CN1022875C - 大型变压器绝缘压圈及制造方法 - Google Patents
大型变压器绝缘压圈及制造方法 Download PDFInfo
- Publication number
- CN1022875C CN1022875C CN 91103110 CN91103110A CN1022875C CN 1022875 C CN1022875 C CN 1022875C CN 91103110 CN91103110 CN 91103110 CN 91103110 A CN91103110 A CN 91103110A CN 1022875 C CN1022875 C CN 1022875C
- Authority
- CN
- China
- Prior art keywords
- press ring
- insulating
- insulating press
- pressing ring
- curing
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
本发明提供了一种大型变压器用的绝缘压圈及制造方法。以前采用电工绝缘板材加工绝缘压圈时,工序多,难度大,浪费材料,浪费能源,并造成环境污染。本发明采用湿法一次成型制造出整体性好、韧性刚性好,电气性能和机械性能好的大型变压器绝缘压圈。本发明可为大型变压器提供各种规格的绝缘压圈,使用方便,省时省料。
Description
本发明涉及电工绝缘材料-大型变压器用绝缘压圈及制造方法。
1988.3.17德国专利公布的DE3630295A,公开了一种高介电强度的“绝缘筒的制造过程”。它是用纤维毡(或网)经过传送辊系统送入浸渍槽,浸过热固性树脂后,由卷心轴驱动的同步传动辊转动、缠绕在卷心轴上,与卷心轴同步转动的封闭箔带,紧贴在已卷好的,浸有树脂的纤维毡(或网)卷上,控制纤维毡(或网)卷的厚度,并使液体树脂均匀分布于卷上,还可收紧该卷,最后制成由多层纤维毡(或网)构成的、高介电强度的“绝缘筒”。这种办法,可使被缠绕的纤维毡(或网)无任何附加应力,有利于获得均匀的介电强度和机械强度,对于筒壁小于20mm,筒长的尺寸比较大时,是可行的。但绕制相当于“筒”长为30mm,壁厚≥100mm的大型变压器“压圈”时,必不能制成合格产品。因为用无拉伸应力的毡(或网)绕制时,织物有界面,当壁后≥20mm时,层间开裂(这是层绕绝缘筒的固有特性),即整体性不好,导致热稳定性差,根本不能作高压、超高压的大型变压器绝缘压圈,另外,为保证被缠绕纤维毡(或网)无拉伸应力,对设备各传动机构同步工作的要求十分严格,致使设备的动态结构复杂化;再说,DE3630295A文件通篇对固化温度、固化时间没有提出要求,如用其作“制造方法”,那末,“工艺技术”公开得不充分,该文只介绍了“制造过程”。1990年2月28日公告的CN2053781U公开了采用环氧玻璃纤维束制成的长方形或圆形绝缘环,没有公开其配方及制造工艺。
真正制造大型变压器绝缘压圈的老方法,是将电工绝缘材料-环氧酚醛玻璃布板材,经过机械加工(锯、车、铣)而成,限于电工绝缘板面积小,加工大直径(如直径1.5m~2m)的变压器绝缘压圈时,只有用几个圆弧拼接起来。这样做工艺麻烦,难度大,浪费材料,浪费能源,加工粉尘大,制造的产品易开裂,影响其电气、机械性能。原民主德国专利DD-205-768A,Mfgtransformer in-sulating ring for ming composite sheet by bon-ding cut strip then rolling into ring,该专利介绍的大型变压器绝缘压圈的制造方法同样存在着加工麻烦,浪费材料,浪费能源的问题。
本发明的目的是提供一种一次湿法成型的且整体性好,气隙含量低,韧性刚性好,并且有优异的电气性能及机械性能的大型变压器用的绝缘压圈。
本发明是用电工玻璃纤维纱在牵引力下浸以绝缘树脂,连续缠绕滚压在特制的模具上,经固化、脱模、加工、浸漆、烘焙而成。
所采用的浸胶树脂,以双酚型环氧树脂为基料,加有酸酐固化剂和叔胺类促进剂。电工玻璃纤维为无碱无捻合股玻璃纤维。绝缘压圈的纤维含量为60-70%。
浸胶树脂组成为:双酚型环氧树脂90-100重量份,酸酐型固化剂60-100重量份,叔胺类促进剂0-4重量份。浸胶树脂为无溶剂树脂,该树脂粘度小,流动性好,固化周期短,工艺性能好,使用方便。
浸胶树脂的制备工艺:将树脂的各组份加入混胶釜,在温度60-80℃进行温升搅拌至均匀为止。
绝缘压圈的制造工艺:玻璃纤维纱在1-3KN/m的线压力下浸以浸胶树脂滚压、缠绕在特制的模具上,缠绕速度3-6m/min。绝缘压圈的固化工艺:温度130-150℃,时间6-10小时。当温度降至50℃以下进行脱模。后浸漆次数为2-3次,后浸漆固化温度为140℃,时间5-8小时。
绝缘压圈的实测技术数据:密度1.6g/cm3;
弯曲强度:平行纤维方向196.5MPa,垂直纤维方向41.1MPa;浸水后绝缘电阻,平行纤维方向1.3×103MΩ;介电强度,垂直纤维方向(于90±2℃变压器油中)23MV/m;击穿电压,平行纤维方向(于90±2℃变压器油中)41.7KV。
本发明为大型变压器提供一种新型的绝缘压圈,其规格为30-80mm×φ250/φ2000mm之间各种尺寸,以前将电工绝缘板材加工成变压器绝缘压圈,材料浪费大,材料的利用率只有40~50%,以一个变压器厂每年需要环氧酚醛玻璃布板为100吨计算,材料费用为200万元,材料利用率以45%计算,那么材料费损失为110万元。一台12万千伏安的大型变压器,使用本发明制造的绝缘压圈,其材料费用可节约13248元,节约了材料,节约了能源,提高了经济效益。
实施例:
浸胶树脂配方:
材料 重量份
6010环氧树脂 100
甲基四氢苯酐 70
苄基二甲胺 3
工艺过程:
1、玻璃纱缠绕速度 6米/分
2、绝缘压圈固化条件 140℃,8h
3、脱模 40℃
4、后浸漆次数 2次
5、后固化条件 150℃,5h
Claims (2)
1、一种制造大型变压器绝缘压圈的方法,用玻璃纤维在牵引为下浸以环氧树脂连续缠绕,滚压在模具上,经固化、脱模、加工、浸漆、烘烙而成,其特征在于所述的玻璃纤维是无碱无捻合成股玻璃纤维纱,缠绕速度为3-6m/min,线压力1-3KN/m,固化温度为130-150℃,固化时间为6-10小时;后浸漆固化温度为140℃,固化时间为5-8小时。
2、采用权利要求1所述方法制造的大型变压器的绝缘压圈,由无碱无捻合股玻璃纤维纱加浸胶树脂绕制而成,其特征在于浸胶树脂的组成为:
双酚型环氧树脂:90~100(重量份)
酸酐型固化剂:60~100(重量份)
叔胺类促进剂:0~4(重量份)