CN102845840A - Dyeing and finishing process of pantyhose fabric - Google Patents
Dyeing and finishing process of pantyhose fabric Download PDFInfo
- Publication number
- CN102845840A CN102845840A CN 201210314350 CN201210314350A CN102845840A CN 102845840 A CN102845840 A CN 102845840A CN 201210314350 CN201210314350 CN 201210314350 CN 201210314350 A CN201210314350 A CN 201210314350A CN 102845840 A CN102845840 A CN 102845840A
- Authority
- CN
- China
- Prior art keywords
- dyeing
- fabric
- treatment
- processing method
- temperature
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention provides a dyeing and finishing process of a pantyhose fabric. The dyeing and finishing process comprises the steps as follows: a) pretreatment of the fabric; b) dyeing treatment of the fabric; and c) final treatment of the fabric. According to the dyeing and finishing process of the pantyhose fabric, the fabric is soft and warm by optimizing and screening process conditions, and arranging the process scientifically and rationally. And meanwhile, the dyeing vapor stains are eliminated, thereby ensuring that the appearance of the pantyhose fabric is attractive, pure and free from the flaws, and meeting the dressing requirements of young women.
Description
Technical field
The present invention relates to a kind of processing method of textile fabric, relate in particular to a kind of dyeing and finishing processing method of panty hose fabric, belong to textile technology field.
Background technology
Day by day raising along with people's living standard and cultural taste, new variation has also occured in the dressing theory, by solid endurable, the warming of traditional emphasis of past to change into current advocate fashion freely, CRUX, Considering Environmental antipollution, health care, comfortable fittingness, random naturally beautiful generous clothes again.As a kind of clothes of women's special use, panty hose just are subjected to numerous women's welcome from the date of birth deeply, and this is a kind of
The clothes of hard-pressed bale from waist to foot's body, it is warming next to the skin, can represent women's graceful stature, deeply is subjected to for many years liking of young woman.The panty hose material is a lot, and cotton, nylon, wool blended etc. are arranged, and the function of panty hose is also a lot, as: sun-proof, prevent varication, prevent oedema etc.
At present, a lot of young woman be unable to do without panty hose throughout the year, as the medium-thick type panty hose, and one of most popular kind of time of the year when autumn changes into winter especially.But, the medium-thick type panty hose easily produces many problems in dyeing and finishing process, especially vapour spot problem dyes, not only have a strong impact on product quality and taken performance, also reduced production efficiency and the profit of enterprise, therefore, be necessary the production technology of this type of yarn fabric is optimized improvement, thereby overcome dyeing color spot problem, improve the quality of taking of fabric.
Summary of the invention
For the demand, the invention provides a kind of dyeing and finishing processing method of panty hose fabric, by optimizing the screening technology condition, scientific and reasonable arrangement operation, make not only soft warming of panty hose fabric, and eliminated dyeing vapour class, and guaranteed that the outward appearance of panty hose fabrics is pure and beautiful indefectible, satisfied young woman's the demand of wearing.
The present invention is a kind of dyeing and finishing processing method of panty hose fabric, and this dyeing and finishing processing method comprises the steps: a) fabric pretreatment, and b) c) fabric post processing is processed in textile dyeing.
In a preferred embodiment of the present invention, in the described step a), fabric pretreatment technique comprises: preboarding, preshrunk and pre-treatment; Wherein, preboarding is adopted and is intervened setting, and its setting temperature is 94 ℃~96 ℃, and fixing time is 20~22s; During preshrunk, first 0.095Mpa vacuumizes 6~8min, preshrunk 20~25min then, and the preshrunk temperature is 105~108 ℃, 0.095Mpa vacuumizes 6~8min again.
In a preferred embodiment of the present invention, 1.8~2.1g/L deoil refining agent and 1.5~1.8g/L soda ash have been selected in described pre-treatment, and bath raio is 1:15~1:25, and temperature retention time is 30~40min; During pre-treatment, fabric immersed in the body lotion and with 1.5~2 ℃/min rise to 98 ℃, after insulation, again discharge opeing, washing, then standby dying.
In a preferred embodiment of the present invention, in the described step b), the textile dyeing treatment process comprises dyeing, washing and fixation; Wherein, acidity and neutral dye have been selected in dyeing, 0.5~0.8g/L levelling agent, 2~5g/L softening agent and 5~10g/L ammonium sulfate, and bath raio is 1:15~1:20, the insulation dyeing time is 45~60min; During dyeing, fabric is at room temperature entered to dye, and rise to 98 ℃ with 1 ℃/min, after insulation, again discharge opeing, washing.
In a preferred embodiment of the present invention, described fixation treatment has been selected 3~5% nylon color-fixing agent BFN and 0.3~0.5g/L acetic acid, and bath raio is 1:15~1:20, and color fixing temperature is 70~80 ℃, and the fixation time is 40~45min.
