CN102608113B - Mildew-proof pH test paper and preparation method thereof - Google Patents

Mildew-proof pH test paper and preparation method thereof Download PDF

Info

Publication number
CN102608113B
CN102608113B CN201210090479.3A CN201210090479A CN102608113B CN 102608113 B CN102608113 B CN 102608113B CN 201210090479 A CN201210090479 A CN 201210090479A CN 102608113 B CN102608113 B CN 102608113B
Authority
CN
China
Prior art keywords
test paper
mildew
proof
coating fluid
resistant
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN201210090479.3A
Other languages
Chinese (zh)
Other versions
CN102608113A (en
Inventor
赵金鹤
王守渔
张啸晨
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SHANGHAI SAN'AISI REAGENT CO Ltd
Original Assignee
SHANGHAI SAN'AISI REAGENT CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SHANGHAI SAN'AISI REAGENT CO Ltd filed Critical SHANGHAI SAN'AISI REAGENT CO Ltd
Priority to CN201210090479.3A priority Critical patent/CN102608113B/en
Publication of CN102608113A publication Critical patent/CN102608113A/en
Application granted granted Critical
Publication of CN102608113B publication Critical patent/CN102608113B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention relates to a mildew-proof pH test paper and a preparation method of the mildew-proof pH test paper. The mildew-proof pH test paper is prepared by dipping filter paper into a pH test paper coating liquid containing a mildew-proof agent O, i.e. 5,6-dichloro benzoxazolinone, for 5-10 seconds; taking out the paper; and drying in hot air or in an infrared drying cabinet at a drying temperature of 70-100 DEG C. The content of the mildew-proof agent O is 0.03-1.0wt% of the total weight of the pH test paper coating liquid. The mildew-proof pH test paper provided by the invention has the characteristics of being good in mildew-proof effect, long in mildew-proof time, small in additive amount of the mildew-proof agent, small in resource investment and the like. The pH test paper product prepared by the method provided by the invention is the first one which is marked with a validity period of three years.

