CN102251440B - Decorative film coated paper for bamboo veneer and production method and device of decorative film coated paper - Google Patents

Decorative film coated paper for bamboo veneer and production method and device of decorative film coated paper Download PDF

Info

Publication number
CN102251440B
CN102251440B CN 201110185903 CN201110185903A CN102251440B CN 102251440 B CN102251440 B CN 102251440B CN 201110185903 CN201110185903 CN 201110185903 CN 201110185903 A CN201110185903 A CN 201110185903A CN 102251440 B CN102251440 B CN 102251440B
Authority
CN
China
Prior art keywords
paper
body paper
glue
roller
film coated
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN 201110185903
Other languages
Chinese (zh)
Other versions
CN102251440A (en
Inventor
吴金保
胡立明
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
YIYANG TAOHUAJIANG BAMBOO DEVELOPMENT CO LTD
Original Assignee
YIYANG TAOHUAJIANG BAMBOO DEVELOPMENT CO LTD
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by YIYANG TAOHUAJIANG BAMBOO DEVELOPMENT CO LTD filed Critical YIYANG TAOHUAJIANG BAMBOO DEVELOPMENT CO LTD
Priority to CN 201110185903 priority Critical patent/CN102251440B/en
Publication of CN102251440A publication Critical patent/CN102251440A/en
Application granted granted Critical
Publication of CN102251440B publication Critical patent/CN102251440B/en
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

The invention discloses decorative film coated paper for a bamboo veneer, and a production method and a production device of the decorative film coated paper. The decorative film coated paper is prepared from low quantitative raw paper and has high sizing amount. The decorative film coated paper is characterized in that: the decorative film coated paper is prepared from raw paper (19) by primary sizing, primary drying, secondary sizing, secondary drying, shearing and packing through the production device of the decorative film coated paper; the surface sizing amount of the raw paper (19) is 140 to 180g/m<2>; and after the raw paper is stored at the room temperature of below 30 DEG C for 90 days and the abrasion resistance reaches 380 revolutions, the base of the raw paper is not exposed. The process is simple, the quantification of the raw paper is light, the produced product has good surface finishment and flatness, the board has good abrasion resistance, ageing resistance and corrosion resistance, and the storage time of the product is greatly prolonged.

Description

The bamboo offset plate is with decorating tectorial paper, its production method and device
Technical field
The present invention relates to a kind of template with decorating tectorial paper, specifically a kind of bamboo offset plate is with decorating tectorial paper, its production method and device.
Background technology
At present, building template has the pollopas of employing glue dipping to produce with the decoration tectorial paper, also has and adopts phenolic resins glue dipping to produce.The poor fluidity of the former glue, water imbibition is strong.Latter's plate surface fineness and planarization are not good enough, and its clad can effect is undesirable.Be 02138420.7 such as the patent No., the applying date is on October 8th, 2002, publication number be CN1415799 patent disclosure a kind of red brown paper dipped with metlbond, it forms body paper through dipping glue, drying, shearing.Because a photoresist coating process that adopts, the body paper spread is few, and plate surface fineness and planarization are not good enough; Used body paper is 60g/ ㎡~90g/ ㎡ quantitatively simultaneously, and production cost is high; And the product of making is sheared, the rear easily adhesion of packing, separates difficulty during use, and storage time is short, only is 15-20 days.
Summary of the invention
The purpose of this invention is to provide the low quantitative body paper of a kind of use, and the high bamboo offset plate of spread decoration tectorial paper, its production method and device.
The present invention adopts following technical scheme to realize its goal of the invention, a kind of bamboo offset plate is with decorating tectorial paper, body paper is made after a gluing, primary drying, secondary gluing, redrying, shearing, packing, body paper surface spread is 140g/ ㎡~180 g/ ㎡, stored 90 days below 30 ℃ in room temperature, ABRASION RESISTANCE reaches 380 and turns rear without grinning effect.
