CN101786827A - 一种抗渗剂 - Google Patents
一种抗渗剂 Download PDFInfo
- Publication number
- CN101786827A CN101786827A CN201010107825A CN201010107825A CN101786827A CN 101786827 A CN101786827 A CN 101786827A CN 201010107825 A CN201010107825 A CN 201010107825A CN 201010107825 A CN201010107825 A CN 201010107825A CN 101786827 A CN101786827 A CN 101786827A
- Authority
- CN
- China
- Prior art keywords
- parts
- impervious
- impervious agent
- permeability agent
- acrylic resin
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种抗渗剂,各原料组分按重量份为:烧碱10-40、甲基硅酸15-45、改性丙烯酸树脂10-30、硅溶胶10-30、水20-50。本发明使建筑物不受风化或减少风化,延长建筑物的使用寿命,具有防水、憎水、耐候性强等优点。
Description
技术领域
本发明涉及建筑材料领域,具体是一种抗渗剂。
背景技术
抗渗剂主要应用于混凝土的防水抗渗、堵漏、密实等,提高混凝土的自防水和抗渗性能,是道路桥梁、地铁、隧道、海防坝的首选材料,抗渗剂综合当前国内外新型防水抗渗材料的全新技术,在原有聚合物混凝土砂浆防水抗渗剂的基础上进一步研制开发,并充分采用国外进口的高级脂肪酸和高分子材料,经过一系列的复杂化学反应过程,制成品质超前的高分子混凝土抗渗剂。
抗渗剂可代替水拌合混凝土或砂浆,在与混凝土或砂浆层反应过程中,其主要成分高分子化合物的原子连接成线形并带有较长分支部网状,抗渗剂一般都是呈现乱向分布的立体结构,密布于混凝土或砂浆层的高分子结构,并完全堵塞混凝土或砂浆的毛细通道,使水泥及水泥砂浆具有憎水性,提高混凝土的抗渗能力,增加其密实度和抗渗性。抗渗剂在加热时不能熔融,只能变软;不能在任何溶剂中溶解,只能微溶胀;所以能够有效弥补在施工过程中各种微小瑕疵。
发明内容
本发明提供了一种抗渗剂,使建筑物不受风化或减少风化,延长建筑物的使用寿命,具有防水、憎水、耐候性强等优点。
本发明的技术方案为:
一种抗渗剂,其特征在于:各原料组分按重量份为:烧碱10-40、甲基硅酸15-45、改性丙烯酸树脂10-30、硅溶胶10-30、水20-50。
所述的抗渗剂,其特征在于:所述的烧碱中氢氧化钠的质量分数为90%以上;所述的改性丙烯酸树脂选用BA-209系纯丙烯酸及官能单体共聚而成的乳液。
本发明集弹性和刚性为一体,渗透力强,可与水泥硅酸盐起反应,生成有机硅酸盐,不仅提高了密实度,堵塞毛细孔、而且能追踪细纹裂纹,从而达到污水的性能;本发明也可直接加入水泥砂浆中,增加水泥砂浆的强度,又避免了水泥砂浆的易开裂性,形成防水砂浆;本发明也可应用到涂料,使涂料具有防水、憎水的性能。
具体实施方式
(1)、一种抗渗剂,各原料组分按重量份为:烧碱10-40、甲基硅酸15-45、改性丙烯酸树脂10-30、硅溶胶10-30、水20-50;
烧碱中氢氧化钠的质量分数为90%以上;改性丙烯酸树脂选用BA-209系纯丙烯酸及官能单体共聚而成的乳液。
(2)、抗渗剂的制备方法:
在搅拌机内按重量份比加入50%的水,然后缓慢加入氢氧化钠、甲基硅酸进行反应,静止1小时后加入剩余50%的水、改性丙烯酸树脂和硅溶胶,搅拌25-35分钟后,得成品。
Claims (2)
1.一种抗渗剂,其特征在于:各原料组分按重量份为:烧碱10-40、甲基硅酸15-45、改性丙烯酸树脂10-30、硅溶胶10-30、水20-50。
2.根据权利要求1所述的抗渗剂,其特征在于:所述的烧碱中氢氧化钠的质量分数为90%以上;所述的改性丙烯酸树脂选用BA-209系纯丙烯酸及官能单体共聚而成的乳液。