CN102528392A - 一种防氧化不变色局部拉丝扣板制备工艺 - Google Patents

一种防氧化不变色局部拉丝扣板制备工艺 Download PDF

Info

Publication number
CN102528392A
CN102528392A CN2011104377569A CN201110437756A CN102528392A CN 102528392 A CN102528392 A CN 102528392A CN 2011104377569 A CN2011104377569 A CN 2011104377569A CN 201110437756 A CN201110437756 A CN 201110437756A CN 102528392 A CN102528392 A CN 102528392A
Authority
CN
China
Prior art keywords
wire drawing
oxidation
buckle
local
wiredrawn
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2011104377569A
Other languages
English (en)
Inventor
卢纯福
张轲
陈龙
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
ZHEJIANG DINMEI ELECTRICAL APPLIANCE CO Ltd
Original Assignee
ZHEJIANG DINMEI ELECTRICAL APPLIANCE CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by ZHEJIANG DINMEI ELECTRICAL APPLIANCE CO Ltd filed Critical ZHEJIANG DINMEI ELECTRICAL APPLIANCE CO Ltd
Priority to CN2011104377569A priority Critical patent/CN102528392A/zh
Publication of CN102528392A publication Critical patent/CN102528392A/zh
Pending legal-status Critical Current

Abstract

一种防氧化不变色局部拉丝扣板制备工艺,所述制备工艺包括以下步骤:1)先对扣板材料进行切割;2)冲压成型;3)突出部位拉丝;4)在扣板拉丝部位涂覆透明涂料,并干燥;所述透明涂料为防氧化涂料;5)在扣板拉丝部位再喷涂装饰涂料,并干燥,制得防氧化不变色局部拉丝扣板。本发明外形美观、立体感较强、制作方便、不易脱落失效。

Description

一种防氧化不变色局部拉丝扣板制备工艺
技术领域
本发明涉及一种吊顶加工工艺,尤其是一种扣板制备工艺。 
背景技术
随着人们生活水平的提高,家居装饰越来越朝高档化发展,室内吊顶也从最初的简单朝美观、实用等方向发展。通常吊顶由铝材加工而成,在传统的吊顶加工过后,有明显的凹凸形状,但缺乏立体感,且形象呆板,由于加工后吊顶加工部位出高能状态容易氧化失去光泽,影响整体美观程度。又由吊顶容易被氧化,吊顶上面着色涂料容易脱落失效。 
发明内容
为了克服已有现有吊顶扣板着色容易脱落失效、立体感较差的不足,本发明提供一种外形美观、立体感较强、制作方便、不易脱落失效的防氧化不变色局部拉丝扣板制备工艺。 
本发明解决其技术问题所采用的技术方案是: 
一种防氧化不变色局部拉丝扣板制备工艺,所述制备工艺包括以下步骤: 
1)先对扣板材料进行切割; 
2)冲压成型; 
3)突出部位拉丝; 
4)在扣板拉丝部位涂覆透明涂料,并干燥;所述透明涂料为防氧化涂料; 
5)在扣板拉丝部位再喷涂装饰涂料,并干燥,制得防氧化不变色局部拉丝扣板。 
进一步,所述步骤4)中,印刷透明涂料采用丝网印刷工艺,干燥温度为60~80℃。 
再进一步,所述步骤4)中,所述透明涂料为热固性涂料。 
更进一步,所述热固性涂料为环氧树脂涂料或聚氨酯涂料。当然,也可以采用其他热固性涂料。 
本发明的有益效果主要表现在:1、外形美观、立体感较强、制作方便、不易脱落失效;2、对扣板进凹凸图形如果经过拉丝处理,可以增加吊顶的美观程度和立体感,且拉丝过程中形状不固定,属唯一形状,这样极大的增加了商品的层次的价值,在加工过程中,被加工部位由于处于高能状态,往往容易被氧化而失去光泽,在表面喷涂上防氧化涂料能很好的解决这一问题,且喷涂防氧化涂料后的吊顶再喷涂其它装饰涂料后不易脱落,从而增大了商品的使用空间。 
具体实施方式
下面对本发明作进一步描述。 
一种防氧化不变色局部拉丝扣板制备工艺,所述制备工艺包括如下步骤: 
1)先对扣板材料进行切割 
2)冲压成型 
3)突出部位拉丝 
4)在扣板拉丝部位涂覆透明涂料,并干燥;所述透明涂料为防氧化涂料; 
5)在扣板拉丝部位再喷涂装饰涂料,并干燥,制得防氧化不变色 局部拉丝扣板。 
所述步骤4)中,印刷透明涂料采用丝网印刷工艺,干燥温度为60~80℃。 
所述的透明涂料是环氧树脂涂料、聚氨酯涂料;所述的环氧树脂涂料是指环氧树脂是平均每个分子含有两个或两个以上环氧基的热固性树脂,所述的聚氨酯涂料是指树脂为基料,以颜料、填料等为辅助材料的涂料。 
实例1:一种防氧化不变色局部拉丝扣板制备工艺,包括如下步骤: 
1、铝板落料且成型;2、在四个角处冲压圆弧形凸台;3、进行拉丝处理;4、拉丝部位表面丝印防氧化环氧树脂透明涂料;5、送入烘干流水线进行烘干处理; 
实例2:一种防氧化不变色局部拉丝扣板制备工艺,包括如下步骤: 
1、铝板落料且成型;2、在扣板任意一边处冲压条形花纹状凸台;3、进行拉丝处理;4、拉丝表面丝印防氧化聚氨酯透明涂料;5、送入烘干流水线进行烘干处理; 
实例3:一种防氧化不变色局部拉丝扣板制备工艺,包括如下步骤: 
1、铝板落料且成型;2、在四角处冲压斜条形状凸台;3、进行拉丝处理;4、拉丝表面丝印防氧化环氧树脂透明涂料;5、送入烘干流水线进行烘干处理; 
实例4:一种防氧化不变色局部拉丝扣板制备工艺,包括如下步骤: 
1、铝板落料且成型;2、在扣板中央处冲压花纹凸台;3、进行拉丝处理;4、拉丝表面丝印防氧化聚氨酯透明涂料;5、送入烘干流水线进行烘干处理。 

Claims (4)

1.一种防氧化不变色局部拉丝扣板制备工艺,其特征在于:所述制备工艺包括以下步骤:
1)先对扣板材料进行切割;
2)冲压成型;
3)突出部位拉丝;
4)在扣板拉丝部位涂覆透明涂料,并干燥;所述透明涂料为防氧化涂料;
5)在扣板拉丝部位再喷涂装饰涂料,并干燥,制得防氧化不变色局部拉丝扣板。
2.如权利要求1所述的防氧化不变色局部拉丝扣板制备工艺,其特征在于:所述步骤4)中,印刷透明涂料采用丝网印刷工艺,干燥温度为60~80℃。
3.如权利要求1或2所述的防氧化不变色局部拉丝扣板制备工艺,其特征在于:所述步骤4)中,所述透明涂料为热固性涂料。
4.如权利要求3所述的1或2所述的防氧化不变色局部拉丝扣板制备工艺,其特征在于:所述热固性涂料为环氧树脂涂料或聚氨酯涂料。
CN2011104377569A 2011-12-23 2011-12-23 一种防氧化不变色局部拉丝扣板制备工艺 Pending CN102528392A (zh)