CN102022950A - 燃气热水器铝合金换热器水管的耐腐蚀处理方法 - Google Patents
燃气热水器铝合金换热器水管的耐腐蚀处理方法 Download PDFInfo
- Publication number
- CN102022950A CN102022950A CN 200910192586 CN200910192586A CN102022950A CN 102022950 A CN102022950 A CN 102022950A CN 200910192586 CN200910192586 CN 200910192586 CN 200910192586 A CN200910192586 A CN 200910192586A CN 102022950 A CN102022950 A CN 102022950A
- Authority
- CN
- China
- Prior art keywords
- heat exchanger
- aluminum alloy
- alloy heat
- water pipe
- heating furnace
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Granted
Abstract
一种燃气热水器铝合金换热器水管的耐腐蚀处理方法,主要技术特征是它由下列工步组成:首先在由铝合金材料制成的翅片、直管、弯管、盘管、水箱整体钎焊形成铝合金换热器后,再向铝合金换热器的水管内通入空气或氧气;然后将铝合金换热器放进200℃~600℃的加热炉内加热20分钟~120分钟进行氧化,形成致密氧化膜。具有能有效地提高燃气热水器铝合金换热器的耐腐蚀性,从而延长热水器的使用寿命等特点。
Description
技术领域:本发明涉及到一种燃气热水器铝合金换热器水管的耐腐蚀处理方法。
背景技术:目前,燃气热水器的换热器一直以来使用紫铜材料制作,由于铜资源越来越紧张,导致铜价迅速飙升,且我国是铜资源匮乏而铝资源丰富的国家,家电产品中开展以铝代铜的原材料应用的技术开发,可降低生产成本。但由于带有氯离子的自来水或一些地区使用的地下水通过燃气热水器的铝合金换热器时,会造成铝合金的均匀腐蚀和点蚀,尤其是点蚀会造成水管的腐蚀穿孔,致使存在铝换热器耐腐蚀较差,热水器使用寿命不长等缺陷。为了克服这些缺陷,对燃气热水器铝合金换热器水管的耐腐蚀处理方法进行了研制。
发明内容:本发明所要解决的技术问题是要提供一种燃气热水器铝合金换热器水管的耐腐蚀处理方法,它能有效地提高燃气热水器铝合金换热器的耐腐蚀性,从而延长热水器的使用寿命。
本发明解决其技术问题采用的技术方案是:它由下列工步组成:首先在由铝合金材料制成的翅片、直管、弯管、盘管、水箱整体钎焊形成铝合金换热器后,再向铝合金换热器的水管内通入空气或氧气;然后将铝合金换热器放进200℃~600℃的加热炉内加热20分钟~120分钟进行氧化,形成致密氧化膜。
所述致密氧化膜的厚度为15~30μm。
在由铝合金材料制成的翅片、直管、弯管、盘管、水箱整体钎焊形成铝合金换热器后,通过气枪向铝合金换热器的水管内通入空气或氧气。
所述的加热炉为链式加热炉。
向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进400℃的加热炉内加热。
向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进加热炉内加热60分钟。
本发明同背景技术相比所产生的有益效果:
1、由于本发明采用首先在由铝合金材料制成的翅片、直管、弯管、盘管、水箱整体钎焊形成铝合金换热器后,再向铝合金换热器的水管内通入空气或氧气;然后将铝合金换热器放进200℃~600℃的加热炉内加热20分钟~120分钟进行氧化,形成致密氧化膜的耐腐蚀处理方法,故它能有效地提高燃气热水器铝合金换热器的耐腐蚀性,从而延长热水器的使用寿命。
附图说明:图1为本发明中铝合金换热器的结构示意图。
具体实施方式:参看附图1所示,由铝合金材料制成的翅片1、直管2、弯管3、盘管4、水箱5等部件整体钎焊形成铝合金换热器后,用气枪把空气或氧气充入铝合金的水管内,然后把铝合金换热器放进200℃~600℃的加热炉内加热一段时间进行氧化,加热炉为链式加热炉,可选200℃、300℃、400℃、500℃、600℃等加热温度,放置时间为20分钟~120分钟,可选30分钟、60分钟、90分钟、120分钟等,使水管内壁加速氧化且氧化膜不断加厚,形成15~30μm的致密晶体结构,形成具有更良好保护性能的致密氧化膜。
Claims (10)
1.一种燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于它由下列工步组成:
首先在由铝合金材料制成的翅片(1)、直管(2)、弯管(3)、盘管(4)、水箱(5)整体钎焊形成铝合金换热器后,再向铝合金换热器的水管内通入空气或氧气;
然后将铝合金换热器放进200℃~600℃的加热炉内加热20分钟~120分钟进行氧化,形成致密氧化膜。
2.根据权利要求1所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于所述致密氧化膜的厚度为15~30μm。
3.根据权利要求1或2所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于在由铝合金材料制成的翅片(1)、直管(2)、弯管(3)、盘管(4)、水箱(5)整体钎焊形成铝合金换热器后,通过气枪向铝合金换热器的水管内通入空气或氧气。
4.根据权利要求1或2所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于所述的加热炉为链式加热炉。
5.根据权利要求3所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于所述的加热炉为链式加热炉。
6.根据权利要求1或2所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进400℃的加热炉内加热。
7.根据权利要求5所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进400℃的加热炉内加热。
8.根据权利要求1或2所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进加热炉内加热60分钟。
9.根据权利要求6所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进加热炉内加热60分钟。
10.根据权利要求7所述的燃气热水器铝合金换热器水管的耐腐蚀处理方法,其特征在于向铝合金换热器的水管内通入空气或氧气后,将铝合金换热器放进加热炉内加热60分钟。