CN105441044B - 一种油基钻井液用堵漏剂 - Google Patents

一种油基钻井液用堵漏剂 Download PDF

Info

Publication number
CN105441044B
CN105441044B CN201410474336.1A CN201410474336A CN105441044B CN 105441044 B CN105441044 B CN 105441044B CN 201410474336 A CN201410474336 A CN 201410474336A CN 105441044 B CN105441044 B CN 105441044B
Authority
CN
China
Prior art keywords
oil base
drilling fluid
sealing agent
fluid sealing
base drilling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN201410474336.1A
Other languages
English (en)
Other versions
CN105441044A (zh
Inventor
封心领
袁俊秀
王康
逯贵广
庞雨微
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
China Petroleum and Chemical Corp
Research Institute of Sinopec Nanjing Chemical Industry Co Ltd
Original Assignee
China Petroleum and Chemical Corp
Research Institute of Nanjing Chemical Industry Group Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by China Petroleum and Chemical Corp, Research Institute of Nanjing Chemical Industry Group Co Ltd filed Critical China Petroleum and Chemical Corp
Priority to CN201410474336.1A priority Critical patent/CN105441044B/zh
Publication of CN105441044A publication Critical patent/CN105441044A/zh
Application granted granted Critical
Publication of CN105441044B publication Critical patent/CN105441044B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种油基钻井液用堵漏剂,各组分重量配比为:纤维15~20%,核桃壳10~25%,吸油聚合物颗粒20~40%,油基核壳膨胀封堵剂40~60%,将上述原料混合均匀即为油基钻井液用堵漏剂。本发明的堵漏剂制备工艺简单、亲油性好、具有良好的悬浮稳定性及膨胀性能、封堵效果好。

Description

一种油基钻井液用堵漏剂
技术领域
本发明涉及一种钻井液处理剂,具体涉及一种油基钻井液用堵漏剂。
背景技术
随着国内页岩气井、水平井、大位移井的发展,油基钻井液使用率逐年增加。但是,油基钻井液的配制成本比水基钻井液高的多,如果钻遇复杂裂缝性地层,油基钻井液大量漏失,不但影响了钻进效率,造成的经济损失更是不可估量。目前,处理油基钻井液井漏的方法是加入封堵材料,但这些封堵材料,基本上都针对水基钻井液体系开发的,水基堵漏剂在油基钻井液体系中应用存在着分散性不好,遇油强度减弱,剪切易破碎,不具备耐油性,并且存在与其它油基钻井液处理剂配伍性不足的问题,在一定程度上影响了现场应用中的堵漏效果。
发明内容
本发明的目的在于提供一种油基钻井液用堵漏剂。
本发明所述的一种油基钻井液堵漏剂,各组分重量配比为:
纤维15~20%;核桃壳10~25%;吸油聚合物颗粒20~40%;油基核壳膨胀封堵剂40~60%;
其中,所述的纤维包括锯末或聚酯纤维或两者的混合物,其尺寸为0.1~2mm,纤维的直径范围为0.01~0.025mm。
所述的核桃壳尺寸为0.05~3mm。
所述的吸油聚合物颗粒为:聚丙烯颗粒或聚氨酯颗粒或其两者的混合物,其颗粒尺寸范围为0.15~0.9mm。
所述的油基核壳膨胀封堵剂为聚甲基丙烯酸酯为核,聚丙烯酸丁酯为壳的核壳共聚物,其颗粒尺寸为:0.01-0.1mm。
配制方法:将上述物质按组分及含量,常温常压下,加入到捏合机中,混合均匀,即为油基钻井液用堵漏剂。
本发明的优点:本发明提供的一种油基钻井液用堵漏剂,亲油性好,有良好的悬浮稳定性,在基础油中具有可膨胀性,能够适应不同尺寸以及形状的空隙或裂缝,制备工艺简单。
具体实施方式
下面通过实施例对本发明做进一步的说明,其目的仅在于更好的理解本发明而非限制本发明保护的范围。
实施例1
将15%锯末,10%核桃壳,20%聚丙烯颗粒,55%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀,得到一种油基钻井液用堵漏剂
实施例2
将20%聚酯纤维,15%核桃壳,30%聚丙烯颗粒,35%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀一种可变形油基钻井液用堵漏剂。
实施例3
将15%聚酯纤维,20%核桃壳,25%聚氨酯颗粒,40%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀一种可变形油基钻井液用堵漏剂。
实施例4
将20%锯末,20%核桃壳,20%聚氨酯颗粒,40%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀一种可变形油基钻井液用堵漏剂。
实施例5
将10%聚酯纤维,10%锯末,20%核桃壳,20%聚氨酯颗粒,40%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀一种可变形油基钻井液用堵漏剂。
实施例6
将15%锯末,15%核桃壳,10%聚氨酯颗粒,10%聚丙烯颗粒,50%油基核壳膨胀封堵剂,常温常压下,加入到捏合机中混合均匀一种可变形油基钻井液用堵漏剂。
取实施例1-6的样品,将一滴白油滴在平整的封堵材料表面上,用JC2000D接触角仪测定白油在封堵材料表面的接触角,并观察白油在封堵材料的润湿性。
表1 样品的接触角
取实施例1-6的样品,进行油基堵漏剂的体积膨胀倍数的测试。封堵材料的吸油倍数为吸油饱和后的质量与吸油前的质量比百分数。
表2 样品的膨胀体积倍数
取实施例1-6的样品,在加量为5wt%条件下,利用QD-2型堵漏仪、选用不同的缝隙版进行承压能力试验。测试结果如表3-5所示。
表3 样品在1mm缝隙版承压能力测试结果
表4 样品在3mm缝隙版承压能力测试结果
表5样品在5mm缝隙版承压能力测试结果
本发明提供的一种油基钻井液用堵漏剂,承压能力强,堵漏效果好。

Claims (5)

1.一种油基钻井液用堵漏剂,其特征是它包含纤维、核桃壳、吸油聚合物颗粒、油基核壳膨胀封堵剂,各组分重量配比为:
纤维: 15~20%
核桃壳: 10~25%
吸油聚合物颗粒: 20~40%
油基核壳膨胀封堵剂: 40~60%。
2.根据权利要求1所述的油基钻井液用堵漏剂,其特征在于,所述的纤维包括锯末或聚酯纤维或两者的混合物,其尺寸为0.1~2mm,纤维的直径范围为0.01~0.025mm。
3.根据权利要求1所述的油基钻井液用堵漏剂,其特征在于,所述的核桃壳尺寸为0.05~3mm。
4.根据权利要求1所述的油基钻井液用堵漏剂,其特征在于,所述的吸油聚合物颗粒为:聚丙烯颗粒或聚氨酯颗粒或其两者的混合物,其颗粒尺寸范围为0.15~0.9mm。
5.根据权利要求1所述的油基钻井液用堵漏剂,其特征在于,所述的油基核壳膨胀封堵剂为聚甲基丙烯酸酯为核,聚丙烯酸丁酯为壳的核壳共聚物,其颗粒尺寸为:0.01-0.1mm。
CN201410474336.1A 2014-09-17 2014-09-17 一种油基钻井液用堵漏剂 Active CN105441044B (zh)