In a preferred embodiment of the present invention, in the described step c), the fabric aftertreatment technology comprises soft and the setting oven dry; Wherein, during soft treatment, selected 1.5~2.5% softening agents, 1.8~2.1% antistatic additive and 0.2~0.3g/L acetic acid, bath raio is 1:10~1:15, and temperature is 50~60 ℃, and the time is 20~25min; Fabric setting bake out temperature is 80~100 ℃.
The present invention has disclosed a kind of dyeing and finishing processing method of panty hose fabric, by optimizing the screening technology condition, scientific and reasonable arrangement operation, make not only soft warming of panty hose fabric, and eliminated dyeing vapour class, the outward appearance that has guaranteed the panty hose fabrics is pure and beautiful indefectible, has satisfied young woman's the demand of wearing.
Description of drawings
The present invention is further detailed explanation below in conjunction with the drawings and specific embodiments:
Fig. 1 is the process figure of embodiment of the invention panty hose fabric finishing processing technology.
The specific embodiment
Below in conjunction with accompanying drawing preferred embodiment of the present invention is described in detail, thereby so that advantages and features of the invention can be easier to be it will be appreciated by those skilled in the art that protection scope of the present invention is made more explicit defining.
Fig. 1 is the process figure of embodiment of the invention panty hose fabric finishing processing technology; This dyeing and finishing processing method comprises the steps: a) fabric pretreatment, and b) c) fabric post processing is processed in textile dyeing.
Embodiment 1
The implementation step is as follows:
A) fabric pretreatment, fabric pretreatment technique comprises: preboarding, preshrunk and pre-treatment; Wherein, preboarding is adopted and is intervened setting, and its setting temperature is 95 ℃, and fixing time is 20s; During preshrunk, first 0.095Mpa vacuumizes 7min, preshrunk 20min then, and the preshrunk temperature is 105 ℃, 0.095Mpa vacuumizes 7min again;
Because fabric carries out first preboarding, after carry out High Temperature Pre contracting, and the preshrunk temperature is higher than again the preboarding temperature, therefore preferably resolve the problem of dyeing color spot, even preboarding has caused fabric vapour spot, make the local-crystalized degree of the fiber that the vapour spot occurs different, but temperature conditions and the preshrunk of long period higher in follow-up preshrunk vacuumize under the condition, or can be tending towards balanced unified, during dyeing, the dye-uptake of each several part fiber can reach relatively consistent state, so fabric the color spot that dyes can not occur; 1.8g/L deoil refining agent and 1.5g/L soda ash have been selected in pre-treatment, and bath raio is 1:20, and temperature retention time is 35min; During pre-treatment, fabric immersed in the body lotion and with 1.5 ℃/min rise to 98 ℃, after insulation, again discharge opeing, washing, then standby dying.
B) textile dyeing is processed, and the textile dyeing treatment process comprises dyeing, washing and fixation; Wherein, acidity and neutral dye have been selected in dyeing, 0.6g/L levelling agent, 3g/L softening agent and 6g/L ammonium sulfate, and bath raio is 1:15, the insulation dyeing time is 50min; During dyeing, fabric is at room temperature entered to dye, and rise to 98 ℃ with 1 ℃/min, after insulation, again discharge opeing, washing; Fixation treatment has been selected 3% nylon color-fixing agent BFN and 0.3g/L acetic acid, and bath raio is 1:15, during fixation, will color-fixing agent squeeze in the overflow dyeing machine after the dilution, is warming up to 75 ℃, insulation fixation 40min, again discharge opeing washing with the speed of 1.5 ℃/min.
C) fabric post processing, fabric aftertreatment technology comprise soft and the setting oven dry; Wherein, during soft treatment, selected 1.5% softening agent, 1.8% antistatic additive and 0.2g/L acetic acid, bath raio is 1:10, after fabric washing is clean, in overflow dyeing machine, add softening agent and antistatic additive, be warming up to 55 ℃, soft 20min with the speed of 1.5 ℃/min, go out again the machine dehydration, the oven dry that formalizes at last, bake out temperature is 85 ℃, the time is as the criterion with oven dry.
Embodiment 2
The implementation step is as follows:
A) fabric pretreatment, fabric pretreatment technique comprises: preboarding, preshrunk and pre-treatment; Wherein, preboarding is adopted and is intervened setting, and its setting temperature is 96 ℃, and fixing time is 22s; During preshrunk, first 0.095Mpa vacuumizes 8min, preshrunk 25min then, and the preshrunk temperature is 107 ℃, 0.095Mpa vacuumizes 8min again;
Because fabric carries out first preboarding, after carry out High Temperature Pre contracting, and the preshrunk temperature is higher than again the preboarding temperature, therefore preferably resolve the problem of dyeing color spot, even preboarding has caused fabric vapour spot, make the local-crystalized degree of the fiber that the vapour spot occurs different, but temperature conditions and the preshrunk of long period higher in follow-up preshrunk vacuumize under the condition, or can be tending towards balanced unified, during dyeing, the dye-uptake of each several part fiber can reach relatively consistent state, so fabric the color spot that dyes can not occur; 2g/L deoil refining agent and 1.8g/L soda ash have been selected in pre-treatment, and bath raio is 1:25, and temperature retention time is 40min; During pre-treatment, fabric immersed in the body lotion and with 2 ℃/min rise to 98 ℃, after insulation, again discharge opeing, washing, then standby dying.
