CN102602559A - Leather attaching technology for mobile phone - Google Patents

Leather attaching technology for mobile phone Download PDF

Info

Publication number
CN102602559A
CN102602559A CN2011100261686A CN201110026168A CN102602559A CN 102602559 A CN102602559 A CN 102602559A CN 2011100261686 A CN2011100261686 A CN 2011100261686A CN 201110026168 A CN201110026168 A CN 201110026168A CN 102602559 A CN102602559 A CN 102602559A
Authority
CN
China
Prior art keywords
mobile phone
glue
leather
technology
housing
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011100261686A
Other languages
Chinese (zh)
Inventor
沈寿明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG TRIUMPH LEATHER CO Ltd
Original Assignee
NANTONG TRIUMPH LEATHER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by NANTONG TRIUMPH LEATHER CO Ltd filed Critical NANTONG TRIUMPH LEATHER CO Ltd
Priority to CN2011100261686A priority Critical patent/CN102602559A/en
Publication of CN102602559A publication Critical patent/CN102602559A/en
Pending legal-status Critical Current

Abstract

The invention discloses a leather attaching technology for a mobile phone. The leather attaching technology is mainly used for attaching leather on a plastic housing of the mobile phone. The leather attaching technology is characterized in that the housing of the mobile phone is subjected to an oil removing process before being attached to the leather, and then is attached with the leather by compound admixture glue; and the compound admixture glue comprises the components by mass of: 84-87% of white glue, 11-13% of yellow glue, and 2-3% of propylene carbonate diluent. The leather attaching technology disclosed by the invention has the advantages that because the housing of the mobile is always processed by spraying oil during producing, and the oil attached to the surface of the mobile phone causes a loss of the performance of the glue, the housing of the mobile phone is processed by removing the oil so that the leather can be covered on the clean housing of the mobile phone and the occurrence of bubbles is avoided. Moreover, the glue used in the technology is a compound mixture which enables the glue to be greater in adhesiveness, to be more suitable for the leather attaching technology; and the purpose of preventing sides from tilting can be achieved even the leather attached to the corners.

