CN102002928A - 一种硬岩与软岩混合的面板坝堆石料 - Google Patents

一种硬岩与软岩混合的面板坝堆石料 Download PDF

Info

Publication number
CN102002928A
CN102002928A CN2009103063425A CN200910306342A CN102002928A CN 102002928 A CN102002928 A CN 102002928A CN 2009103063425 A CN2009103063425 A CN 2009103063425A CN 200910306342 A CN200910306342 A CN 200910306342A CN 102002928 A CN102002928 A CN 102002928A
Authority
CN
China
Prior art keywords
rock
soft
hard rock
hard
dam
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2009103063425A
Other languages
English (en)
Inventor
湛正刚
范福平
蔡大咏
慕洪友
杨泽艳
刘雯
张合作
敖大华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Hydrochina Guiyang Engineering Corp
Original Assignee
Hydrochina Guiyang Engineering Corp
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hydrochina Guiyang Engineering Corp filed Critical Hydrochina Guiyang Engineering Corp
Priority to CN2009103063425A priority Critical patent/CN102002928A/zh
Publication of CN102002928A publication Critical patent/CN102002928A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种硬岩与软岩混合的面板坝堆石料,它由硬岩与软岩混合而成;硬岩所占质量百分比为60%~80%,软岩所占质量百分比为40%~20%。本发明采用硬岩与软岩的混合料用作面板坝堆石料,料源选择空间更大,满足了就地取材的原则,不需要选择运距较远的料场进行运输,这样运距短,投资省,经济可行,而且面板坝堆石料的结构较稳定,突破了面板坝在常规料源选择上的局限性。本发明能用于面板坝主堆石区及次堆石区,具有显著的经济效益和社会效益。

Description

一种硬岩与软岩混合的面板坝堆石料
技术领域
本发明涉及一种面板坝堆石料,特别是一种由硬岩与软岩混合而成的面板坝堆石料。
背景技术
在水利水电工程中,因灌溉取水或发电等需要,通常要筑坝形成水库。坝主要有混凝土坝及堆石坝等类型,堆石坝中常用的坝型有心墙堆石坝及钢筋混凝土面板堆石坝(以下简称面板坝)。面板坝主体分为主堆石区及次堆石区进行填筑,堆石料通常采用硬岩(饱和抗压强度大于30MPa)筑坝,一般要求具有低压缩、高密度、高抗剪强度及自由排水等性能,有时在次堆石区采用软岩(饱和抗压强度小于30MPa)填筑。面板坝堆石料的选择主要考虑就地取材的原则,这样运距短,投资省。面板坝料源选择方面,有的工程能满足传统要求,有的工程则不能满足,此时,若选择运距较远的料场,将增加运距,增大工程投资。
发明内容
本发明所要解决的技术问题在于提供一种料源选择空间更大、经济性好的硬岩与软岩混合的面板坝堆石料,从而克服面板坝在常规料源选择上的局限性。
为解决上述技术问题,本发明的技术方案:一种硬岩与软岩混合的面板坝堆石料。该面板坝堆石料是由硬岩与软岩混合而成;其中硬岩所占质量百分比较好的是60%~80%,软岩所占质量百分比较好的是40%~20%。
上述的硬岩与软岩混合的面板坝堆石料中,硬岩所占质量百分比更好的是70%,软岩所占质量百分比更好的是30%。
前述的硬岩与软岩混合的面板坝堆石料中,硬岩与软岩是混合在一起的,包括岩性自然组合和人工混合两种。
本发明的有益效果:与现有技术相比,本发明采用硬岩与软岩的混合料用作面板坝堆石料,料源选择空间更大,满足了就地取材的原则,不需要选择运距较远的料场进行运输,这样运距短,投资省,经济可行,而且面板坝堆石料的结构较稳定,突破了面板坝在常规料源选择上的局限性。本发明能用于面板坝主堆石区及次堆石区,具有显著的经济效益和社会效益。
经过大量的试验研究和分析计算并通过具体应用和验证,本发明中的硬岩的质量百分比最好的是占70%,软岩占30%,因为过多的软岩筑坝可能使坝体沉降偏大,造成面板坝结构性裂缝,不能满足坝体结构稳定要求。硬岩与软岩是混合在一起的,包括岩性自然组合和人工混合两种。硬岩饱和抗压强度为30MPa以上,软岩的饱和抗压强度为30MPa以下。
下面结合具体实施方式对本发明作进一步的说明。
具体实施方式
实施例1。将现场爆破开挖的硬岩与软岩混合,其中的硬岩所占质量百分比为70%,软岩所占质量百分比为30%。硬岩与软岩是混合在一起的,混合方式包括岩性自然组合和人工混合两种。硬岩饱和抗压强度为30MPa以上,软岩的饱和抗压强度为30MPa以下。
堆砌面板堆石坝时,用汽车将上述由硬岩与软岩混合而成的面板坝堆石料运至面板堆石坝堆石区,采用推土机铺平,层厚80cm,然后洒水15%,采用25t重型振动碾碾压8~10遍,满足孔隙率15~20%的要求。继续上述步骤,直至填筑完成。
实施例2。将现场爆破开挖的硬岩与软岩混合,其中的硬岩所占质量百分比为80%,软岩所占质量百分比为20%。硬岩与软岩是混合在一起的,混合方式包括岩性自然组合和人工混合两种。硬岩饱和抗压强度为30MPa以上,软岩的饱和抗压强度为30MPa以下。
堆砌面板堆石坝时,用汽车将上述由硬岩与软岩混合而成的面板坝堆石料运至面板堆石坝堆石区,采用推土机铺平,层厚80cm,然后洒水15%,采用25t重型振动碾碾压8~10遍,满足孔隙率15~20%的要求。继续上述步骤,直至填筑完成。
实施例3。将现场爆破开挖的硬岩与软岩混合,其中的硬岩所占质量百分比为60%,软岩所占质量百分比为40%。硬岩与软岩是混合在一起的,混合方式包括岩性自然组合和人工混合两种。硬岩饱和抗压强度为30MPa以上,软岩的饱和抗压强度为30MPa以下。
堆砌面板堆石坝时,用汽车将上述由硬岩与软岩混合而成的面板坝堆石料运至面板堆石坝堆石区,采用推土机铺平,层厚80cm,然后洒水15%,采用25t重型振动碾碾压8~10遍,满足孔隙率15~20%的要求。继续上述步骤,直至填筑完成。
本发明的实施方式不限于上述实施例,在不脱离本发明宗旨的前提下做出的各种变化均属于本发明的保护范围之内。

Claims (3)

1.一种硬岩与软岩混合的面板坝堆石料,其特征在于:由硬岩与软岩混合而成;硬岩所占质量百分比为60%~80%,软岩所占质量百分比为40%~20%。
2.根据权利要求1所述的硬岩与软岩混合的面板坝堆石料,其特征在于:所述的硬岩所占质量百分比为70%,软岩所占质量百分比为30%。
3.根据权利要求1所述的硬岩与软岩混合的面板坝堆石料,其特征在于:所述的硬岩与软岩是混合在一起的,包括岩性自然组合和人工混合两种。
CN2009103063425A 2009-08-31 2009-08-31 一种硬岩与软岩混合的面板坝堆石料 Pending CN102002928A (zh)