The quantitative of the used body paper of the present invention is 45g/ ㎡~55g/ ㎡.
A kind of as mentioned above bamboo offset plate production method of decorating tectorial paper, it comprises the following steps:
⑴ a gluing: body paper sent in the glue in the gumming mechanism flood 2s~3s, gelatin viscosity is that 15s~17s, solid content are 38 ﹪~40 ﹪ under 40 ℃ of the temperature;
⑵ primary drying: the body paper after will flooding is sent in the primary drying mechanism and is dried, and bake out temperature is 150 ℃~180 ℃, and drying time is 10s~12s, and the body paper moisture content is 25 ﹪~30 ﹪ behind the primary drying, and spread is 100g/ ㎡~120 g/ ㎡;
⑶ secondary gluing: the body paper behind the primary drying is sent into gluing in the secondary gumming mechanism, at first glue evenly is coated on the body paper behind the step ⑵, gelatin viscosity is that 20s~25s, solid content are 38 ﹪~40 ﹪ under 40 ℃ of the temperature;
⑷ redrying: the body paper behind step ⑶ sent in the redrying mechanism dry, bake out temperature is 140 ℃~170 ℃, and drying time is 10s~12s, and the body paper moisture content is 10 ﹪~12 ﹪ after the redrying, and spread is 140g/ ㎡~180 g/ ㎡;
⑸ shear, packing: will send into through the body paper behind the step ⑷ and get the product decoration tectorial paper after cutting mechanism is sheared, packed by dimensional requirement.
For being convenient for changing paper roll, prevent from simultaneously being broken when body paper from flooding in glue, make body paper progressively adapt to the traction of haulage gear.The present invention in step ⑴, at first with body paper through holding paper, tension adjustment mechanism, again glue is coated in the one side of body paper, then send in the glue and flood.
For preventing that product from shearing, the packing posterior synechia, separate difficulty during use.The present invention scrapes off the glue of dual-side on the body paper behind step ⑶.
A kind of decoration tectorial paper process units of realizing said method, it comprises main frame, be arranged on the haulage gear of main frame afterbody, cutting mechanism, described main frame is a rack-mounted gumming mechanism successively, primary drying mechanism, the secondary gumming mechanism, redrying mechanism, described secondary gumming mechanism comprises rack-mounted upper rubber-coated mechanism, lower rubber-coated mechanism and the floating mechanism that is formed by two pairs of smooth rolls, described upper rubber-coated mechanism comprises the upper glue roller that is installed in the body paper top, gluing case, described lower rubber-coated mechanism comprise the lower rubber roller that is installed in the body paper below, lower glue case.
The present invention prevents body paper 19 because of quantitatively low simultaneously for being convenient for changing paper roll, is broken when flooding in glue, makes body paper progressively adapt to the traction of haulage gear.A gumming mechanism of the present invention comprises rack-mounted paper, tension adjustment mechanism, coating mechanism and the impregnating mechanism of holding, describedly hold paper, tension adjustment mechanism comprises adjustment roller, lower adjustment roller, described coating mechanism comprises applicator roll, the glue case that is installed in the body paper below; Described impregnating mechanism comprises the dip roll that is installed in the glue case; Body paper, is connected with transition roller around dip roll through applicator roll through around upper adjustment roller, lower adjustment roller.
The present invention separates difficulty for preventing that product from shearing, the packing posterior synechia during use.The present invention is provided with behind lower rubber-coated mechanism be used to the frictioning mechanism that scrapes off body paper dual-side glue.
Frictioning of the present invention mechanism comprises the lower rubber roller that is located at the body paper below, and both sides, lower rubber roller top are provided with scraping blade, and scraping blade is installed on the frame by support.
The present invention adjusts for convenient, and scraping blade of the present invention is rack-mount by adjustment rack.
