CN102407709A - Method for manufacturing gold-sprayed plate of printing and dyeing roller - Google Patents
Method for manufacturing gold-sprayed plate of printing and dyeing roller Download PDFInfo
- Publication number
- CN102407709A CN102407709A CN2011102437705A CN201110243770A CN102407709A CN 102407709 A CN102407709 A CN 102407709A CN 2011102437705 A CN2011102437705 A CN 2011102437705A CN 201110243770 A CN201110243770 A CN 201110243770A CN 102407709 A CN102407709 A CN 102407709A
- Authority
- CN
- China
- Prior art keywords
- handled
- glue
- corrosion
- engraving
- printing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
The invention relates to a printing and dyeing roller manufacturing technology, in particular to a gold-sprayed plate manufacturing method of a printing and dyeing roller, which comprises the following process steps of machining, nickel plating, grinding, manuscript manufacturing, glue spraying, laser engraving and corrosion.
Description
[technical field]
The present invention relates to a kind of printing and dyeing system roller technology, a kind of printing roller spills gold version manufacturing approach specifically.
[background technology]
The gold version is spilt in common laser corrosion, generally uses the network process that adds of 10-201/cm, and is generally all more sparse after bronze is spread across on the pattern; Abundant inadequately and brightness does not reach the effect of expectation, and how guaranteeing to spill bronze, to be sprinkled upon on the pattern back bronze abundant beautiful, is problem to be solved by this invention; If only do version through overstriking mesh and intensification corrosion depth, seem and can reach, but after actual test; Otherwise the amount of being exactly is not enough, otherwise is exactly that scumming phenomenon in printing process is serious.
[summary of the invention]
The present invention provides spilling of a kind of printing roller golden version manufacturing approach in order to overcome the deficiency of prior art.
To achieve these goals, the utility model has designed the golden version manufacturing approach of spilling of a kind of printing roller, and its processing step comprises machining; Nickel plating is ground, and contribution is made; Spray glue, laser engraving, corrosion; It is characterized in that: comprise the processing of secondary spray glue after the described corrosion treatment, the secondary laser engraving is handled, and anticaustic is handled and chromium plating is handled.
Described contribution is made, and passes through the computer software design pattern according to customer requirement, and it is littler 0.2 to 0.4 millimeter than spilling the following pattern of gold part that it spills the pattern of gold part.
Described spray glue carries out gluing and handles on glue sprayer, the workshop temperature is 20 to 25 degree, and humidity is below 60%, and black adhesiveness is 18 seconds, and evenly coating one deck is deceived glue, 3 to 5 microns of bondline thickness on the version roller.
Described laser engraving is carved through the programmed in advance program of computer software, and engraving machine adopts straight mode of carving, and by 9 settings of corrosion depth, the carver leads 15 to 20 watts, and Revolution Per Minute 800 to 1000 changes.
Described corrosion, corrosion depth are 9.
Described secondary spray glue is handled, and the black glue of spraying for the first time on the intaglio plate is cleaned, and it is carried out secondary spray glue; Its workshop temperature is 20 to 25 degree, and humidity is humidity below 60%, and black adhesiveness is 18 seconds; Evenly coating one deck is deceived glue, 3 to 5 microns of bondline thickness on the version roller.
Described secondary laser engraving is handled, and with the same program of engraving employing for the first time, the engraving mode adopts 20 lines, and corrosion depth is set to 9, and laser power is 15 to 20 watts, and rotating speed is that per minute 800 to 1000 changes.
Described anticaustic is handled, and corrosion depth is 9, and the leader height is 1 to 5 micron.
Described chromium plating is handled, and its chromium layer thickness is 1 to 1.2.
The present invention compares with prior art, on the seal roller, can be made into the different degree of depth through difference being schemed line according to needs, enough makes the embossing effect of the embossing effect arrival glue surface wallpaper on pure living paper and the non-woven paper, is rich in third dimension and stereovision.
[specific embodiment]
Female roller version of the present invention is long 600 millimeters, 233.50 millimeters of diameters, and female roller plated end nickel, and the thickness of nickel is 1, further specifies manufacturing approach of the present invention below.
Machining, female roller processing length is 750 millimeters, diameter is 233.50 millimeters.