Description

A kind of mobile phone lagging technology
Technical field
The present invention relates to a kind of mobile phone lagging technology, specifically is a kind of technology of on the mobile phone shell of plastic material, pasting leathercraft.
Background technology
Mobile phone lagging technology has been a traditional technology at present, and general way forms the lagging mobile phone for the leathercraft that on mobile phone shell, fastens with glue.This technology is simple to operation, and the lagging mobile phone can make cell phone appearance variation, adapts to very much modern society's cell phone appearance multiple demands.But there is following shortcoming in this technology, makes the quality of lagging mobile phone and life-span be difficult to guarantee, for threshold has been set up in the application of high-end mobile phone: the bonding bad bubble that occurs of A, leathercraft and mobile phone shell; B, the bonding processing of leathercraft and mobile phone shell corner do not pass a test easy rake angle during use; C, above-mentioned defective effect outward appearance.
Summary of the invention
Main task of the present invention is to provide a kind of mobile phone lagging technology, specifically is a kind of mobile phone lagging technology that can effectively prevent to form bubble between leathercraft and the mobile phone shell, prevent leathercraft corner rake angle.
In order to solve above technical matters; A kind of mobile phone lagging technology of the present invention; Be mainly and carry out the cladding moulding earlier; The cladding goods that on the mobile phone shell of plastic material, fasten with glue then is characterized in that: before pasting the cladding goods, to the mobile phone shell processing of deoiling, paste with composite mixing glue then; Said composite glue component is: white glues 84-87% mass parts, yellow glue 11-13% mass parts, carbonic allyl ester diluent 2-3% mass parts.
The invention has the advantages that: earlier to the mobile phone shell processing of deoiling, purpose is the mobile phone shell of cleaning is covered skin, avoids the generation of bubble in the present invention.Because mobile phone shell when producing, generally all can have the process of oil spout processing, this processing makes the mobile phone surface with oily matter, makes its performance of glue forfeiture.In addition, the present invention selects composite on glue, makes the viscosity of glue strengthen, and is more suitable for mobile phone lagging technology, even the applying of edge also can reach the not purpose of alice.
The specific embodiment
Lagging technology on the mobile phone shell of the suitable PC material of the present invention.
At first, the outward appearance of setting according to mobile phone is carried out conventional moulding with cladding.
In second step, with evenly wiping behind the spraying degreaser on the mobile phone shell, the grease that brings when purpose is to remove mobile phone production is cleared up its surface.In this step, degreaser is a white spirit, formal name used at school: normal heptane, constitutional formula are CH3 (CH2) 5CH3, mol wt: 100.21.Colourless transparent liquid.Relative density (20 ℃/4 ℃)>0.6594, solidfying point-90.6 ℃, 98.4 ℃ of boiling points. flash-point-4 ℃, 204 ℃ of burning-points, ratio of refraction 1.38512, viscosity (20 ℃) 0.4mPas, solubility parameter δ=7.4.
The 3rd step was composite glue: component is: white glues 84-87% mass parts, yellow glue 11-13% mass parts, carbonic allyl ester diluent 2-3% mass parts; Generally with white glues: yellow glue: the diluent weight ratio is: 15:2:25 is best.Carbonic allyl ester diluent of the present invention is specially carbonic allyl ester (PC) model E-101; Molecular formula: C 4H 6O 3Colourless or light yellow transparent liquid, mol wt 102.08, fusing point are-48.8 ℃, boiling point is 242 ℃, ratio of refraction (nd20) 1.4189 (20 ℃), water-soluble and carbon tetrachloride, miscible with ether, acetone, benzene etc., be a kind of good polar solvent.Purposes: one, be used for epoxy systems, as activated thinner, consumption 5-10%; Two, the activated thinner that can be used as SPUA A component except reducing effectively the viscosity of A component, also has following characteristics: the mixing efficiency of 1. improving system.2. keep even the physical property of enhance elasticity body.3. can reduce the required pressure of spraying.4. water resistance that can the enhance elasticity body, and can make thinner film.5. can form the beta-hydroxy carbonic ester with the amine reaction.Film forming is participated in the NCO reaction of this hydroxyl ability and A component.
In this step, white glues, yellow glue mix and with the reason of diluent: white glues, yellow glue are fully dissolved, reach and better put up effect; If white glues, yellow glue do not use the consequence of diluent: the glue smell is heavier, adhibit quality is not strong, and the phenomenon of bubbling takes place the corrosion raw MAT'L easily.
The 4th step is for after mixing said components;, the mobile phone shell greasy dirt just begins gluing after disposing; Be specially the surface that evenly is coated in mobile phone shell or leathercraft; Particularly edge will be handled and put in place, and after normal temperature 20-22 degree was placed 15-20 minute, glue had probably been done gluing one-time-reach-place under 50% the situation.
The 5th step was generally with relevant moulds of industrial equipment floating from top to bottom for leathercraft and mobile phone shell are carried out the routine compacting.The compacting state is: mobile phone shell and leathercraft are fitted fully.After PROCESS FOR TREATMENT of the present invention, the mobile phone lagging can be covered in the outside face of mobile phone shell securely, and is not easy to come off.
By the mobile phone lagging that technology of the present invention makes, index of quality is following:
(quality system meets ISO 9001:2000 standard)
Figure 593101DEST_PATH_IMAGE001

Claims (1)

1. a mobile phone lagging technology is mainly the leathercraft that on the mobile phone shell of plastic material, fastens with glue, and it is characterized in that: before pasting the cladding goods, to the mobile phone shell processing of deoiling, paste with composite mixing glue then; It is composite mixing glue that said lagging uses glue, and component is: white glues 84-87% mass parts, yellow glue 11-13% mass parts, carbonic allyl ester diluent 2-3% mass parts.
CN2011100261686A 2011-01-25 2011-01-25 Leather attaching technology for mobile phone Pending CN102602559A (en)