CN102642014A - 铸造金属模具加热装置 - Google Patents
铸造金属模具加热装置 Download PDFInfo
- Publication number
- CN102642014A CN102642014A CN2011100417976A CN201110041797A CN102642014A CN 102642014 A CN102642014 A CN 102642014A CN 2011100417976 A CN2011100417976 A CN 2011100417976A CN 201110041797 A CN201110041797 A CN 201110041797A CN 102642014 A CN102642014 A CN 102642014A
- Authority
- CN
- China
- Prior art keywords
- cast metal
- gas pipe
- mould
- housing
- die
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种铸造金属模具加热装置,包括外框和燃气管,以使用方向为基准,外框呈上下开口的中空筒状体,燃气管一端伸入外框内,燃气管内通有可燃气体,所述外框恰能够插置于铸造金属模具的上、下模之间,伸入外框内的燃气管上下两侧均设有若干出气孔,本发明直接在铸造金属模具的上、下模之间对上、下模的模腔进行直接加热,上、下模的模腔升温快,加热均匀,提高了加热效果,且由于外框位于上、下模之间,其保温性好,热量不易外散,使得模具加热速度更快,有效提高生产效率。
Description
技术领域
本发明涉及一种铸造金属模具辅助装置,尤其是一种铸造金属模具加热装置。
背景技术
铸造金属模具在铸造成型前需要对模具进行预热处理,目前常用的方法是在模具整体外侧套设一个外框,外框内放置燃气管,燃气管也套设在模具整体外侧,燃气管朝向模具一侧开有出气孔,出气孔喷火对模具进行加热,然而这种预加热方式是火焰在模具外侧对模具加热,一方面热量容易外扩散热到外侧空间中,另一方面模具的模腔内加热速度慢,加热不均匀,影响模具预热效果同时因加热速度慢,导致生产效率低。
发明内容
为了克服上述缺陷,本发明提供一种铸造金属模具加热装置,该铸造金属模具加热装置结构简单,能够对铸造金属模具进行快速均匀的加热。
本发明为了解决其技术问题所采用的技术方案:一种铸造金属模具加热装置,包括外框和燃气管,以使用方向为基准,外框呈上下开口的中空筒状体,燃气管一端伸入外框内,燃气管内通有可燃气体,所述外框恰能够插置于铸造金属模具的上、下模之间,伸入外框内的燃气管上下两侧均设有若干出气孔,当铸造金属模具处于开模状态时,将加热装置放置在上、下模之间,燃气管上下两侧的出气孔就分别向上、下模喷火对上、下模的模腔同时加热,上、下模的模腔内温度在短时间内迅速升至设定温度,这样就可以缩短铸造过程中模具的加热准备时间,提高生产效率。
作为本发明的进一步改进,所述铸造金属模具的上、下模恰完全覆盖于外框上下两侧,即外框径向尺寸小于等于上、下模径向尺寸,保证燃气管喷出的所有火力都喷射在上下模的模腔内,热量不易扩散,从而达到集中加热的效果。
作为本发明的进一步改进,所述燃气管伸入到外框内的一端呈环形结构,增大火焰与上、下模的加热面积,使加热均匀、快速。
作为本发明的进一步改进,所述燃气管内的可燃气体为天然气和空气的混合气体,保证可燃气体充分燃烧。
作为本发明的进一步改进,所述外框上、下两端的开口内径大于中间内径。
本发明的有益效果是:本发明直接在铸造金属模具的上、下模之间对上、下模的模腔进行直接加热,上、下模的模腔升温快,加热均匀,提高了加热效果,且由于外框位于上、下模之间,其保温性好,热量不易外散,使得模具加热速度更快,有效提高生产效率。
附图说明
图1为本发明结构原理示意图;
图2为图1中A-A向剖视图;
图3为本发明的使用状态示意图。
具体实施方式
实施例:一种铸造金属模具加热装置,包括外框1和燃气管2,以使用方向为基准,外框1呈上下开口的中空筒状体,燃气管2一端伸入外框1内,燃气管2内通有可燃气体,所述外框1恰能够插置于铸造金属模具的上、下模之间,伸入外框1内的燃气管2上下两侧均设有若干出气孔3,当铸造金属模具处于开模状态时,将加热装置放置在上、下模之间,燃气管2上下两侧的出气孔3就分别向上、下模喷火对上、下模的模腔同时加热,上、下模的模腔内温度在短时间内迅速升至设定温度,这样就可以缩短铸造过程中模具的加热准备时间,提高生产效率。
所述铸造金属模具的上、下模恰完全覆盖于外框1上下两侧,即外框1径向尺寸小于等于上、下模径向尺寸,保证燃气管2喷出的所有火力都喷射在上下模的模腔内,热量不易扩散,从而达到集中加热的效果。
所述燃气管2伸入到外框1内的一端呈环形结构,增大火焰与上、下模的加热面积,使加热均匀、快速。
所述燃气管2内的可燃气体为天然气和空气的混合气体,保证可燃气体充分燃烧。
所述外框上、下两端的开口内径大于中间内径。
Claims (5)
1.一种铸造金属模具加热装置,包括外框(1)和燃气管(2),以使用方向为基准,外框(1)呈上下开口的中空筒状体,燃气管(2)一端伸入外框(1)内,燃气管(2)内通有可燃气体,其特征在于:所述外框(1)恰能够插置于铸造金属模具的上、下模之间,伸入外框(1)内的燃气管(2)上下两侧均设有若干出气孔(3)。
2.根据权利要求1所述的铸造金属模具加热装置,其特征在于:所述铸造金属模具的上、下模恰完全覆盖于外框(1)上下两侧。
3.根据权利要求1所述的铸造金属模具加热装置,其特征在于:所述燃气管(2)伸入到外框(1)内的一端呈环形结构。
4.根据权利要求1所述的铸造金属模具加热装置,其特征在于:所述燃气管(2)内的可燃气体为天然气和空气的混合气体。
5.根据权利要求1所述的铸造金属模具加热装置,其特征在于:所述外框上、下两端的开口内径大于中间内径。