CN101973108A - 一种能够提高成型产品外观质量的模具结构 - Google Patents
一种能够提高成型产品外观质量的模具结构 Download PDFInfo
- Publication number
- CN101973108A CN101973108A CN2010102617169A CN201010261716A CN101973108A CN 101973108 A CN101973108 A CN 101973108A CN 2010102617169 A CN2010102617169 A CN 2010102617169A CN 201010261716 A CN201010261716 A CN 201010261716A CN 101973108 A CN101973108 A CN 101973108A
- Authority
- CN
- China
- Prior art keywords
- cooling water
- cooling jacket
- cooling
- quiet module
- static module
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开一种能够提高成型产品外观质量的模具结构,该模具结构包括静模块和热咀。热咀外周套有冷却水套,热咀末端的咀尖露于冷却水套外。冷却水套置于静模块内,静模块和冷却水套之间留有冷却水路,冷却水路的进水管、出水管并行设置在静模块内。进水管、出水管接入冷却水套外侧壁向下方延伸的两流水槽,两流水槽的下部由冷却水套下部的环形水槽连通。此种模具结构,由静模块和冷却水套共同构成的冷却水路,相比单纯在静模块上布置冷却水管路,冷却水路距离静模块的产品成型面的距离相比于常规模具更近,达到了10~14毫米,产品的冷却效率显著提升,模具的整体强度和耐久性无任何影响。
Description
技术领域
本发明涉及一种模具结构,具体涉及一种能够提高成型产品外观质量的模具结构。
背景技术
热流道注塑模具,热咀的前端部直接点在产品表面进胶。熔融塑料注射完成后,由于热咀上有加热元件,致使热咀周边区域的模具温度高于其它区域。需要对该高温区域做特殊的降温处理,在热咀周围的模具上开冷却水管路是一种常用的解决方式。但冷却水管路的布置一方面要考虑冷却的效果,另一方面需要考虑模具开冷却水管路后的强度。此种模具结构整体冷却还不够均匀,特别是热咀附近的冷却与其它区域的冷却速度不同步,成型后产品在热咀附近容易出现色差,影响成型产品的外观质量。
发明内容
本发明的目的在于提供一种能够提高成型产品外观质量的模具结构,该模具具有结构简单,成型产品外观色度均匀,无色差。
本发明为实现上述目的,采用的技术解决方案是:
一种能够提高成型产品外观质量的模具结构,包括静模块和热咀,热咀外周套有冷却水套,热咀末端的咀尖露于冷却水套外,冷却水套置于静模块内,静模块和冷却水套之间留有冷却水路,冷却水路的进水管、出水管并行设置在静模块内,进水管、出水管接入冷却水套外侧壁向下方延伸的两流水槽,两流水槽的下部由冷却水套下部的环形水槽连通。
上述冷却水套底部距离静模块的产品成型面的尺寸在10~14毫米之间。
上述冷却水套通过螺栓紧固在静模块上。
上述冷却水套和静模块之间设置有密封胶圈。
本发明的有益效果:
传统模具的冷却水管路,由于加工工艺的限制,在模具内是布置在同一个平面上的。若冷却水管路距离产品成型面太近,静模块上穿管较多,静模块的表面强度势必要大大降低,模具使用寿命较短。此种模具结构,静模块和冷却水套之间形成立体结构的冷却水路,仅在热咀末端的咀尖周围形成环形管路,保证了模具的整体强度,冷却水路加工方式简便,而且冷却效果较好,成型产品外观色度均匀,无色差。
此种模具结构,由静模块和冷却水套共同构成的冷却水路,相比单纯在静模块上布置冷却水管路,冷却水路距离静模块的产品成型面的距离相比于常规模具更近,达到了10~14毫米,产品的冷却效率显著提升,模具的整体强度和耐久性无任何影响。
附图说明
图1为模具结构的结构示意图。
图2为冷却水套的正面图。
图3为冷却水套的立体图。
具体实施方式
下面结合图1至图3,对本发明进行详细说明:
一种能够提高成型产品外观质量的模具结构,包括静模块1和热咀2。热咀2外周套有冷却水套3,热咀2末端的咀尖4露于冷却水套3外。冷却水套3置于静模块1内,静模块1和冷却水套3之间留有冷却水路5,冷却水路5的进水管、出水管并行设置在静模块1内。进水管、出水管接入冷却水套3外侧壁向下方延伸的两流水槽6,两流水槽6的下部由冷却水套下部的环形水槽7连通。冷却水套3底部距离静模块1的产品成型面8的尺寸为10、12或14毫米。冷却水套3通过螺栓紧固在静模块1上。冷却水套3和静模块1之间设置有密封胶圈9。
使用过程中,冷却水由静模块内的进水管进入冷却水套外侧壁上的竖直流水槽,经过冷却水套下部的环形水槽后,再流入冷却水套外侧壁上的另一竖直流水槽,最后通过静模块内的出水管流出,实现对热咀末端部的冷却。通过调节冷却水的温度,可以调节该部位的冷却速度,尽可能的使该部位温度下降速度与模具的其它部位的一致,成型产品外观质量高。
当然,上述说明并非是对本发明的限制,本发明也并不仅限于上述举例,本技术领域的技术人员在本发明的实质范围内所做出的变化、改型、添加或替换,也应属于本发明的保护范围。
Claims (4)
1.一种能够提高成型产品外观质量的模具结构,包括静模块和热咀,其特征在于:所述热咀外周套有冷却水套,热咀末端的咀尖露于冷却水套外,冷却水套置于静模块内,静模块和冷却水套之间留有冷却水路,冷却水路的进水管、出水管并行设置在静模块内,进水管、出水管接入冷却水套外侧壁向下方延伸的两流水槽,两流水槽的下部由冷却水套下部的环形水槽连通。
2.根据权利要求1所述的一种能够提高成型产品外观质量的模具结构,其特征在于:所述冷却水套底部距离静模块的产品成型面的尺寸在10~14毫米之间。
3.根据权利要求1所述的一种能够提高成型产品外观质量的模具结构,其特征在于:所述冷却水套通过螺栓紧固在静模块上。
4.根据权利要求1至3任一项所述的一种能够提高成型产品外观质量的模具结构,其特征在于:所述冷却水套和静模块之间设置有密封胶圈。