000转/分钟的转速下搅拌20分钟,再将经过高速搅拌试样悬浮液倒入250ml的烧杯中,使用NDJ-1型旋转粘度计进行测试其悬浮液的粘度,测试粘度值≥2200 mPa·s的凹凸棒石粘土粉为高粘凹凸棒石粘土粉,本发明选用高粘凹凸棒石粘土粉的颗粒细度≤0.074毫米。
CN 201210373161 2012-09-30 2012-09-30 凹凸棒火山碎屑岩轻质生料粉 Active CN102863236B (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN 201210373161 CN102863236B (zh) 2012-09-30 2012-09-30 凹凸棒火山碎屑岩轻质生料粉

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN 201210373161 CN102863236B (zh) 2012-09-30 2012-09-30 凹凸棒火山碎屑岩轻质生料粉

Publications (2)

Publication Number Publication Date
CN102863236A true CN102863236A (zh) 2013-01-09
CN102863236B CN102863236B (zh) 2013-10-16

Family

ID=47442407

Family Applications (1)

Application Number Title Priority Date Filing Date
CN 201210373161 Active CN102863236B (zh) 2012-09-30 2012-09-30 凹凸棒火山碎屑岩轻质生料粉

Country Status (1)

Country Link
CN (1) CN102863236B (zh)

Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH10231166A (ja) * 1997-02-18 1998-09-02 Tokyo Yogyo Co Ltd 廃棄物を活用した焼成建材ブロック
CN101007718A (zh) * 2007-01-29 2007-08-01 袁长兵 凹凸棒日光温室保温砖
CN101333083A (zh) * 2008-08-05 2008-12-31 中国建筑材料科学研究总院 一种高性能膨胀性水泥熟料及其制备得到的系列膨胀剂
CN102503323A (zh) * 2011-11-10 2012-06-20 许庆华 免烧圆柱形凹凸棒耐火陶粒
CN102503490A (zh) * 2011-11-10 2012-06-20 许庆华 免烧碎石形凹凸棒耐火陶粒

Patent Citations (5)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
JPH10231166A (ja) * 1997-02-18 1998-09-02 Tokyo Yogyo Co Ltd 廃棄物を活用した焼成建材ブロック
CN101007718A (zh) * 2007-01-29 2007-08-01 袁长兵 凹凸棒日光温室保温砖
CN101333083A (zh) * 2008-08-05 2008-12-31 中国建筑材料科学研究总院 一种高性能膨胀性水泥熟料及其制备得到的系列膨胀剂
CN102503323A (zh) * 2011-11-10 2012-06-20 许庆华 免烧圆柱形凹凸棒耐火陶粒
CN102503490A (zh) * 2011-11-10 2012-06-20 许庆华 免烧碎石形凹凸棒耐火陶粒

Also Published As

Publication number Publication date
CN102863236B (zh) 2013-10-16

Similar Documents

Publication Publication Date Title
CN102863242B (zh) 凹凸棒火山碎屑岩隔热生料粉
CN102863229B (zh) 凹凸棒火山碎屑岩碱性耐火骨料砂
CN102863234B (zh) 凹凸棒火山碎屑岩高铝耐火砖
CN102875120B (zh) 凹凸棒耐火陶粒保温板的生产方法
CN102863228B (zh) 凹凸棒火山碎屑岩隔热耐火砖
CN102863244B (zh) 凹凸棒火山碎屑岩高铝生料粉
CN102863236B (zh) 凹凸棒火山碎屑岩轻质生料粉
CN102863235B (zh) 凹凸棒火山碎屑岩轻质耐火骨料的生产方法
CN102875119B (zh) 凹凸棒耐火陶粒保温砖
CN102863239A (zh) 凹凸棒火山碎屑岩高铝质耐火骨料砂
CN102863246B (zh) 凹凸棒火山碎屑岩轻质耐火骨料砂
CN102951910B (zh) 凹凸棒火山碎屑岩粘土质耐火砖
CN102875164B (zh) 凹凸棒火山碎屑岩硅质耐火砖
CN102863196A (zh) 免烧凹凸棒耐火陶粒保温砖
CN102875172B (zh) 凹凸棒火山碎屑岩隔热耐火骨料的生产方法
CN102875163B (zh) 凹凸棒火山碎屑岩碱性生料粉
CN102875169B (zh) 凹凸棒火山碎屑岩隔热耐火骨料砂
CN102875165B (zh) 凹凸棒火山碎屑岩粘土质生料粉
CN102875167B (zh) 凹凸棒火山碎屑岩轻质熟料粉
CN102863233B (zh) 凹凸棒火山碎屑岩硅质生料粉
CN102863243B (zh) 凹凸棒火山碎屑岩高铝质耐火骨料的生产方法
CN102863240B (zh) 凹凸棒火山碎屑岩轻质耐火砖
CN102898177B (zh) 凹凸棒页岩耐火烧结多孔砖
CN102863241B (zh) 凹凸棒火山碎屑岩碱性耐火骨料的生产方法
CN102863237A (zh) 凹凸棒火山碎屑岩粘土质耐火骨料砂

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C14 Grant of patent or utility model
GR01 Patent grant
ASS Succession or assignment of patent right

Owner name: NANTONG TWELFTH COTTON TEXTILE CO., LTD.

Free format text: FORMER OWNER: XU QINGHUA

Effective date: 20131113

C41 Transfer of patent application or patent right or utility model
COR Change of bibliographic data

Free format text: CORRECT: ADDRESS; FROM: 211700 HUAIAN, JIANGSU PROVINCE TO: 226300 NANTONG, JIANGSU PROVINCE

TR01 Transfer of patent right

Effective date of registration: 20131113

Address after: 226300 Jiangsu city of Nantong province Tongzhou District Stone Town Shimbashi West first

Patentee after: Nantong twelfth Cotton Textile Co., Ltd.

Address before: 211700 Huaian City, Jiangsu province Xuyi County Xu town of Stonebridge Road No. 40

Patentee before: Xu Qinghua