CN102074746A - 一种铅酸蓄电池极群包覆pvc膜装壳技术 - Google Patents
一种铅酸蓄电池极群包覆pvc膜装壳技术 Download PDFInfo
- Publication number
- CN102074746A CN102074746A CN2010106024478A CN201010602447A CN102074746A CN 102074746 A CN102074746 A CN 102074746A CN 2010106024478 A CN2010106024478 A CN 2010106024478A CN 201010602447 A CN201010602447 A CN 201010602447A CN 102074746 A CN102074746 A CN 102074746A
- Authority
- CN
- China
- Prior art keywords
- pvc film
- pvc
- film
- polar group
- technology
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种铅酸蓄电池极群包覆PVC膜装壳技术,依以下步骤对极群包覆PVC膜并装壳:将PVC膜(1)平整的放置,把极群(2)放置到PVC膜(1)上,剰下PVC膜的另一半U型包覆到极群上,极群(2)和PVC膜(1)一起装入电池壳内,经过封盖、加酸、充电工序形成铅酸蓄电池。本发明的PVC膜保护了极板,使极板表面不受损伤,避免了极板表面铅膏被电池壳壁刮落,保存了活性物质,增加了电池装配压力,为提高电池装配压力提供了保证。
Description
技术领域
本发明涉及铅酸蓄电池极群装壳技术,具体涉及一种铅酸蓄电池极群包覆PVC膜装壳技术。
背景技术
在阀控密封铅酸蓄电池生产过程中,有一极群装壳过程,此过程是把铸焊好的极群按正确的极性分别装到电池壳内,在装壳时会经常出现边极板被刮伤和极板下压阻力大的问题,这样会使得电池出现极板松膏、正负极耳弯曲、隔板损坏等现象,最终导致电池失效,为了避免装壳时产生的这些问题,所以需要新的装壳方式。当前大部分情况是,减小隔板厚度降低装配压力,但这样就会有以下问题产生:1、大电流放电性能变差;2、容易出现枝筋短路;3、极板刮伤;4、表面活性物质脱落,活性物质量减小,容量变低。
发明内容
本发明的目的在于:提出一种铅酸蓄电池极群包覆PVC膜装壳技术,采用该极群包覆PVC膜装壳技术,不仅会减小装壳对极板损坏外,极群还可以在原来的基础上增加装配压力,提高电池性能。
本发明的技术解决方案是:在电池极群铸焊好后,外面U型包覆PVC膜,然后将PVC膜和极群一起装入电池壳内。
该极群包覆PVC膜装壳技术包括以下步骤:将PVC膜平整的放置,把极群放置到PVC膜上,剰下PVC膜的另一半U型包覆到极群上,极群和PVC膜一起装入电池壳内,经过封盖、加酸、充电工序形成铅酸蓄电池。
本发明具有以下优点:1、PVC膜保护了极板,使极板表面不受损伤;2、避免了极板表面铅膏被电池壳壁刮落,保存了活性物质;3、增加了电池装配压力;4、PVC膜装入壳内不需要拿下来,为提高电池装配压力提供了保证。
附图说明
图1为本发明的结构示意图。
图中:1、PVC包覆膜,2、极群。
具体实施方式
如图1所示,依以下步骤对极群包覆PVC膜并装壳:将PVC膜1平整的放置,把极群2放置到PVC膜1上,剰下PVC膜的另一半U型包覆到极群上,极群2和PVC膜1一起装入电池壳内,经过封盖、加酸、充电工序形成铅酸蓄电池。
Claims (1)
1. 一种铅酸蓄电池极群包覆PVC膜装壳技术,其特征在于依以下步骤对极群包覆PVC膜并装壳:将PVC膜(1)平整的放置,把极群(2)放置到PVC膜(1)上,剰下PVC膜的另一半U型包覆到极群上,极群(2)和PVC膜(1)一起装入电池壳内,经过封盖、加酸、充电工序形成铅酸蓄电池。