CN102133592A - 一种钣金零件凹陷制作方法 - Google Patents
一种钣金零件凹陷制作方法 Download PDFInfo
- Publication number
- CN102133592A CN102133592A CN 201010565622 CN201010565622A CN102133592A CN 102133592 A CN102133592 A CN 102133592A CN 201010565622 CN201010565622 CN 201010565622 CN 201010565622 A CN201010565622 A CN 201010565622A CN 102133592 A CN102133592 A CN 102133592A
- Authority
- CN
- China
- Prior art keywords
- sheet metal
- metal part
- depression
- overlap joint
- panel beating
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及一种钣金零件凹陷制作方法,包括以下步骤:(1)将钣金零件搭接,形成搭接台阶;(2)在搭接台阶的一侧加一辅助支撑面;(3)在搭接台阶的另一侧向辅助支撑面的方向锤击施加钣金力,钣金零件受到钣金料厚边缘的反向力,形成凹陷,用简单的方法实现了钣金凹陷的制作,无需工装模具,成本低廉、实用性强。
Description
技术领域
本发明涉及一种钣金技术领域,具体地说是一种钣金零件凹陷制作方法。
背景技术
传统的钣金零件凹陷加工需用工装模具制作,可是制作模具的周期长、成本高,无法对市场需求作出快速的反应。
发明内容
本发明的目的是提供一种工艺简单、快速制作钣金零件凹陷的钣金零件凹陷制作方法。
本发明所采用的技术方案是这样的:一种钣金零件凹陷制作方法,包括以下步骤:(1)将钣金零件搭接,形成搭接台阶;(2)在搭接台阶的一侧加一辅助支撑面;(3)在搭接台阶的另一侧向辅助支撑面的方向锤击施加钣金力,钣金零件受到钣金料厚边缘的反向力,形成凹陷。
所述凹陷的深度与钣金料厚相同。
通过采用前述技术方案,本发明的有益效果是:用简单的方法实现了钣金凹陷的制作,无需工装模具,成本低廉、实用性强。
附图说明
图1为本发明钣金零件凹陷制作的示意图;
具体实施方式
以下结合附图和具体实施例来进一步说明本发明。
如图1所示,一种钣金零件凹陷制作方法,先将将钣金零件1、2、3搭接,形成搭接台阶;在搭接台阶的一侧加一辅助支撑面4;在搭接台阶的另一侧向辅助支撑面4的方向锤击施加钣金力C,使钣金零件3受到钣金料厚边缘的反向力,形成凹陷5。
以上显示和描述了本发明的基本原理和主要特征及其优点,本行业的技术人员应该了解,本发明不受上述实施例的限制,上述实施例和说明中描述的只是说明本发明的原理,在不脱离本发明精神和范围的前提下,本发明还会有各种变化和改进,这些变化和改进都落入要求保护的本发明范围内,本发明要求保护范围由所附的权利要求书及其等效方法界定。
Claims (2)
1.一种钣金零件凹陷制作方法,其特征在于包括以下步骤:(1)将钣金零件搭接,形成搭接台阶;(2)在搭接台阶的一侧加一辅助支撑面;(3)在搭接台阶的另一侧向辅助支撑面的方向锤击施加钣金力,钣金零件受到钣金料厚边缘的反向力,形成凹陷。
2.根据权利要求1所述的一种钣金零件凹陷制作方法,其特征在于:所述凹陷的深度与钣金料厚相同。