Owing to adopt technique scheme, the present invention has realized goal of the invention preferably, technique is simple, body paper quantitatively light, product surface fineness and the planarization produced are fine, sheet material ABRASION RESISTANCE, anti-aging and corrosion resistance good, the product storage time prolongs greatly, can store 90 days below 30 ℃ in room temperature.
Description of drawings
Fig. 1 is structural principle schematic diagram of the present invention.
The specific embodiment
The invention will be further described below in conjunction with drawings and Examples.
A kind of bamboo offset plate is with decorating tectorial paper, body paper 19 is made after a gluing, primary drying, secondary gluing, redrying, shearing, packing, body paper 19 surface sizing amounts are 140g/ ㎡~180 g/ ㎡, store 90 days below 30 ℃ in room temperature, and ABRASION RESISTANCE reaches 380 and turns rear without grinning effect.The present embodiment glue is the phenolic resins glue.
The quantitative of the used body paper of the present invention is 45g/ ㎡~55g/ ㎡ (present embodiment is 50g/ ㎡).
A kind of as mentioned above bamboo offset plate production method of decorating tectorial paper, it comprises the following steps:
⑴ a gluing: body paper 19 sent into to flood 2s~3s(present embodiment in glue in the gumming mechanism 1 be 2s), gelatin viscosity is that 15s~17s(present embodiment is 17s under 40 ℃ of the temperature), solid content is 38 ﹪~40 ﹪ (present embodiment is 40 ﹪);
⑵ primary drying: the body paper 19 after will flooding is sent into oven dry in the primary drying mechanism 5, bake out temperature is 150 ℃~180 ℃ (present embodiment is 170 ℃), drying time is that 10s~12s(present embodiment is 12 s), body paper 19 moisture content are 25 ﹪~30 ﹪ (present embodiment is 25 ﹪) behind the primary drying, and spread is 100g/ ㎡~120 g/ ㎡ (present embodiment is 120 g/ ㎡);
⑶ secondary gluing: the body paper 19 behind the primary drying is sent into gluing in the secondary gumming mechanism 6, at first glue evenly is coated on the body paper 19 behind the step ⑵, gelatin viscosity is under 40 ℃ of the temperature, 20s~25s(present embodiment is 20s), solid content is 38 ﹪~40 ﹪ (present embodiment is 38 ﹪);
⑷ redrying: the body paper 19 behind step ⑶ is sent into oven dry in the redrying mechanism 11, bake out temperature is 140 ℃~170 ℃ (present embodiment is 150 ℃), drying time is that 10s~12s(present embodiment is 10 s), body paper 19 moisture content are 10 ﹪~12 ﹪ (present embodiment is 11 ﹪) after the redrying, and spread is 140g/ ㎡~180 g/ ㎡ (present embodiment is 170 g/ ㎡);
⑸ shear, packing: will send into through the body paper 19 behind the step ⑷ and get the product decoration tectorial paper after cutting mechanism 12 is sheared, packed by dimensional requirement.
For being convenient for changing paper roll, prevent simultaneously body paper 19 because of quantitatively low, broken when in glue, flooding, make body paper 19 progressively adapt to the traction of haulage gear.The present invention in step ⑴, at first with body paper 19 through holding paper, tension adjustment mechanism 2, again glue is coated in the one side of body paper 19, then send in the glue and flood.
For preventing that product from shearing, the packing posterior synechia, separate difficulty during use.The present invention scrapes off the glue of dual-side on the body paper 19 behind step ⑶.
As shown in Figure 1, a kind of as mentioned above decoration tectorial paper process units of method of realizing, it comprises main frame, be arranged on the haulage gear of main frame afterbody, cutting mechanism 12, described main frame is a rack-mounted gumming mechanism 1 successively, primary drying mechanism 5, secondary gumming mechanism 6, redrying mechanism 11, described secondary gumming mechanism 6 comprises rack-mounted upper rubber-coated mechanism, lower rubber-coated mechanism and the floating mechanism that is formed by two pairs of smooth rolls 13, described upper rubber-coated mechanism comprises the upper glue roller 8 that is installed in body paper 19 tops, gluing case 7, described lower rubber-coated mechanism comprises the lower rubber roller 14 that is installed in body paper 19 belows, lower glue case 15.
