CN102492450A - 一种挥发份大于32%的肥煤的配煤方法 - Google Patents
一种挥发份大于32%的肥煤的配煤方法 Download PDFInfo
- Publication number
- CN102492450A CN102492450A CN2011104299803A CN201110429980A CN102492450A CN 102492450 A CN102492450 A CN 102492450A CN 2011104299803 A CN2011104299803 A CN 2011104299803A CN 201110429980 A CN201110429980 A CN 201110429980A CN 102492450 A CN102492450 A CN 102492450A
- Authority
- CN
- China
- Prior art keywords
- coal
- blending
- rich
- fat
- fat coal
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
一种挥发份大于32%的肥煤的配煤方法,它是先对肥煤进行挥发份及流变性指标固-软温度区间、log最大流动度的测定,选取其中挥发份大于32%、固-软温度区间大于100℃并且log最大流动度大于或等于4.6的肥煤为第一肥煤,然后将第一肥煤按照如下质量百分数配煤:气肥煤:0-10%、第一肥煤:0-10%、1/3焦煤:20-35%、焦煤:40-45%、瘦煤:10-15%。用本发明的配煤方法进行配煤可以对肥煤资源合理使用,科学配煤。本发明利用肥煤的流变性指标来选取进行配煤的肥煤,并且通过合理的配煤,不仅稳定了焦炭质量,还可以降低配煤成本。
Description
技术领域
本发明属于炼焦配煤技术领域,具体是指一种挥发份大于32%的肥煤的配煤方法。
背景技术
随着我国焦炉大型化的发展,各个焦化企业对强黏结性煤的使用比例越来越高。而我国的强黏结性的肥煤资源仅占炼焦煤资源的10%,炼焦煤资源与炼焦配煤的需求之间矛盾严重。因此,如何利用肥煤配煤的方法来利用好有限的焦煤资源,成了炼焦工作者必需面临的问题。目前,我国对肥煤的煤质评价方法主要依赖于传统的煤质指标(G、Y、挥发份)和煤岩指标(镜质组反射率及其分布),一般选用参与配煤的强黏结性的肥煤G>90、Y>25mm、挥发份不小于32%。但是部分肥煤的煤质较为复杂,这些指标存在一定缺陷,不能对肥煤做到合理使用,因此不能达到稳定提高焦炭质量和降低配煤成本的目的。
挥发份大于32%的肥煤属于高挥发份的肥煤,这类肥煤挥发份较高,虽然价格较低,但是质量要劣于低挥发份肥煤,在现有的配煤应用中,会使焦炭质量不能得到保证,因此一般不采用挥发份大于32%的肥煤进行配煤。
发明内容
本发明的目的是根据上述不足提供一种挥发份大于32%的肥煤的配煤方法,用该方法配煤既可以稳定提高焦炭质量,又可以降低配煤成本。
本发明是通过如下技术方案实现的:一种挥发份大于32%的肥煤的配煤方法,它是先对肥煤进行挥发份及流变性指标固-软温度区间、log最大流动度的测定,选取其中挥发份大于32%、固-软温度区间大于100℃,并且log最大流动度大于或等于4.6的肥煤为第一肥煤,然后将第一肥煤按照如下质量百分数配煤:气肥煤:0-10%、第一肥煤0-10%、1/3焦煤:20-35%、焦煤:40-45%、瘦煤:10-15%。
优选的,所述挥发份大于32%的肥煤按如下质量百分数配煤:气肥煤:5%、第一肥煤:5%、1/3焦煤:35%、焦煤:42%、瘦煤:13%。
用本发明的配煤方法进行配煤可以对挥发份大于32%的肥煤资源进行合理使用,科学配煤,解决了挥发份大于32%的肥煤资源不能用于实际配煤中的问题。本发明利用肥煤的流变性指标来选取进行配煤的肥煤,并且通过合理的配煤,将挥发份大于32%的肥煤和气肥煤应用于配煤中,不仅稳定了焦炭质量,还可以大大降低配煤成本。
具体实施方式
以下结合具体实施例来进一步说明本发明:
首先对肥煤进行挥发份Vdaf的测定,然后进行流变性指标的测定, 对测定结果提取Vdaf(挥发份)、固-软温度区间、LogMF(log最大流动度)这三个指标。选取其中挥发份Vdaf>32%,固-软温度区间>100℃,LogMF≥4.6的肥煤作为第一肥煤,然后将第一肥煤按照表1所示质量百分数进行配煤:
表1:
实施例 | 气肥煤 | 第一肥煤 | 1/3焦煤 | 焦煤 | 瘦煤 |
1 | 5% | 10% | 20% | 50% | 15% |
2 | 0 | 10% | 35% | 40% | 15% |
3 | 5% | 5% | 35% | 42% | 13% |
4 | 3% | 10% | 27% | 50% | 10% |
5 | 10% | 0 | 35% | 40% | 15% |
现有技术按照如下质量百分数配煤得到实施例6的配煤:挥发份不大于32%的肥煤:30%、1/3焦煤:10%、焦煤:50%、瘦煤:10%。
将实施例1-6的配煤进行焦炭热性能测定,测定结果如表2所示:
表2:
实施例 | CRI(焦炭反应性) | CSR(焦炭反应后强度) |
1 | 18.5% | 71.4% |
2 | 18.0% | 73.9% |
3 | 19.0% | 72.1% |
4 | 17.0% | 72.0% |
5 | 19.8% | 71.3% |
6(现有技术) | 17.0% | 73.5% |
从表2可以看出,用本发明方法用成本较低的挥发份大于32%的高挥发份肥煤配煤可以达到与现有技术中采用挥发份不大于32%的肥煤配煤相同的焦炭热性能,不仅焦炭热性能稳定,而且肥煤用量减少,因此大大节省了成本,提高了性价比。
Claims (2)
1.一种挥发份大于32%的肥煤的配煤方法,它是先对肥煤进行挥发份及流变性指标固-软温度区间、log最大流动度的测定,选取其中挥发份大于32%、固-软温度区间大于100℃并且log最大流动度大于或等于4.6的肥煤为第一肥煤,然后将第一肥煤按照如下质量百分数配煤:气肥煤:0-10%、第一肥煤:0-10%、1/3焦煤:20-35%、焦煤:40-45%、瘦煤:10-15%。
2.根据权利要求1所述挥发份大于32%的肥煤的配煤方法,其特征在于:所述肥煤按如下质量百分数配煤:气肥煤:5%、第一肥煤:5%、1/3焦煤:35%、焦煤:42%、瘦煤:13%。