CN101969143A - 一种纳米高能免维护铅酸蓄电池的制备方法 - Google Patents

一种纳米高能免维护铅酸蓄电池的制备方法 Download PDF

Info

Publication number
CN101969143A
CN101969143A CN2010102912691A CN201010291269A CN101969143A CN 101969143 A CN101969143 A CN 101969143A CN 2010102912691 A CN2010102912691 A CN 2010102912691A CN 201010291269 A CN201010291269 A CN 201010291269A CN 101969143 A CN101969143 A CN 101969143A
Authority
CN
China
Prior art keywords
battery
lead
battery case
nano
grid
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN2010102912691A
Other languages
English (en)
Inventor
陈国培
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Individual
Original Assignee
Individual
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Individual filed Critical Individual
Priority to CN2010102912691A priority Critical patent/CN101969143A/zh
Publication of CN101969143A publication Critical patent/CN101969143A/zh
Pending legal-status Critical Current

Abstract

本发明公开了一种纳米高能免维护铅酸蓄电池的制备方法,包括以下步骤:(1)在用纳米陶瓷粉和铅金属粉材料制成的格状板栅表面设一超细玻璃纤维层,然后在超细玻璃纤维层上再涂覆一层均匀的铅膏,将若干由格状板栅、铅膏和超细玻璃纤维层构成的极板单元,叠合构成层状结构,制成电池芯;(2)选用两组由单磁体材料制成的电极,两组电极分置于电池芯的左右两端;(3)安装电池盒、盒盖与端子。本发明纳米陶瓷板栅的使用可以有效增加极板的机械强度,提高其导电性能;而采用单磁体材料作为极板间的连接材料,可以有效减少充电时间,提高充电效率;此外,由于采用复合板栅,使得参与电化转换的组分有效增加,从而大幅度提高蓄电池的容量。

Description

一种纳米高能免维护铅酸蓄电池的制备方法
技术领域
本发明涉及一种纳米高能免维护铅酸蓄电池的制备方法。
背景技术
近年来,随着汽车工业、电信及IT网络等基础设施,动力车辆以及再生能源产业的飞速发展,作为首选的铅酸蓄电池及其电池工业得到了快速的发展。由于国际市场对铅酸蓄电池的需求量不断加大,欧盟、美国等发达国家出于保护本国环境的敏感,早已限制铅酸蓄电池制造业在本国的生产,转而向发展中国家采购。中国已成为目前世界上最大的铅酸蓄电池出口国之一。随着我国对新型能源的日益重视,安全高效节能的铅酸蓄电池受到越来越广泛的关注。而目前市场上现有的铅酸蓄电池普遍存在容量不高、性价比差、使用寿命短等缺陷,已无法满足现有的市场需求。
发明内容
本发明所要解决的技术问题就是提供一种纳米高能免维护铅酸蓄电池的制备方法,制备出的铅酸蓄电池免维护、容量高、体积小、重量轻,且耐震动性好、耐冲击性强、使用寿命长。
为解决上述技术问题,本发明采用如下技术方案:一种纳米高能免维护铅酸蓄电池的制备方法,其特征在于制备过程包括以下步骤:
(1)在用纳米陶瓷粉和铅金属粉材料制成的格状板栅表面设一超细玻璃纤维层,然后在超细玻璃纤维层上再涂覆一层均匀的铅膏,将如此若干由格状板栅、铅膏和超细玻璃纤维层构成的极板单元,叠合构成层状结构,制成所需的电池芯;
(2)选用两组由单磁体材料制成的电极,每组电极由连体的横、竖棒构成倒“T”字形状,其中竖棒为外接线端子,置于壳体内的横棒则作为极板连接体,两组电极分置于电池芯的左右两端,并将横棒分别与每个极板单元的板栅连接;
(3)安装电池盒、盒盖与端子,将电池芯与电极组合体装入电池盒,端子设于电池盒的两端,一端端子设于电池盒底部中心,另一端端子穿出盒盖并通过盒盖封装于电池盒上。
进一步的,所述纳米陶瓷粉与铝金属粉混合制成的格状板栅,其单位面积电阻值0.003Ω/cm2
本发明研制而成的纳米高能免维护铅酸蓄电池,采用纳米陶瓷、金属材料作为蓄电池极板的板栅,然后涂覆一层均匀的铅膏,再在相邻的板栅与铅膏组合体之间,间隔一道超细玻璃纤维层;然后再将由单磁体材料制成的电极分别与每个极板单元的板栅连接。其中,纳米陶瓷板栅的使用可以有效增加极板的机械强度,提高其导电性能,提高蓄电池的工作性能;而采用单磁体材料作为极板间的连接材料,可以有效减少充电时间,提高充电效率,并可实现大电流快速充电。此外,由于采用复合板栅取代传统的纯铅板栅,使得参与电化转换的组分有效增加,从而大幅度提高蓄电池的容量。本发明进一步完善了铅酸蓄电池的各项能力,具有高温特性好、比能量高、环境无污染、性价比高等优点,是一种极具发展前途的二次新型能源装置。
具体实施方式
实施例,一种纳米高能免维护铅酸蓄电池的制备方法,其特征在于制备过程包括以下步骤:
(1)在用纳米陶瓷粉和铅金属粉材料制成的格状板栅表面设一超细玻璃纤维层,然后在超细玻璃纤维层上再涂覆一层均匀的铅膏,将如此若干由格状板栅、铅膏和超细玻璃纤维层构成的极板单元,叠合构成层状结构,制成所需的电池芯;
(2)选用两组由单磁体材料制成的电极,每组电极由连体的横、竖棒构成倒“T”字形状,其中竖棒为外接线端子,置于壳体内的横棒则作为极板连接体,两组电极分置于电池芯的左右两端,并将横棒分别与每个极板单元的板栅连接;
(3)安装电池盒、盒盖与端子,将电池芯与电极组合体装入电池盒,端子设于电池盒的两端,一端端子设于电池盒底部中心,另一端端子穿出盒盖并通过盒盖封装于电池盒上。
其中,盒盖上设有安全阀及阀盖,两端端子分别向内连接有汇流排,汇流排与端子间设有密封垫片,电池盒底部设有用于注入电解液的阀孔,阀孔上设工艺塞堵。

Claims (2)

1.一种纳米高能免维护铅酸蓄电池的制备方法,其特征在于制备过程包括以下步骤:
(1)在用纳米陶瓷粉和铅金属粉材料制成的格状板栅表面设一超细玻璃纤维层,然后在超细玻璃纤维层上再涂覆一层均匀的铅膏,将如此若干由格状板栅、铅膏和超细玻璃纤维层构成的极板单元,叠合构成层状结构,制成所需的电池芯;
(2)选用两组由单磁体材料制成的电极,每组电极由连体的横、竖棒构成倒“T”字形状,其中竖棒为外接线端子,置于壳体内的横棒则作为极板连接体,两组电极分置于电池芯的左右两端,并将横棒分别与每个极板单元的板栅连接;
(3)安装电池盒、盒盖与端子,将电池芯与电极组合体装入电池盒,端子设于电池盒的两端,一端端子设于电池盒底部中心,另一端端子穿出盒盖并通过盒盖封装于电池盒上。
2.根据权利要求1所述的一种纳米高能免维护铅酸蓄电池的制备方法,其特征在于:所述纳米陶瓷粉与铝金属粉混合制成的格状板栅,其单位面积电阻值0.003Ω/cm2
CN2010102912691A 2010-09-21 2010-09-21 一种纳米高能免维护铅酸蓄电池的制备方法 Pending CN101969143A (zh)