The present invention prevents from being broken when body paper 19 from flooding in glue for being convenient for changing paper roll simultaneously, makes body paper 19 progressively adapt to the traction of haulage gear.A described gumming mechanism 1 comprises rack-mounted paper, tension adjustment mechanism 2, coating mechanism 3 and the impregnating mechanism 4 of holding, describedly hold paper, tension adjustment mechanism 2 comprises adjustment roller 20, lower adjustment roller 21, described coating mechanism 3 comprises applicator roll 18, the glue case 16 that is installed in body paper 19 belows; Described impregnating mechanism 4 comprises the dip roll 17 that is installed in the glue case 16; Body paper 19, is connected with transition roller around dip roll 17 through applicator roll 18 through around upper adjustment roller 20, lower adjustment roller 21.
The present invention separates difficulty for preventing that product from shearing, the packing posterior synechia during use.Behind lower rubber-coated mechanism, be provided be used to the frictioning mechanism that scrapes off body paper 19 dual-side glues.
Described frictioning mechanism comprises the lower rubber roller 14 that is located at body paper 19 belows, and both sides, lower rubber roller 14 top are provided with scraping blade 10, and scraping blade 10 is installed on the frame by support 9.
The present invention makes things convenient for adjustment need scrape width and the thickness of glue, and scraping blade 10 is installed on the support 9 by adjustment rack.
When the present invention works, body paper 19 on the paper roll progressively adapts to the traction of haulage gear around upper adjustment roller 20, lower adjustment roller 21, and adjusts its tension force, then the one side gluing of giving body paper 19 through applicator roll 18 again floods a gluing finishing body paper 19 around 17 pairs of body paper 19 of dip roll.When need are changed paper roll, can in non-stop-machine situation, utilize and hold paper, the upper distance of adjusting between roller 20 and the lower adjustment roller 21 of tension adjustment mechanism 2 adjustment, realize the replacing of paper roll.
Body paper 19 is after primary drying mechanism 5 dryings, and its spread is 100g/ ㎡~120 g/ ㎡ (present embodiment is 120 g/ ㎡).Because the body paper spread is few, be applied to sheet material after, surface smoothness and planarization are not good enough, so body paper 19 is carried out the secondary gluing, the secondary gluing is adopted and is applied.Two gluings that body paper 19 is given body paper 19 through upper glue roller 8, lower rubber roller 14, then by the floating mechanism that two pairs of smooth rolls 13 form that the glue on the body paper 19 is floating.
For preventing that product from shearing, the packing posterior synechia, separate difficulty during use.Both sides, lower rubber roller 14 top are provided with scraping blade 10, by scraping blade 10 glue on body paper 19 dual-sides are scraped off, and by the adjustment of adjustment rack, capable of regulating scrapes off the width of glue.Because body paper 19 dual-sides are ventilated better in the middle of the body paper 19 without adhesion, the temperature in the middle of reducing, the product storage time prolongs greatly, can store 90 days below 30 ℃ in room temperature.
Body paper 19 is sheared, is packed after redrying mechanism 11 dryings, and spread is 140g/ ㎡~180 g/ ㎡ (present embodiment is 170 g/ ㎡), stores 90 days below 30 ℃ in room temperature, and ABRASION RESISTANCE reaches 380 and turns rear without grinning effect.