B) textile dyeing is processed, and the textile dyeing treatment process comprises dyeing, washing and fixation; Wherein, acidity and neutral dye have been selected in dyeing, 0.8g/L levelling agent, 4g/L softening agent and 7g/L ammonium sulfate, and bath raio is 1:20, the insulation dyeing time is 60min; During dyeing, fabric is at room temperature entered to dye, and rise to 98 ℃ with 1 ℃/min, after insulation, again discharge opeing, washing; Fixation treatment has been selected 4% nylon color-fixing agent BFN and 0.5g/L acetic acid, and bath raio is 1:20, during fixation, will color-fixing agent squeeze in the overflow dyeing machine after the dilution, is warming up to 80 ℃, insulation fixation 45min, again discharge opeing washing with the speed of 1.5 ℃/min.
C) fabric post processing, fabric aftertreatment technology comprise soft and the setting oven dry; Wherein, during soft treatment, selected 2% softening agent, 2% antistatic additive and 0.3g/L acetic acid, bath raio is 1:15, after fabric washing is clean, in overflow dyeing machine, add softening agent and antistatic additive, be warming up to 60 ℃, soft 25min with the speed of 1.5 ℃/min, go out again the machine dehydration, the oven dry that formalizes at last, bake out temperature is 95 ℃, the time is as the criterion with oven dry.
The present invention has disclosed a kind of dyeing and finishing processing method of panty hose fabric, by optimizing the screening technology condition, scientific and reasonable arrangement operation, make not only soft warming of panty hose fabric, and eliminated dyeing vapour class, the outward appearance that has guaranteed the panty hose fabrics is pure and beautiful indefectible, has satisfied young woman's the demand of wearing.
The above; it only is the specific embodiment of the present invention; but protection scope of the present invention is not limited to this; any those of ordinary skill in the art are in the disclosed technical scope of the present invention; variation or the replacement that can expect without creative work all should be encompassed within protection scope of the present invention.Therefore, protection scope of the present invention should be as the criterion with the protection domain that claims were limited.
Claims (6)
1. the dyeing and finishing processing method of a panty hose fabric is characterized in that, this dyeing and finishing processing method comprises the steps: a) fabric pretreatment, and b) c) fabric post processing is processed in textile dyeing.
2. the dyeing and finishing processing method of panty hose fabric according to claim 1 is characterized in that, in the described step a), fabric pretreatment technique comprises: preboarding, preshrunk and pre-treatment; Wherein, preboarding is adopted and is intervened setting, and its setting temperature is 94 ℃~96 ℃, and fixing time is 20~22s; During preshrunk, first 0.095Mpa vacuumizes 6~8min, preshrunk 20~25min then, and the preshrunk temperature is 105~108 ℃, 0.095Mpa vacuumizes 6~8min again.
3. the dyeing and finishing processing method of panty hose fabric according to claim 2 is characterized in that, 1.8~2.1g/L deoil refining agent and 1.5~1.8g/L soda ash have been selected in described pre-treatment, and bath raio is 1:15~1:25, and temperature retention time is 30~40min; During pre-treatment, fabric immersed in the body lotion and with 1.5~2 ℃/min rise to 98 ℃, after insulation, again discharge opeing, washing, then standby dying.
4. the dyeing and finishing processing method of panty hose fabric according to claim 1 is characterized in that, in the described step b), the textile dyeing treatment process comprises dyeing, washing and fixation; Wherein, acidity and neutral dye have been selected in dyeing, 0.5~0.8g/L levelling agent, 2~5g/L softening agent and 5~10g/L ammonium sulfate, and bath raio is 1:15~1:20, the insulation dyeing time is 45~60min; During dyeing, fabric is at room temperature entered to dye, and rise to 98 ℃ with 1 ℃/min, after insulation, again discharge opeing, washing.
5. the dyeing and finishing processing method of panty hose fabric according to claim 4, it is characterized in that, described fixation treatment has been selected 3~5% nylon color-fixing agent BFN and 0.3~0.5g/L acetic acid, and bath raio is 1:15~1:20, color fixing temperature is 70~80 ℃, and the fixation time is 40~45min.
6. the dyeing and finishing processing method of panty hose fabric according to claim 1 is characterized in that, in the described step c), the fabric aftertreatment technology comprises soft and the setting oven dry; Wherein, during soft treatment, selected 1.5~2.5% softening agents, 1.8~2.1% antistatic additive and 0.2~0.3g/L acetic acid, bath raio is 1:10~1:15, and temperature is 50~60 ℃, and the time is 20~25min; Fabric setting bake out temperature is 80~100 ℃.