CN102554251B - 一种银粉洗涤的工艺 - Google Patents

一种银粉洗涤的工艺 Download PDF

Info

Publication number
CN102554251B
CN102554251B CN201010590977.5A CN201010590977A CN102554251B CN 102554251 B CN102554251 B CN 102554251B CN 201010590977 A CN201010590977 A CN 201010590977A CN 102554251 B CN102554251 B CN 102554251B
Authority
CN
China
Prior art keywords
reactor
technique
argentum powder
powder
hydrochloric acid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201010590977.5A
Other languages
English (en)
Other versions
CN102554251A (zh
Inventor
李学强
翁占平
徐忠敏
国洪柱
孙英翔
彭剑平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Ejinaqi round Mining Co., Ltd.
Zhaojin Mining Industry Co., Ltd.
Original Assignee
Zhaojin Mining Industry Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Zhaojin Mining Industry Co Ltd filed Critical Zhaojin Mining Industry Co Ltd
Priority to CN201010590977.5A priority Critical patent/CN102554251B/zh
Publication of CN102554251A publication Critical patent/CN102554251A/zh
Application granted granted Critical
Publication of CN102554251B publication Critical patent/CN102554251B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

一种银粉洗涤的工艺,是在反应釜中用铁粉置换出银粉后,同时伴随着产生HCL并且溶于水形成盐酸,加入1立方米/300kg的自来水,此时向反应釜内加入NaOH,调整反应釜内溶液的PH值在7.5-8之间,同时开搅拌加速反应。由于置换银粉化学反应与盐酸氢氧化钠中和反应所产生的热量,此时的反应釜内溶液温度可达到60℃以上,反应釜内反应大约0.5小时即可过滤,产生银粉。

Description

一种银粉洗涤的工艺
技术领域:
本发明涉及一种银粉洗涤的工艺,特别是在全湿法冶金生产过程中对产出的银粉的洗涤工艺。
背景技术:
近几年来,随着国家对节能减排和环境污染的重视,对高耗能、高排放、高污染的企业要逐渐的淘汰,对落后的生产工艺要进行创新改造。在全湿法冶金中对产出的银粉,所采取传统的洗涤工艺越来越不适合社会发展的需要,一是采用燃油锅炉蒸汽加热高温洗涤,需要消耗大量的柴油;二是每洗涤一次需要消耗大量的自来水;三是洗涤过程所产生的酸性废水易造成环境污染或增加治理成本。通过全新的洗涤工艺,解决了上述问题,达到了节能减排,消除了酸性废水对环境的污染或对其的治理成本,提高了生产效率缩短了生产周期,节约了生产成本。
发明内容:
本发明的目的是提供一种节能、降耗、环保的银粉洗涤的工艺。
本发明的目的是这样实现的:
在反应釜中用铁粉置换出银粉后,同时伴随着产生HCL并且溶于水形成盐酸,加入1立方米/300kg的自来水,此时向反应釜内加入NaOH,调整反应釜内溶液的PH值在7.5-8之间,同时开搅拌加速反应。由于置换银粉化学反应与盐酸氢氧化钠中和反应所产生的热量,此时的反应釜内溶液温度可达到60℃以上,反应釜内反应大约0.5小时即可过滤,产生银粉。
本发明的最优生产参数如下:
每300公斤银粉自来水的加入量1立方,NaOH调整反应釜内溶液PH值在7.5-8之间;反应釜搅拌运行时间为0.5小时。
本发明与现有技术相比具有以下优点:
由于采用了利用余热的工艺,去除了工艺中的锅炉利用,降低了反应温度,节约了水和柴油,实现了银粉的有效回收,并且改善了作业环境,实现了清洁生产,具有工艺简单、实用,回收率高的优点。
具体实施方式:
实施实例:
编号为A1-A3为传统洗涤方式
编号为B1-B3改进后洗涤方式
由上述表格可以看出,优化后的工艺反应温度降低25%,水的利用率降低80%,反应时间降低87.5%,节省全部柴油消耗。

Claims (1)

1.一种银粉洗涤的工艺,其特征在于在反应釜中用铁粉置换出银粉后,同时伴随着产生HCL并且溶于水形成盐酸,加入自来水,自来水的加入量为1000公斤/300公斤银粉;
所述反应釜加入水后,再加入NaOH,调整反应釜内溶液的PH值在7.5-8之间,反应时间为0.5小时。
CN201010590977.5A 2010-12-08 2010-12-08 一种银粉洗涤的工艺 Active CN102554251B (zh)