Description

A kind of preparation method of pH test paper of mildew-resistant
One, technical field
The present invention relates to a kind of test paper for detection of solution acid alkalinity and preparation method thereof, relate in particular to pH test paper of a kind of mildew-resistant and preparation method thereof.
Two, background technology
Detect the method for solution acid alkalinity, conventional have pH instrument and a pH test paper.PH test paper has again the feature of simple and easy, convenient, fast, cheapness and non-secondary pollution because of it, more and more be widely used in chemical analysis, industry, agricultural, aquaculture and medicine and other fields, and to water analysis, in the analysis and daily life of the saliva of human body, sweat, blood, urine.Along with the large batch of production of pH test paper, civilian pH test paper life cycle is long, and the problem of going mouldy of test paper is more outstanding, has restricted production and the use of pH test paper.Domestic and international existing technology all adopts carrier directly to make the pH test paper of different size at the indicator dipping of different proportionings, and carrier is the filter paper of being made up of the raw material such as cotton fiber, starch.In production, packaging, storage and the use procedure of pH test paper, because the effect of microorganism is gone mouldy, in pH test strips, just there will be mildew and large stretch of mouldization, particularly pH test paper outward appearance is blue or green for more very, cause the mistake of test result, make pH test paper afunction, and lose use value.The clear 61-30755 of JP, JP2000-171456 and Britain GB96083, open by apply the technology of the water-fast synthetic resin of one deck and air insulated on pH test paper surface respectively, reach the stable effect of test paper.This technical difficulty is high, has high input, and causes the colour developing of test paper slow.Current prior art does not have effectively to solve the method for pH test paper mildew-resistant.
Three, summary of the invention
The object of the invention is, in order to overcome the shortcoming in background technology, provides pH test paper of a kind of mildew-resistant and preparation method thereof.
The present invention is achieved in that a kind of pH test paper of mildew-resistant, is characterized in: the pH test paper of this mildew-resistant is taken out and makes containing after mildewproof agent O flooded for 5~10 seconds in the pH test paper coating fluid of 5,6-dichloro benzo oxazoline ketone by filter paper; The content of mildewproof agent O accounts for 0.03~1.0wt% of pH test paper coating fluid general assembly (TW).
The preparation method of the pH test paper of this mildew-resistant is: the mildewproof agent O being dissolved in 95wt% ethanol is joined in pH test paper coating fluid, obtain the pH test paper coating fluid that contains mildewproof agent O, the content of mildewproof agent O accounts for 0.03~1.0wt% of pH test paper coating fluid general assembly (TW), and in the pH test paper coating fluid that contains mildewproof agent O, the weight ratio of second alcohol and water is 0.5~1.0:1.0; Regulate the pH value of the coating fluid that contains mildewproof agent O to equal 4~8 with NaOH solution or HCl solution; After being flooded to 5~10 seconds in the pH test paper coating fluid that contains mildewproof agent O, takes out by filter paper, dry in hot-air or infrared drying oven, 70~100 DEG C of baking temperatures, obtain the pH test paper of mildew-resistant, and the pH test paper of dried mildew-resistant is through cutting packing cost, circle or bar.
Mildewproof agent O in the present invention i.e. content >=the 98wt% of 5,6-dichloro benzo oxazoline ketone.
The present invention's tool compared with domestic and international prior art has the following advantages::
1, in currently available technology, also do not carry out the research of mildew-resistant and the report of achievement about pH test paper with mildewproof agent.
2, in currently available technology, cannot indicate the use term of validity of pH test paper, the pH test paper of mildew-resistant of the present invention can be indicated the use term of validity of pH test paper.
3, mildewproof agent O of the present invention is by applicant's first development and production at home, and offers the scientific research institutions of cable, electrical equipment, light industry, coating, in the mildew-resistant application in the fields such as cable, electrical equipment, leatheret, resin, coating.The present invention is the mildew-resistant for pH test paper with mildewproof agent O, is to make bacteriostasis property, the working concentration to the mildew-resistant of pH test paper to other type mildewproof agent, and make on the performance test of impact on test paper color development and anti-mold effect and Performance Ratio basis.The pH test paper of mildew-resistant of the present invention has pH test paper quality influence little, and anti-mold effect is good, and the mildew-resistant time is long and mildewproof agent addition is few, and resource drops into the features such as little.The pH test paper product of the production of mildew-resistant of the present invention is first test paper of having indicated 3 years terms of validity.
Four, embodiment
In order to implement better the present invention especially exemplified by following embodiment, but embodiment is not the restriction to invention.
Embodiment 1
The pH test paper of mildew-resistant is to take out and make after flooding for 5~10 seconds by filter paper in the pH test paper coating fluid that contains indicator and mildewproof agent O.
The preparation of the pH test paper coating fluid of mildew-resistant: mildewproof agent O i.e. content >=the 98wt% of 5,6-dichloro benzo oxazoline ketone; The above-mentioned mildewproof agent O being dissolved in 95wt% ethanol is joined in the pH test paper coating fluid that contains indicator, obtain the pH test paper coating solution that contains mildewproof agent O, mildewproof agent O content accounts for 0.03~1.0wt% of pH test paper coating fluid general assembly (TW), and in the pH test paper coating fluid that contains mildewproof agent O, the weight ratio of second alcohol and water is 0.5~1.0:1.0; Regulating the pH value of the coating fluid that contains mildewproof agent O with NaOH solution or HCl solution is 4~8.
The preparation of test paper: take out after filter paper is flooded to 5~10 seconds in the pH test paper coating fluid that contains mildewproof agent O, dry in hot-air or infrared drying oven, 70~100 DEG C of baking temperatures, obtain the pH test paper of mildew-resistant, and dried mildew-resistant pH test paper is through cutting packing cost, circle or bar.The pH test paper energy mildew-resistant of this mildew-resistant and maintenance are stable, and the term of validity is 3 years.
Standard color card is made: use respectively 0.2mol/L Potassium Hydrogen Phthalate solution, 0.1mol/L sodium hydroxide solution, 0.1mol/L aminoacetic acid and 0.1mol/L sodium chloride mixed liquor, 0.1mol/L and 0.2mol/L hydrochloric acid solution, 0.2mol/L boric acid and 0.2mol/L potassium chloride mixed liquor, 0.2mol/L Klorvess Liquid, the standard solution such as 0.2mol/L potassium dihydrogen phosphate, prepare the buffer solution of the pH test paper standard look version of all size on request.The mildew-resistant pH test paper of making, immerse respectively in corresponding standard buffer solution and take out immediately.According to aobvious color modulation standard color card after 5 seconds.
The requirement of making by the pH test paper of above-mentioned mildew-resistant, prepare respectively pH test paper mildew-resistant coating fluid, make the mildew-resistant pH test paper of pH1~14,0.5~5.0,3.8~5.4 equal-specifications, preparation pH1~14,0.5~5.0, the standard buffer solutions corresponding with test paper specification such as 3.8~5.4, respectively test paper is immersed in corresponding standard buffer solution, take out immediately, according to aobvious color modulation standard color card after 5 seconds, through cutting and binding cost, circle or bar, make the mildew-resistant pH test paper of pH1~14,0.5~5.0,3.8~5.4 equal-specifications; The pH test paper product of this mildew-resistant indicates that the term of validity is 3 years.
Using method: get test strips, take out immediately in the liquid that immersion can be surveyed, with standard color card comparison, can directly obtain test result after 5 seconds.

Claims (1)

1. a preparation method for the pH test paper of mildew-resistant, is characterized in that: the pH test paper of this mildew-resistant is taken out and makes containing after mildewproof agent O flooded for 5~10 seconds in the pH test paper coating fluid of 5,6-dichloro benzo oxazoline ketone by filter paper; The content of mildewproof agent O accounts for 0.03~1.0wt% of pH test paper coating fluid general assembly (TW); The mildewproof agent O being dissolved in 95wt% ethanol is joined in pH test paper coating fluid, obtain the pH test paper coating fluid that contains mildewproof agent O, the content of mildewproof agent O accounts for 0.03~1.0wt% of pH test paper coating fluid general assembly (TW), and in the pH test paper coating fluid that contains mildewproof agent O, the weight ratio of second alcohol and water is 0.5~1.0: 1.0; Regulate the pH value of the coating fluid that contains mildewproof agent O to equal 4~8 with NaOH solution or HCl solution; After filter paper is flooded to 5~10 seconds in the pH test paper coating fluid that contains mildewproof agent O, take out, dry in hot-air or infrared drying oven, 70~100 DEG C of baking temperatures, obtain the pH test paper of mildew-resistant.
CN201210090479.3A 2012-03-30 2012-03-30 Mildew-proof pH test paper and preparation method thereof Expired - Fee Related CN102608113B (en)