Claims (6)

1. a bamboo offset plate is characterized in that with the production method of decorating tectorial paper it comprises the following steps:
⑴ a gluing: body paper (19) sent in the glue in the gumming mechanism (1) flood 2s~3s, gelatin viscosity is under 40 ℃ of the temperature, 15s~17s, solid content is 38 ﹪~40 ﹪, in step ⑴, at first with body paper (19) through holding paper, tension adjustment mechanism (2), again glue is coated in the one side of body paper (19), then send in the glue and flood, the quantitative of used body paper (19) is 45g/ ㎡~55g/ ㎡;
⑵ primary drying: the body paper after will flooding (19) is sent into oven dry in the primary drying mechanism (5), bake out temperature is 150 ℃~180 ℃, drying time is 10s~12s, and body paper behind the primary drying (19) moisture content is 25 ﹪~30 ﹪, and spread is 100g/ ㎡~120 g/ ㎡;
⑶ secondary gluing: the body paper behind the primary drying (19) is sent into gluing in the secondary gumming mechanism (6), at first glue evenly is coated on the body paper behind the step ⑵ (19), gelatin viscosity is that 20s~25s, solid content are 38 ﹪~40 ﹪ under 40 ℃ of the temperature;
⑷ redrying: the body paper (19) behind step ⑶ is sent into oven dry in the redrying mechanism (11), bake out temperature is 140 ℃~170 ℃, drying time is 10s~12s, body paper after the redrying (19) moisture content is 10 ﹪~12 ﹪, and spread is 140g/ ㎡~180 g/ ㎡;
⑸ shearing, packing: will send into through the body paper behind the step ⑷ (19) and get the product decoration tectorial paper after cutting mechanism (12) is sheared, packed by dimensional requirement, decorate tectorial paper and stored 90 days below 30 ℃ in room temperature, ABRASION RESISTANCE reaches 380 and turns rear without grinning effect.
2. described bamboo offset plate is characterized in that behind step ⑶ with the production method of decorating tectorial paper according to claim 1, and the glue of body paper (19) being gone up dual-side scrapes off.
3. realize the as claimed in claim 1 or 2 decoration tectorial paper process units of method for one kind, it comprises main frame, be arranged on the haulage gear of main frame afterbody, cutting mechanism (12), described main frame is a rack-mounted gumming mechanism (1) successively, primary drying mechanism (5), secondary gumming mechanism 6, redrying mechanism (11), it is characterized in that a described gumming mechanism (1) comprises the rack-mounted paper that holds, tension adjustment mechanism (2), coating mechanism (3) and impregnating mechanism (4), the described paper that holds, tension adjustment mechanism (2) comprises adjustment roller (20), lower adjustment roller (21), described coating mechanism (3) comprise the applicator roll (18) that is installed in body paper (19) below, glue case (16); Described impregnating mechanism (4) comprises the dip roll (17) that is installed in the glue case (16); Body paper (19), is connected with transition roller around dip roll (17) through applicator roll (18) through around upper adjustment roller (20), lower adjustment roller (21); Described secondary gumming mechanism (6) comprises rack-mounted upper rubber-coated mechanism, lower rubber-coated mechanism and the floating mechanism that is comprised of two pairs of smooth rolls (13), described upper rubber-coated mechanism comprises upper glue roller (8), the gluing case (7) that is installed in body paper (19) top, and described lower rubber-coated mechanism comprises lower rubber roller (14), the lower glue case (15) that is installed in body paper (19) below.
4. described decoration tectorial paper process units according to claim 3 is characterized in that being provided with the frictioning mechanism be used to scraping off body paper (19) dual-side glue behind lower rubber-coated mechanism.
5. described decoration tectorial paper process units according to claim 4, it is characterized in that described frictioning mechanism comprises the lower rubber roller (14) that is located at body paper (19) below, both sides, lower rubber roller (14) top are provided with scraping blade (10), and scraping blade (10) is installed on the frame by support (9).
6. described decoration tectorial paper process units according to claim 5 is characterized in that scraping blade (10) is installed on the support (9) by adjustment rack.
CN 201110185903 2011-07-05 2011-07-05 Decorative film coated paper for bamboo veneer and production method and device of decorative film coated paper Expired - Fee Related CN102251440B (en)