CN102086334A - 一种改进环氧氨基底漆 - Google Patents

一种改进环氧氨基底漆 Download PDF

Info

Publication number
CN102086334A
CN102086334A CN2009103109819A CN200910310981A CN102086334A CN 102086334 A CN102086334 A CN 102086334A CN 2009103109819 A CN2009103109819 A CN 2009103109819A CN 200910310981 A CN200910310981 A CN 200910310981A CN 102086334 A CN102086334 A CN 102086334A
Authority
CN
China
Prior art keywords
epoxy
primer
improved epoxy
epoxy amino
amino
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009103109819A
Other languages
English (en)
Inventor
张志云
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Tianjin Xinyu Color Plate Co Ltd
Original Assignee
Tianjin Xinyu Color Plate Co Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Tianjin Xinyu Color Plate Co Ltd filed Critical Tianjin Xinyu Color Plate Co Ltd
Priority to CN2009103109819A priority Critical patent/CN102086334A/zh
Publication of CN102086334A publication Critical patent/CN102086334A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种改进环氧氨基底漆,主要配方为:

Description

一种改进环氧氨基底漆
所属技术领域
本发明涉及一种材料涂漆,特别是一种改进环氧氨基底漆,适合于各种卷材钢板。
背景技术
目前,预涂卷材钢板用底漆主要采用环氧型或聚酯树脂型,硬度和抗磨擦及抗水煮性能方面不太理想,物理机械性能会随时间的延长而逐渐衰减。
发明内容
本发明所要解决的问题在于,克服现有底漆的缺点,提供了一种改进环氧氨基底漆。该底漆不仅提高了产品质量,,而且降低生产成本,使其生产工艺简单化,便于操作。
本发明采用的技术方案是:改进环氧氨基底漆配方为:
Figure B2009103109819D0000011
为了进一步提高产品的特性及要求,其最佳改进环氧氨基底漆配方为:
Figure B2009103109819D0000021
通过实施本发明,可以见到以下显著效果:
本发明不仅具有良好的硬度和抗磨擦及耐水煮性能,其他各项常规物理机械性能也达到彩板的实际使用要求,并能解决逐步衰减的物理机械性能的问题。
本发明的有益效果是,该底漆不仅提高了产品质量,而且降低生产成本,使其生产工艺简单化,便于操作。
具体实施方式
改进环氧氨基底漆配方为:
为了进一步提高产品的特性及要求,其最佳改进环氧氨基底漆配方为:
Figure B2009103109819D0000023
Figure B2009103109819D0000031
通过实施本发明,可以见到以下显著效果:
本发明不仅具有良好的硬度和抗磨擦及耐水煮性能,其他各项常规物理机械性能也达到彩板的实际使用要求,并能解决逐步衰减的物理机械性能的问题。

Claims (2)

1.一种改进环氧氨基底漆,其特征在于:改进环氧氨基底漆配方为:
Figure F2009103109819C0000011
2.根据权利要求1所述的一种改进环氧氨基底漆,其特征在于:其最佳配方为:
Figure F2009103109819C0000012
Figure F2009103109819C0000021
CN2009103109819A 2009-12-07 2009-12-07 一种改进环氧氨基底漆 Pending CN102086334A (zh)