CN102478483A - 一种起泡剂半衰期的测定方法 - Google Patents

一种起泡剂半衰期的测定方法 Download PDF

Info

Publication number
CN102478483A
CN102478483A CN2010105675433A CN201010567543A CN102478483A CN 102478483 A CN102478483 A CN 102478483A CN 2010105675433 A CN2010105675433 A CN 2010105675433A CN 201010567543 A CN201010567543 A CN 201010567543A CN 102478483 A CN102478483 A CN 102478483A
Authority
CN
China
Prior art keywords
half life
foaming agent
frothing agent
life period
time
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010105675433A
Other languages
English (en)
Inventor
袁连海
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010105675433A priority Critical patent/CN102478483A/zh
Publication of CN102478483A publication Critical patent/CN102478483A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种起泡剂半衰期的测定方法。该起泡剂半衰期的测定方法包括:称取一定量起泡剂倒入100ml纯水中;搅拌至全部溶解后倒入搅拌杯中;高速搅拌一段时间;倒入量筒中,读取泡沫体积V;观察泡沫的变化情况,记录泡沫中析出50ml液体所需的时间t,该时间t即为起泡剂半衰期等步骤。本发明能快速测定出起泡剂的半衰期,且测试时间短,测试精度高,测试成本低,通过测定的半衰期,从而分析出起泡剂的性能。

Description

一种起泡剂半衰期的测定方法
技术领域
本发明涉及一种起泡剂半衰期的测定方法。
背景技术
泡沫是一种不稳定的物质体系,起泡剂的筛选与评价是所有泡沫流体应用中的重要工作,不同的应用目的,对于起泡剂有不同的要求。不同类型的起泡剂适应性有较大的差别,泡沫压裂液对于起泡剂主要有以下要求:
(1)起泡性能好,泡沫基液与气体接触后可产生大量泡沫,即泡沫体积膨胀倍数高。
(2)泡沫具有较好稳定性。
(3)抗污染能力强,与其它流体配伍性好。
(4)用量少,成本低。
(5)起泡剂制造原料充分,供应货源广泛。
起泡剂性能主要从两个方面进行评价,一是起泡能力,另一方面是稳定性。
常用的起泡剂主要有阴离子型起泡剂、非离子型起泡剂、复合型起泡剂、高聚物型起泡剂等几种类型,各种起泡剂基本的起泡性能差别较大。
稠化剂是压裂液体系中性能参数最重要、成本较高的添加剂。它的选择不仅影响压裂液的成本,更直接影响压裂工艺实施的成败。由于煤层温度一般比较低而且极易受到污染伤害,所以稠化剂的合理选择对压裂成功起着重要作用。水基压裂液稠化剂主要可分为三类:①植物胶及其衍生物瓜胶、香豆胶、皂仁胶、田菁胶、决明子胶等;②纤维素系列如羧甲基纤维素钠CMC、羟乙基纤维素HEC、羧甲基羟乙基纤维素CMHEC等;③合成聚合物如聚丙烯酰胺PAM、
甲叉基聚丙烯酰胺、尼龙树脂胶等。稠化剂性能主要以起增粘能力、交联能力和残渣含量表征。对具有相同增粘能力和交联能力的稠化剂,其残渣含量应以重点考虑,据文献报道稠化剂的残渣将严重影响支撑裂缝导流能力;同时含水率的高低也影响粉剂的用量。在煤层储层温度较低这一特征条件下,选择适当的稠化剂,不但要满足煤层储层的特点、压裂工艺和成本的要求,而且要考虑其残渣对煤层气井储层的伤害。
发明内容
本发明的目的在于克服上述现有技术的缺点和不足,提供一种起泡剂半衰期的测定方法,该测试方法能快速测定出起泡剂的半衰期,且测试时间短,测试精度高,测试成本低,通过测定的半衰期,从而分析出起泡剂的性能。
本发明的目的通过下述技术方案实现:一种起泡剂半衰期的测定方法,包括以下步骤:
(a)在室温下,称取一定量起泡剂倒入100ml纯水中;
(b)搅拌至全部溶解后倒入搅拌杯中;
(c)高速搅拌一段时间;
(d)倒入量筒中,读取泡沫体积V;
(e)观察泡沫的变化情况,记录泡沫中析出50ml液体所需的时间t,该时间t即为起泡剂半衰期。
所述步骤(c)中,搅拌速度为10000r/min。
所述步骤(c)中,搅拌时间为60s。
所述步骤(d)中,量筒的容积为500ml或1000ml。
综上所述,本发明的有益效果是:能快速测定出起泡剂的半衰期,且测试时间短,测试精度高,测试成本低,通过测定的半衰期,从而分析出起泡剂的性能。
具体实施方式
下面结合实施例,对本发明作进一步的详细说明,但本发明的实施方式不仅限于此。
实施例:
本发明涉及的一种起泡剂半衰期的测定方法,其具体步骤如下:
(a)在室温下,称取一定量起泡剂倒入100ml纯水中;
(b)搅拌至全部溶解后倒入搅拌杯中;
(c)高速搅拌一段时间;
(d)倒入量筒中,读取泡沫体积V;
(e)观察泡沫的变化情况,记录泡沫中析出50ml液体所需的时间t,该时间t即为起泡剂半衰期。
所述步骤(c)中,搅拌速度为10000r/min。
所述步骤(c)中,搅拌时间为60s。
所述步骤(d)中,量筒的容积为500ml或1000ml。
上述测试方法能快速测定出起泡剂的半衰期,且测试时间短,测试精度高,测试成本低,通过测定的半衰期,从而分析出起泡剂的性能。
以上所述,仅是本发明的较佳实施例,并非对本发明做任何形式上的限制,凡是依据本发明的技术实质,对以上实施例所作的任何简单修改、等同变化,均落入本发明的保护范围之内。

Claims (4)

1.一种起泡剂半衰期的测定方法,其特征在于,包括以下步骤:
(a)在室温下,称取一定量起泡剂倒入100ml纯水中;
(b)搅拌至全部溶解后倒入搅拌杯中;
(c)高速搅拌一段时间;
(d)倒入量筒中,读取泡沫体积V;
(e)观察泡沫的变化情况,记录泡沫中析出50ml液体所需的时间t,该时间t即为起泡剂半衰期。
2.根据权利要求1所述的一种起泡剂半衰期的测定方法,其特征在于,所述步骤(c)中,搅拌速度为10000r/min。
3.根据权利要求1所述的一种起泡剂半衰期的测定方法,其特征在于,所述步骤(c)中,搅拌时间为60s。
4.根据权利要求1所述的一种起泡剂半衰期的测定方法,其特征在于,所述步骤(d)中,量筒的容积为500ml或1000ml。
CN2010105675433A 2010-11-22 2010-11-22 一种起泡剂半衰期的测定方法 Pending CN102478483A (zh)