CN101781537B - Eva鞋底粘合剂的制备方法 - Google Patents

Eva鞋底粘合剂的制备方法 Download PDF

Info

Publication number
CN101781537B
CN101781537B CN2010101229895A CN201010122989A CN101781537B CN 101781537 B CN101781537 B CN 101781537B CN 2010101229895 A CN2010101229895 A CN 2010101229895A CN 201010122989 A CN201010122989 A CN 201010122989A CN 101781537 B CN101781537 B CN 101781537B
Authority
CN
China
Prior art keywords
eva
add
chloroprene rubber
preparation
gram
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN2010101229895A
Other languages
English (en)
Other versions
CN101781537A (zh
Inventor
聂秋林
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NANTONG GUANGTAI BIOCHEMICAL PRODUCT Co Ltd
Original Assignee
Hangzhou Dianzi University
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by Hangzhou Dianzi University filed Critical Hangzhou Dianzi University
Priority to CN2010101229895A priority Critical patent/CN101781537B/zh
Publication of CN101781537A publication Critical patent/CN101781537A/zh
Application granted granted Critical
Publication of CN101781537B publication Critical patent/CN101781537B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及一种EVA鞋底粘合剂的制备方法。本发明方法首先将氯丁橡胶和氯化聚乙烯加入混合溶剂(组分为甲苯、乙酸乙酯、丁酮和丙酮)中搅拌,完全溶解后充入氮气,加入甲基丙烯酸甲酯和醋酸乙烯酯,升温至75~90℃后加入过氧化苯甲酰进行聚合反应;聚合反应2~3小时后,加入丙烯酸,继续反应1~2小时后关闭氮气,降温至30~50℃,然后加入2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。本发明方法制备的EVA鞋底粘合剂综合性能好、价格便宜、对EVA鞋底的粘接强度高。该方法工艺简单,可实现规模化生产。

