CN101824882B - 外墙保温装饰板制造工艺 - Google Patents
外墙保温装饰板制造工艺 Download PDFInfo
- Publication number
- CN101824882B CN101824882B CN2009100164689A CN200910016468A CN101824882B CN 101824882 B CN101824882 B CN 101824882B CN 2009100164689 A CN2009100164689 A CN 2009100164689A CN 200910016468 A CN200910016468 A CN 200910016468A CN 101824882 B CN101824882 B CN 101824882B
- Authority
- CN
- China
- Prior art keywords
- heat insulating
- thermal insulating
- decorative panel
- panel
- wall
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Expired - Fee Related
Abstract
一种外墙保温装饰板制造工艺,涉及一种外墙体装饰板材生产技术。该制造工艺采用复合材料高温高压成型工艺,注射聚氨酯发泡工艺使保温材料与装饰板腔体严密结合;其工艺步骤如包括:1、模具内成型,2、保温材料填充,3、板面喷涂:4、干燥,5、表面后处理,获得外墙保温装饰一体板。本发明制造工艺简便易行,制作成本低,工作效率高,无放射性元素,不污染生存空间。所生产外墙保温装饰一体板重量轻,减轻了墙体承重,不受环境温度制约,缩短施工周期。达到了坚实耐用,美观保温,环保节能的最佳效果。
Description
技术领域
本发明涉及一种外墙体装饰板材生产技术。
技术背景
目前,墙外保温结构是在外墙基层上用粘接砂浆粘结保温板,在保温板外侧固定钢筋焊架和金属网。再按间隔布置若干个锚钉垂直穿过金属网,钢筋焊架,保温板,粘结砂浆层至墙基层进行紧固。在金属网外抹一层砂浆层,再粘结装饰材料。所用装饰材料通常为大理石,面砖,涂料。涂料使用寿命短,易褪色;大理石与面砖生产工艺复杂,安装工序繁杂,墙体承重大,工作强度大,环境温度影响力大,施工周期长,牢固性差,费工费时费力成本高。多年来,建筑行业急需研制一种专用的外墙体装饰板材。
发明内容
本发明的目的是提供一种外墙保温装饰板制造工艺,以解决现有技术中生产工艺复杂,安装工序繁琐,墙体承重大,工作强度大,受环境温度制约力大,施工周期长,牢固性差,费工费时,成本高,使用寿命短,易褪色等问题。
本发明解决其技术问题的技术方案是采用高分子树脂、玻璃纤维增强复合材料,高温高压成型工艺,注射聚氨酯发泡工艺使保温材料与墙板腔体严密结合,获得外墙保温装饰一体板材;其工艺步骤如下:
1、高分子复合材料成型:外墙保温装饰板通过模具高温高压成型制作出墙板基材。其上面板的凹凸造型,装饰板一端定位块,对应另一端扩展定位槽设置,对应边榫槽与插榫的设置,桥式加强筋与支撑柱的设置,在专用模具中一次成型,制成一体结构。
2、保温材料填充:外墙保温装饰板的保温材料采用聚氨酯发泡材料,通过注射聚氨酯发泡工艺使保温材料与装饰板腔体严密结合,达到保温的最佳效果。
3、板面喷涂:
1)对步骤1制造的外墙保温装饰板模压型材外表面首先做打磨处理,使其表面的脱模剂完全去除。
2)喷涂底漆:然后把仿石漆通过喷枪均匀的喷射到以喷涂底漆的表面上,厚度要求:视喷涂漆料颗粒大小而定,要求在2-3mm,不能过厚,在喷涂表面直接用沾有面漆的圆棍在仿石漆涂层稍加力滚压,要求用力均匀。另外,可以根据不同需求做出不同仿石色彩和纹理效果。
4、干燥:干燥时间要求环境温度55-70度条件下,放置5-7小时左右,使其充分干燥。
5、表面后处理:对外墙保温装饰板表面的过于不平的表面进行后处理,获得成品装饰板。
采用本发明的积极效果是本制造工艺简便易行,制作成本低,工作效率高,所生产外墙保温装饰板重量轻,减轻了墙体承重,达到了坚实耐用,美观保温的最佳效果。
具体实施方式
以生产上面板为蘑菇形的外墙保温装饰板为例,其制造工艺包括以下具体步骤:
1、高分子树脂、玻璃纤维增强复合成型:外墙保温装饰板通过模具高温高压成型制作出墙板基材。其上面板的蘑菇状凹凸造型,装饰板一端定位块,对 应另一端扩展定位槽设置,对应边榫槽与插榫的设置,桥式加强筋与支撑柱的设置,制成一体结构,在专用模具中一次成型。
2、保温材料填充:外墙保温装饰板的保温材料采用聚氨酯发泡材料,通过注射聚氨酯发泡工艺使是填充材料与装饰板腔体严密结合,达到保温的最佳效果。
3、墙板喷涂:
1)对步骤1制造的外墙保温装饰板模压型材外表面首先做打磨处理,使其表面的脱模剂完全去除。
2)在处理后的模压型材表面喷涂底漆,然后把仿石漆通过喷枪均匀的喷射到以喷涂底漆的表面上,厚度要求:视喷涂漆料颗粒大小而定,要求在2-3mm,不能过厚,在喷涂表面直接用沾有面漆的圆棍在仿石漆涂层稍加力滚压,要求用力均匀。另外,可以根据不同需求做出不同仿石色彩和纹理效果。
4、干燥:干燥时间要求环境温度60度条件下,放置6小时左右,使其充分干燥。
5、表面后处理,对表面的过于不平的表面进行后处理,获得成品装饰板。
Claims (1)
1.一种外墙保温装饰板制造工艺,采用高分子树脂,玻璃纤维增强复合材料高温高压成型工艺,注射聚氨酯发泡工艺使保温材料与装饰板腔体严密结合,获得外墙保温装饰板有平面板、蘑菇面板、艺术造型板,其工艺步骤如下:
(1)高分子复合材料成型:外墙保温装饰板通过模具高温高压成型制作出墙板基材,其上面板的凹凸造型,装饰板一端定位块,对应另一端扩展定位槽设置,对应边榫槽与插榫的设置,桥式加强筋、与墙基锚固的支撑柱设置,为一体结构,均在专用模具中一次成型;
(2)保温材料填充:外墙保温装饰板的保温材料采用聚氨酯发泡材料,通过注射聚氨酯发泡工艺使保温材料与装饰板腔体严密结合,达到保温的最佳效果;
(3)板面喷涂:
1)对步骤1制造的外墙保温装饰板模压型材外表面首先做打磨处理,使其表面的脱模剂完全去除;
2)在处理后的模压型材表面喷涂底漆,然后把仿石漆通过喷枪均匀的喷射到已喷涂底漆的表面上,厚度要求:视喷涂漆料颗粒大小而定,要求在2-3mm,不能过厚,在喷涂表面直接用沾有面漆的圆棍在仿石漆涂层稍加力滚压,要求用力均匀,根据不同需求做出不同仿石色彩和纹理效果;
(4)干燥:干燥时间要求环境温度55-70度条件下,放置5-7小时,使其充分干燥;
(5)表面后处理:对表面的过于不平的表面进行后处理。