CN1028090C - 一种粉煤灰微肥的生产方法 - Google Patents

一种粉煤灰微肥的生产方法 Download PDF

Info

Publication number
CN1028090C
CN1028090C CN89106627A CN89106627A CN1028090C CN 1028090 C CN1028090 C CN 1028090C CN 89106627 A CN89106627 A CN 89106627A CN 89106627 A CN89106627 A CN 89106627A CN 1028090 C CN1028090 C CN 1028090C
Authority
CN
China
Prior art keywords
fertilizer
flyash
trace element
pyrolusite
borax
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN89106627A
Other languages
English (en)
Other versions
CN1043691A (zh
Inventor
石振鑫
冯斌
王德才
党战海
刘占祥
Original Assignee
石振鑫
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 石振鑫 filed Critical 石振鑫
Priority to CN89106627A priority Critical patent/CN1028090C/zh
Publication of CN1043691A publication Critical patent/CN1043691A/zh
Application granted granted Critical
Publication of CN1028090C publication Critical patent/CN1028090C/zh
Anticipated expiration legal-status Critical
Expired - Fee Related legal-status Critical Current

Abstract

本发明涉及一种粉煤灰微肥的生产方法,它主要是利用工业废渣粉煤灰与破碎后的硼砂,闪锌矿石,软锰矿石,根据需要按一定比例分别混合或全部混合,经高温锻烧生产出含微量元素的粉煤灰微肥,它可大大提高了肥效,易于被植物吸收,在土壤中不易流失,起到了变废为宝的作用。

Description

本发明涉及一种粉煤灰微肥的生产方法,特别涉及一种用粉煤灰、硼砂、闪锌矿、软锰矿生产粉煤灰微肥的方法。
现有技术中,微量元素因是植株体内的酶或辅酶的组成部分,具有作物生长发育不可缺少的作用,由于微量元素易被土壤固定,所以往土壤里施用微量元素,其肥效不易充分发挥,为了提高肥效,目前国内外研制和试用各种形式的微肥,例如:将玻璃与微量元素一起熔融制成玻璃肥,这些肥料或者制备工艺复杂,要求严格,成本高,或者释放过缓,肥效慢,或者在阳光照射雨水冲刷下,微量元素损失严重,其肥效很低,另外,粉煤灰是热电厂燃烧煤粉所产生的灰渣,其中,所含营养元素(包括微量元素)低,因此肥效不高。
本发明的目的在于:提供一种肥效长,易被植物吸收,稳定的粉煤灰微肥的生产方法,
为了实现上述目的,本发明采用了新的方法生产结晶微量元素肥料,具体方法是:以火力发电厂锅炉废渣……粉煤灰作主要原料,然后将含有微量元素的硼砂、闪锌矿石、软锰矿石破碎,制成细小颗粒,根据需要按一定比例分别将其部分或全部含微量元素的原料与粉煤灰混合入窑,在温度1300℃-1600℃高温下,锻烧成为含微量元素硼,微量元素锌、微量元素锰,或含微量元素的粉煤灰微肥。
本发明所采用的上述四种原料范围如下:(配料时根据所需肥料或是每种原料单独与粉煤灰混合锻烧,或是三种原料全部与粉煤灰混合锻烧)。
名称    重量百分比
粉煤灰    90~98
硼砂    2~10
闪锌矿    2~10
软锰矿    1~5
采用以上方法生产出的结晶硅酸盐微量元素硼肥,结晶硅酸盐微量元素锌肥,结晶硅酸盐微量元素锰肥,结晶硅酸盐微量元素肥料由于是结晶状的肥料,在土壤里不易流失,而且这些肥料施在地里与土壤根系分泌出的有机酸发生反应,变成可溶性的盐类,易于被植物吸收利用;肥效高,安全可靠,而且利用粉煤灰这种工业废渣生产化肥起到了变废为宝,消除公害的作用,可使谷物、亚麻、棉花、蔬菜、果树等增产生10%~50%,是一种安全理想的肥料。
下面是本发明的具体实施方式:
实施方式1:硼砂经粉碎后,制成细小颗粒取8份(按重量计,下同),粉煤灰取92份,充分搅拌混合均匀,喂入窑内,在温度为1300℃-1600℃时锻烧成熔融体,再制成粉状,即成含硼的粉煤灰微肥。
实施方式2:闪锌矿石经粉碎后,制成细小颗粒取8份(按重量计,下同),粉煤灰取92份,充分搅拌混合均匀,喂入窑内,在温度为1300℃-1600℃时锻烧成熔融体,再制成粉状,即成含锌的粉煤灰微肥。
实施方式3:软锰矿石经粉碎后,制成细小颗粒取2份(按重量计,下同),粉煤灰取98份,充分搅拌混合均匀,喂入窑内,在温度为1300℃-1600℃时锻烧成熔融体,再制成粉状,即成含硼的粉煤灰微肥。
实施方式4:硼砂闪锌矿石软锰矿石经粉碎后,制成细小颗粒,取硼砂4份(按重量计,下同),闪锌矿石3份,软锰矿石1份,粉煤灰取92份,充分搅拌混合均匀,喂入窑内,在温度为1300℃-1600℃时锻烧成熔融体,再制成粉状,即成含硼锌锰的粉煤灰微肥。

Claims (1)

1、一种粉煤灰微肥的生产方法,其特征在于:将硼砂、闪锌矿石、软锰矿石粉碎后,按下述配比(以重量计)分别将其部分或全部上述原料与粉煤灰搅拌混合均匀,再在温度为1300℃-1600℃下锻炼,最后制成粉状:
(1)粉煤灰  90~98
   硼砂    2~10
(2)粉煤灰  95~98
   软锰矿  2~5
(3)粉煤灰  90~98
   闪锌粉  2~10
(4)粉煤灰  92
   硼砂    4
   闪锌矿  3
   软锰矿  1
CN89106627A 1989-09-02 1989-09-02 一种粉煤灰微肥的生产方法 Expired - Fee Related CN1028090C (zh)