CN101875583B - 凹凸棒固体水插花泥及其生产方法 - Google Patents

凹凸棒固体水插花泥及其生产方法 Download PDF

Info

Publication number
CN101875583B
CN101875583B CN2010101326503A CN201010132650A CN101875583B CN 101875583 B CN101875583 B CN 101875583B CN 2010101326503 A CN2010101326503 A CN 2010101326503A CN 201010132650 A CN201010132650 A CN 201010132650A CN 101875583 B CN101875583 B CN 101875583B
Authority
CN
China
Prior art keywords
attapulgite
solid water
mud
flowers
attapulgite clay
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Active
Application number
CN2010101326503A
Other languages
English (en)
Other versions
CN101875583A (zh
Inventor
蒋文兰
吴宏敬
朱勇
许庆华
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
Nantong Jinmao Explosion-proof Electrical Co., Ltd.
Original Assignee
蒋文兰
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 蒋文兰 filed Critical 蒋文兰
Priority to CN2010101326503A priority Critical patent/CN101875583B/zh
Publication of CN101875583A publication Critical patent/CN101875583A/zh
Application granted granted Critical
Publication of CN101875583B publication Critical patent/CN101875583B/zh
Active legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明公开了一种凹凸棒固体水插花泥及其生产方法,其技术方案的要点是,凹凸棒固体水插花泥由高粘凹凸棒石粘土粉、膨润土粉、颗粒状高吸水树脂、尿素、磷酸二氢钾和去离子水组成。先将尿素和磷酸二氢钾加入去离子水中进行搅拌,将高粘凹凸棒石粘土粉和膨润土粉加入搅拌机内进行搅拌为半成品,将半成品加入透明的容器内后,再将固体水加在半成品的上面,组成凹凸棒固体水插花泥的成品。凹凸棒固体水插花泥层次分明,上部为晶莹透亮的固体水,下部为粘度高保水性强的凹凸棒插花泥,含有鲜花生长所需要的营养成分,确保插入凹凸棒固体水插花泥的鲜花挺立美观,提高其观赏效果。凹凸棒固体水插花泥适用于花店、宾馆、写字楼及家庭对鲜花进行保鲜。

Description

凹凸棒固体水插花泥及其生产方法
技术领域
本发明涉及插花泥,具体涉及一种凹凸棒固体水插花泥及其生产方法。
背景技术
水晶泥是高吸水树脂吸水后形成的块状弹性凝胶体,是一种新型无土栽培花草的新材料,它不仅取代了肮脏的泥土,而且集时尚、美观、环保和便捷于一体。水晶泥盆景特别适合家庭、宾馆、酒店、酒吧、歌舞厅、西餐厅、茶艺馆等作为装饰摆设,也可作为送礼之佳品。
水晶泥用于插花的不足之处是:(1)水晶泥是一种块状弹性凝胶体,相互之间呈松散状,花草植物很难直立在水晶泥之中,影响观赏效果;(2)水晶泥内不含花草植物所需要的营养成份,花草植物所需要的营养是依靠容器内的水提供,花草植物生长过程受到抑制;(3)水晶泥很容易干涸,造成鲜花和枝叶很快就会凋谢。
发明内容
本发明的目的是克服现有技术中不足之处,提供一种凹凸棒固体水插花泥及其生产方法。
凹凸棒固体水插花泥由高粘凹凸棒石粘土粉、膨润土粉、颗粒状高吸水树脂、尿素、磷酸二氢钾和去离子水组成。先将尿素和磷酸二氢钾加入去离子水中进行搅拌,将高粘凹凸棒石粘土粉和膨润土粉加入搅拌机内进行搅拌为半成品,将半成品加入透明的容器内后,再将固体水加在半成品的上面,组成凹凸棒固体水插花泥的成品。
凹凸棒石粘土在含水的情况下具有较高的可塑性,稳定性好,凹凸棒石粘土的硬度为莫氏2~3度;凹凸棒石粘土潮湿时呈粘性,粘度可达到3000mPa·s以上,凹凸棒石粘土干燥后收缩率小,且不产生龟裂。高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的粉状凹凸棒石粘土。
膨润土具有强的吸湿性和膨胀性,可吸附8~15倍于自身体积的水量,体积膨胀可达数倍至30倍;在水介质中能分散成胶凝状和悬浮状。
高吸水树脂的吸水倍率可达自身重量的数百倍甚至上千倍,所述颗粒状高吸水树脂是选用颗粒直径大于2毫米的高吸水树脂。
尿素外观呈白色晶体或粉末,易溶于水,是一种高浓度氮肥。
磷酸二氢钾是一种速效磷钾复合肥,其外观为白色晶体,性质稳定,易溶于水,极易被植物吸收利用。
本发明通过下述技术方案予以实现:
1、凹凸棒固体水插花泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉25~50%、膨润土粉5~25%、固体水1~20%、尿素0.01~1%、磷酸二氢钾0.01~1%和去离子水10~35%;
所述固体水的配料按重量百分比由下列组分组成:颗粒状高吸水树脂0.1~2%和去离子水98~99.9%;
所述膨润土粉的颗粒细度小于0.074毫米。
2、凹凸棒固体水插花泥的生产方法:(1)先将去离子水加入搅拌机内,再将尿素和磷酸二氢钾加入去离子水中进行搅拌;(2)当尿素和磷酸二氢钾溶于去离子水中后,将高粘凹凸棒石粘土粉和膨润土粉加入搅拌机内进行搅拌,搅拌混合均匀后为凹凸棒固体水插花泥的半成品;(3)先将凹凸棒固体水插花泥的半成品加入透明的容器内后,再将固体水加在凹凸棒固体水插花泥半成品的上面,组成凹凸棒固体水插花泥的成品。
所述固体水的生产方法:将颗粒状高吸水树脂加入去离子水中进行浸泡,颗粒状高吸水树脂吸入去离子水后,逐渐膨胀为不规则的块状高吸水树脂凝胶体,这些块状高吸水树脂凝胶体内含有大量的去离子水,因此,这种高吸水树脂凝胶体称为固体水,直径大于2毫米的高吸水树脂,吸入去离子水后能逐渐膨胀到8毫米以上的块状高吸水树脂凝胶体。
所述高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,其特征在于,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
上述生产工艺是采用由本发明人于2005年6月20日申请的“提高凹凸棒石粘土粘度的加工工艺”,中国专利授权公告号为:CN 1317067C,授权公告日:2007年5月23日。
凹凸棒固体水插花泥层次分明,上部为晶莹透亮的固体水,根据鲜花对水分的需要,能不间断缓慢的释放出固体水内的水分;下部为粘度高保水性强的凹凸棒插花泥,含有鲜花生长所需要的营养成分,有利于枝叶的正常生长和延长花期不凋谢,确保插入凹凸棒固体水插花泥的鲜花挺立美观,提高其观赏效果。
凹凸棒固体水插花泥适用于花店、宾馆、写字楼及家庭种植鲜花和对鲜花进行保鲜。
具体实施方式
下面结合实施例对本发明作进一步的描述:
1、凹凸棒固体水插花泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉36%、膨润土粉18%、固体水16%、尿素0.3%、磷酸二氢钾0.2%和去离子水29.5%;
所述固体水的配料按重量百分比由下列组分组成:颗粒状高吸水树脂0.6%和去离子水99.4%。
2、凹凸棒固体水插花泥的生产方法:(1)先将去离子水加入搅拌机内,再将尿素和磷酸二氢钾加入去离子水中进行搅拌;(2)当尿素和磷酸二氢钾溶于去离子水中后,将高粘凹凸棒石粘土粉和膨润土粉加入搅拌机内进行搅拌,搅拌混合均匀后为凹凸棒固体水插花泥的半成品;(3)先将凹凸棒固体水插花泥的半成品加入透明的容器内后,再将固体水加在凹凸棒固体水插花泥半成品的上面,组成凹凸棒固体水插花泥的成品。