Description

EVA鞋底粘合剂的制备方法
技术领域
本发明属于高分子材料技术领域,涉及一种胶粘剂的制备方法,具体是一种用于EVA鞋底粘合的胶粘剂的制备方法。
背景技术
目前制鞋行业大部分采用冷粘工艺,用于EVA(乙烯-醋酸乙烯酯共聚物)鞋底粘合的胶粘剂通常采用接枝氯丁胶粘剂。所谓接枝氯丁胶粘剂就是在一混合溶剂中,在引发剂的作用下,将活性单体连接在氯丁橡胶上。这样制成的接枝氯丁胶粘剂既有了骨架聚合物氯丁橡胶的内聚强度,又因活性单体的存在改善了界面性质,从而提高胶粘剂的粘合强度。由于接枝氯丁胶粘剂的广泛应用,人们在氯丁橡胶的接枝改性方面进行了大量研究并取得了进展。马小丽、杨性坤等制备了氯丁橡胶和甲基丙烯酸甲酯二元接枝氯丁胶粘剂[信阳师范学院学报(自然科学版)2005,18(4),446-448],谢纯等制备了氯丁橡胶、甲基丙烯酸甲酯和丙烯酸三元接枝氯丁胶[中国胶粘剂,1997,6(3):20-22],蒋遥明,程雁飞等研制了氯丁橡胶、丁苯橡胶、甲基丙烯酸甲酯和甲基丙烯酸正丁酯四元接技氯丁胶粘剂[粘接,1999,20(3):9-11],谭淑珍等研制了氯丁橡胶、甲基丙烯酸甲酯、甲基丙烯酸正丁酯和丙烯酸四元接技氯丁胶粘剂[精细石油化工,2001,5,37-39],夏门大学潘容华研制了带有第二活性单体组分的接枝氯丁胶[CN1006708B]。
发明内容
本发明的目的就是提供一种用于EVA鞋底粘合的胶粘剂的制备方法。
本发明采用如下技术方案:
将混合溶剂加入带有搅拌和回流装置的反应釜中,然后投入氯丁橡胶和氯化聚乙烯,进行搅拌,控制温度为50~70℃;待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入甲基丙烯酸甲酯和醋酸乙烯酯,升温至75~90℃后加入过氧化苯甲酰进行聚合反应;聚合反应2~3小时后,加入丙烯酸,继续反应1~2小时后关闭氮气,降温至30~50℃,然后加入2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。
以上各物质加入的重量份数为:
混合溶剂                1000~1400
氯丁橡胶                100
氯化聚乙烯              20~30
甲基丙烯酸甲酯          20~30
醋酸乙烯酯              20~30
过氧化苯甲酰            0.6~1.2
丙烯酸                  5~10
2,6一二叔丁基对甲酚    0.6~1.5
所述的混合溶剂的组分及各组分的重量百分比为:
甲苯                    20~50%
乙酸乙酯                10~30%
丁酮                    10~40%
丙酮                    10~30%
本发明的EVA鞋底粘合剂由氯丁橡胶、氯化聚乙烯、甲基丙烯酸甲酯、醋酸乙烯酯和丙烯酸在混合溶剂中进行五元接枝共聚而成。该胶粘剂中,组分氯化聚乙烯橡胶和醋酸乙烯酯活性单体对EVA材料亲合性好,适合EVA鞋底的粘接,价格也相应地较氯丁橡胶和丙烯酸酯类活性单体便宜。因此本发明方法制备的EVA鞋底粘合剂综合性能好、价格便宜、对EVA鞋底的粘接强度高。该方法工艺简单,可实现规模化生产。
具体实施方式
实施例1
将1400克混合溶剂(组分为甲苯50w%、乙酸乙酯10w%、丁酮10w%、丙酮30w%)加入带有搅拌和回流装置的反应釜中,然后投入100克氯丁橡胶和20克氯化聚乙烯,进行搅拌,控制温度为50℃。待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入20克甲基丙烯酸甲酯和20克醋酸乙烯酯,升温至75℃后加入1.2克过氧化苯甲酰进行聚合反应。聚合反应2小时后,再加入5克丙烯酸,继续反应1小时后关闭氮气,降温至30℃,然后加入0.6克2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。
实施例2
将1000克混合溶剂(组分为甲苯20w%、乙酸乙酯30w%、丁酮40w%、丙酮10w%)加入带有搅拌和回流装置的反应釜中,然后投入100克氯丁橡胶和30克氯化聚乙烯,进行搅拌,控制温度为70℃。待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入25克甲基丙烯酸甲酯和30克醋酸乙烯酯,升温至90℃后加入0.8克过氧化苯甲酰进行聚合反应。聚合反应3小时后,再加入10克丙烯酸,继续反应2小时后关闭氮气,降温至50℃,然后加入1.5克2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。
实施例3
将1200克混合溶剂(组分为甲苯35w%、乙酸乙酯25w%、丁酮20w%、丙酮20w%)加入带有搅拌和回流装置的反应釜中,然后投入100克氯丁橡胶和25克氯化聚乙烯,进行搅拌,控制温度为60℃。待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入30克甲基丙烯酸甲酯和25克醋酸乙烯酯,升温至80℃后加入1克过氧化苯甲酰进行聚合反应。聚合反应2.5小时后,再加入8克丙烯酸,继续反应1.5小时后关闭氮气,降温至40℃,然后加入1克2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。
实施例4
将1000克混合溶剂(组分为甲苯40w%、乙酸乙酯20w%、丁酮20w%、丙酮20w%)加入带有搅拌和回流装置的反应釜中,然后投入100克氯丁橡胶和30克氯化聚乙烯,进行搅拌,控制温度为65℃。待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入25克甲基丙烯酸甲酯和28克醋酸乙烯酯,升温至85℃后加入0.6克过氧化苯甲酰进行聚合反应。聚合反应3小时后,再加入7克丙烯酸,继续反应2小时后关闭氮气,降温至35℃,然后加入1.2克2,6一二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂。

Claims (1)

1.EVA鞋底粘合剂的制备方法,其特征在于该方法具体是:将混合溶剂加入带有搅拌和回流装置的反应釜中,然后投入氯丁橡胶和氯化聚乙烯,进行搅拌,控制温度为50~70℃;待氯丁橡胶和氯化聚乙烯完全溶解后向反应釜内充入氮气,加入甲基丙烯酸甲酯和醋酸乙烯酯,升温至75~90℃后加入过氧化苯甲酰进行聚合反应;聚合反应2~3小时后,加入丙烯酸,继续反应1~2小时后关闭氮气,降温至30~50℃,然后加入2,6-二叔丁基对甲酚,搅匀后出料,得到EVA鞋底粘合剂;
以上各物质加入的重量份数为:
混合溶剂               1000~1400
氯丁橡胶               100
氯化聚乙烯             20~30
甲基丙烯酸甲酯         20~30
醋酸乙烯酯             20~30
过氧化苯甲酰           0.6~1.2
丙烯酸                 5~10
2,6-二叔丁基对甲酚    0.6~1.5
所述的混合溶剂的组分及各组分的重量百分比为:
甲苯                   20~50%
乙酸乙酯               10~30%
丁酮                   10~40%
丙酮                   10~30%。
CN2010101229895A 2010-03-12 2010-03-12 Eva鞋底粘合剂的制备方法 Expired - Fee Related CN101781537B (zh)