Copper facing, the monolateral copper facing thickness of female roller is 25.
Grind, grinding copper layer to monolateral copper layer is 20 to 23.
Contribution is made, and passes through the computer software design pattern according to customer requirement, and it is littler 0.2 to 0.4 millimeter than spilling the following pattern of gold part that it spills the pattern of gold part, in order to avoid spill the pattern register trouble of gold version below it, and influence attractive in appearance.
Spray glue carries out gluing and handles on glue sprayer, the workshop temperature is 20 to 25 degree, and humidity is below 60%, and black adhesiveness is 18 seconds, on the version roller, evenly is coated with the black glue of one deck, 3 to 5 microns of bondline thickness.
Laser engraving is carved through the programmed in advance program of computer software, and engraving machine adopts straight mode of carving, and by 9 settings of corrosion depth, the carver leads 15 to 20 watts, and Revolution Per Minute 800 to 1000 changes.
Corrosion, corrosion depth is 9.
Secondary spray glue is handled, and the black glue of spraying for the first time on the intaglio plate is cleaned, and it is carried out secondary spray glue; Its workshop temperature is 20 to 25 degree, and humidity is humidity below 60%, and black adhesiveness is 18 seconds; Evenly coating one deck is deceived glue, 3 to 5 microns of bondline thickness on the version roller.
The secondary laser engraving, with the same program of engraving employing for the first time, the engraving mode adopts 20 lines, and corrosion depth is set to 9, and laser power is 15 to 20 watts, and rotating speed is that per minute 800 to 1000 changes.
Anticaustic, corrosion depth are 9, and the leader height is 1 to 5 micron.
Chromium plating, its chromium layer thickness are 1 to 1.2.
Corrosion depth of the present invention is total up to 18; Wherein 9 of corrosion earlier adopt straight mode of carving to guarantee the bronze amount; Corrode 9 in addition again and adopt screening 20 lines, leader is controlled at 1 to 5 micron, guarantees to support scraper by leader; Occur leaking the phenomenon of pattern and scumming in avoiding printing, the gold version of spilling that this each technology is worked it out has just satisfied the abundant beautiful requirement of bronze.
Claims (3)
- A printing roller spill gold version manufacturing approach, its processing step comprises machining, nickel plating is ground; Contribution is made, spray glue, laser engraving, corrosion; It is characterized in that: comprise the processing of secondary spray glue after the described corrosion treatment, the secondary laser engraving is handled, and anticaustic is handled and chromium plating is handled;Described contribution is made, and passes through the computer software design pattern according to customer requirement, and it is littler 0.2 to 0.4 millimeter than spilling the following pattern of gold part that it spills the pattern of gold part;Described spray glue carries out gluing and handles on glue sprayer, the workshop temperature is 20 to 25 degree, and humidity is below 60%, and black adhesiveness is 18 seconds, and evenly coating one deck is deceived glue, 3 to 5 microns of bondline thickness on the version roller;Described laser engraving is carved through the programmed in advance program of computer software, and engraving machine adopts straight mode of carving, and by 9 settings of corrosion depth, the carver leads 15 to 20 watts, and Revolution Per Minute 800 to 1000 changes;Described corrosion, corrosion depth are 9.
- Printing roller according to claim 1 spill gold version manufacturing approach, it is characterized in that:Described secondary spray glue is handled, and the black glue of spraying for the first time on the intaglio plate is cleaned, and it is carried out secondary spray glue; Its workshop temperature is 20 to 25 degree, and humidity is humidity below 60%, and black adhesiveness is 18 seconds; Evenly coating one deck is deceived glue, 3 to 5 microns of bondline thickness on the version roller;Described secondary laser engraving is handled, and with the same program of engraving employing for the first time, the engraving mode adopts 20 lines, and corrosion depth is set to 9, and laser power is 15 to 20 watts, and rotating speed is that per minute 800 to 1000 changes;Described anticaustic is handled, and corrosion depth is 9, and the leader height is 1 to 5 micron.
- 3. according to the method for manufacturing printing plate of the claim 1 or the many degree of depth of described printing roller, it is characterized in that: described chromium plating is handled, and its chromium layer thickness is 1 to 1.2.