Prior art keywords
water
panel
furnace door
cooled furnace
cooling
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN201010272231XA
Other languages
English (en)
Inventor
沈剑
冯吉军
罗成坚
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN201010272231XA priority Critical patent/CN102382936A/zh
Publication of CN102382936A publication Critical patent/CN102382936A/zh
Pending legal-status Critical Current

Links

Images

Landscapes

  • Furnace Housings, Linings, Walls, And Ceilings (AREA)

Abstract

本发明公开了一种转炉水冷炉口,包括进水管、面板、外侧板和中间法兰,所述面板向内凹陷形成弧形。所述进水管的弯曲处为一体无缝连接,所述中间法兰向外伸出并与外侧板底边固定连接。本发明结构合理,水冷炉口抗压能力提高,水冷炉口内冷却水在管内迂回,流速均匀不会有冷却死角,也增加了水的流量,热交换能力得到了提高,水冷炉口的使用寿命普通达到6个月左右,消除了炉口漏水现象以及因漏水可能引起的事故隐患,也增加了使用寿命,降低了使用成本。

Description

转炉水冷炉口
技术领域
本发明涉及一种炼钢设备转炉,尤其涉及一种转炉水冷炉口。
背景技术
目前国内使用氧气顶吹转炉炼钢均在1600℃以上的高温下进行。转炉炉体一般由炉帽、炉壳、炉底三部分组成,为延长炉帽的金属壳和炉衬使用寿命,一般在炉帽顶部设有圆形炉口,以便工作时加料插入氧枪排出炉气和倒渣,为了保护炉口,普遍采用循环水冷却炉口。通常的水冷炉口由钢板铆焊而成,冷却水同侧双进双出式,冷却水环绕一周后排出,安装形式是卡板式焊接。,这种转炉水冷炉口的缺点是:炉口内水流速度不均匀,水流不稳定,造成热交换能力差,水冷炉口各部位冷却不一致,易发生汽化,局部蒸汽压很高时水冷炉口易产生裂缝而漏水。水冷炉口有效使用寿命短,只有1个月左右,从而使用成本高。在更换安装时,靠卡板焊接连接,焊接工作量大,更换一次需6~8h,严重制约了生产。
发明内容
本发明所要解决的技术问题时针对上述现有技术的不足提供一种水流量大、水流速均匀、热交换效率高的转炉水冷炉口。
为解决上述技术问题,本发明采用的技术方案为:一种转炉水冷炉口,包括进水管、面板、外侧板和中间法兰,所述面板向内凹陷形成弧形。弧形面板承受着水冷炉口内部水流的一定的压力,将转炉的面板压制成弧形,能够提高抗压能力,减轻因高温带来的热胀危险。
作为本发明进一步改进的技术方案,所述进水管的弯曲处为一体无缝连接。进水管弯曲处原用冲压弯头连接,现用整管事先弯曲后安装,减少焊缝,同时提高冷却水流量,流速均匀不会有冷却死角,提高热交换能力。
作为本发明进一步改进的技术方案,所述中间法兰向外伸出并与外侧板底边固定连接。中间法兰与外侧板焊接形式改变,现将中间法兰伸出,外侧板打外坡口,能够提高焊接强度,减少漏水现象。
本发明结构合理,水冷炉口抗压能力提高,水冷炉口内冷却水在管内迂回,流速均匀不会有冷却死角,也增加了水的流量,热交换能力得到了提高,水冷炉口的使用寿命普通达到6个月左右,消除了炉口漏水现象以及因漏水可能引起的事故隐患,也增加了使用寿命,降低了使用成本。
下面结合附图对本发明作进一步详细描述。
附图说明
图1为本发明的俯视示意图。
图2为图1的A-A向剖视示意图。
图3为图2的B处局部放大示意图。
图4为图2的C处局部放大示意图。
具体实施方式
实施例1
参见图1和图2,一种转炉水冷炉口,包括进水管1、面板2、外侧板3和中间法兰4,面板2下方设有底板5,进水管1位于面板2和底板5之间,面板2为圆形板,外侧板3为环形侧面板,外侧板3的上边缘与面板2的外边缘固定连接。如图3所示,所述面板2向内凹陷形成弧形,弧形面板承受着水冷炉口内部水流的一定的压力,将转炉的面板2压制成弧形,能够提高抗压能力,减轻因高温带来的热胀危险。所述进水管1的弯曲处为一体无缝连接,进水管1的弯曲处原用冲压弯头连接,现用整管事先弯曲后安装,减少焊缝,同时提高冷却水流量,流速均匀不会有冷却死角,提高热交换能力。如图4所示,所述中间法4向外伸出并与外侧板4底边固定连接,中间法兰4与外侧板3焊接形式改变,现将中间法兰4伸出,外侧板3打外坡口,能够提高焊接强度,减少漏水现象。