Claims (1)

1.一种凹凸棒固体水插花泥,其特征在于,凹凸棒固体水插花泥的配料按重量百分比由下列组分组成:高粘凹凸棒石粘土粉25~50%、膨润土粉5~25%、固体水1~20%、尿素0.01~1%、磷酸二氢钾0.01~1%和去离子水10~35%;
所述固体水的配料按重量百分比由下列组分组成:颗粒状高吸水树脂0.1~2%和去离子水98~99.9%;
所述膨润土粉的颗粒细度小于0.074毫米;
所述凹凸棒固体水插花泥的生产方法:(1)先将去离子水加入搅拌机内,再将尿素和磷酸二氢钾加入去离子水中进行搅拌;(2)当尿素和磷酸二氢钾溶于去离子水中后,将高粘凹凸棒石粘土粉和膨润土粉加入搅拌机内进行搅拌,搅拌混合均匀后为凹凸棒固体水插花泥的半成品;(3)先将凹凸棒固体水插花泥的半成品加入透明的容器内后,再将固体水加在凹凸棒固体水插花泥半成品的上面,组成凹凸棒固体水插花泥的成品;
所述固体水的生产方法:将颗粒状高吸水树脂加入去离子水中进行浸泡,颗粒状高吸水树脂吸入去离子水后,逐渐膨胀为不规则的块状高吸水树脂凝胶体,这些块状高吸水树脂凝胶体内含有大量的去离子水为固体水;
所述高粘凹凸棒石粘土粉是采用提高凹凸棒石粘土粘度的加工工艺生产的凹凸棒石粘土,其特征在于,从矿区开采的凹凸棒石粘土,需要经过30~120天的自然风化;改性处理方法是:以重量百分比计算,取自然风化后的凹凸棒石粘土94~98%,均匀加入2~6%碳酸钠,共同输入浸泡池中,加入清水进行浸泡陈化,浸泡时间为72~120小时;取浸泡后的凹凸棒石粘土,输入搅拌机中进行搅拌,并将搅拌后的凹凸棒石粘土,经挤压机挤成薄片,其厚度控制在0.5~2毫米,将凹凸棒石粘土薄片,进行晾晒,晾晒后的凹凸棒石粘土薄片,其含水量≤15%;配料以重量百分比计算:晾晒后的凹凸棒石粘土94~98%、高吸水树脂0.5~5%和纤维素0.5~3%,将上述配料进行搅拌,搅拌均匀后输入磨机中进行磨粉,颗粒细度≤0.074毫米。
CN2010101326503A 2010-03-26 2010-03-26 凹凸棒固体水插花泥及其生产方法 Active CN101875583B (zh)