Claims (3)

1.一种转炉水冷炉口,包括进水管(1)、面板(2)、外侧板(3)和中间法兰(4),其特征在于:所述面板(2)向内凹陷形成弧形面板。
2.根据权利要求1所述的转炉水冷炉口,其特征在于:所述进水管(1)的弯曲处为一体无缝连接。
3.根据权利要求1或2所述的转炉水冷炉口,其特征在于:所述中间法兰(4)向外伸出并与外侧板(3)底边固定连接。
CN201010272231XA 2010-09-03 2010-09-03 转炉水冷炉口 Pending CN102382936A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN201010272231XA CN102382936A (zh) 2010-09-03 2010-09-03 转炉水冷炉口

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN201010272231XA CN102382936A (zh) 2010-09-03 2010-09-03 转炉水冷炉口

Publications (1)

Publication Number Publication Date
CN102382936A true CN102382936A (zh) 2012-03-21

Family

ID=45822765

Family Applications (1)

Application Number Title Priority Date Filing Date
CN201010272231XA Pending CN102382936A (zh) 2010-09-03 2010-09-03 转炉水冷炉口

Country Status (1)

Country Link
CN (1) CN102382936A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105154618A (zh) * 2015-11-02 2015-12-16 上海宝钢铸造有限公司 水冷炉口防熔脱装置及方法
CN114517245A (zh) * 2022-03-03 2022-05-20 河北工业职业技术学院 转炉水冷炉口结构及转炉

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN105154618A (zh) * 2015-11-02 2015-12-16 上海宝钢铸造有限公司 水冷炉口防熔脱装置及方法
CN114517245A (zh) * 2022-03-03 2022-05-20 河北工业职业技术学院 转炉水冷炉口结构及转炉

Similar Documents

Publication Publication Date Title
CN102976312B (zh) 一种提高煅后焦换热器寿命的换热器结构
CN100465290C (zh) 一种叠合式冷却壁
CN201548055U (zh) Lf炉冷却炉盖
CN102382936A (zh) 转炉水冷炉口
CN102958214B (zh) 矿热炉的保护屏
CN202813780U (zh) 冷凝式燃气壁挂炉
CN201785430U (zh) 转炉水冷炉口
CN2801795Y (zh) 长寿命水冷炉口
CN206001450U (zh) 一种防脱落的钟罩式风帽
CN202907250U (zh) 矿热炉的保护屏
CN202808837U (zh) 一种设有凸台的铜冷却壁
CN213013033U (zh) 一种烟化炉多枪风口铸铜水套
CN209244615U (zh) 一种汽轮机低压缸冷却装置
CN101526309B (zh) 一种密闭式电石炉加料嘴及制造工艺
CN103542761A (zh) 一种列管式换热器管箱用密封垫
CN208983314U (zh) 具有缓冲热应力与提高换热效率的水冷壁管鳍片
CN203561248U (zh) 一种保护气—水换热器
CN201560196U (zh) 高炉新型风口带冷却壁
CN202885495U (zh) 一种冲天炉热风炉胆
CN214830447U (zh) 一种热风炉热风出口炉壳临时冷却吹扫装置
CN103343977B (zh) 换热器及其制作方法
CN209584302U (zh) 一种不锈钢光亮退火炉圆型结构炉胆
CN216049382U (zh) 一种补偿器保护结构及预热器
CN212770822U (zh) 一种转炉炉体冷却结构
CN213977533U (zh) 新型焦粉冷却装置

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Application publication date: 20120321