CN101769681A - 加热炉水冷梁快速维修方法 - Google Patents
加热炉水冷梁快速维修方法 Download PDFInfo
- Publication number
- CN101769681A CN101769681A CN200810204884A CN200810204884A CN101769681A CN 101769681 A CN101769681 A CN 101769681A CN 200810204884 A CN200810204884 A CN 200810204884A CN 200810204884 A CN200810204884 A CN 200810204884A CN 101769681 A CN101769681 A CN 101769681A
- Authority
- CN
- China
- Prior art keywords
- water
- heating furnace
- maintenance method
- refractory
- quick maintenance
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明涉及加热炉维修,尤其涉及加热炉水冷梁的维修方法。一种加热炉水冷梁快速维修方法,所述维修方法包括如下步骤:拆除耐火材料的受损外层步骤、拆除受损的耐火陶瓷纤维步骤、拆除受损的Y型锚固件步骤、有选择性地更换内芯钢管步骤、更换损坏的Y型锚固件步骤、包裹耐火陶瓷纤维步骤、利用喷涂机向水冷梁喷涂耐火材料步骤、局部修整步骤和烘烤步骤。本发明充分利用喷涂工艺对耐火材料维修,不需要支模板,大大缩短施工时间,提高施工效率,减少对钢铁企业的影响。
Description
技术领域
本发明涉及加热炉维修,尤其涉及加热炉水冷梁的维修方法。
背景技术
加热炉是轧钢厂或锻钢厂用于加热钢坯或小型钢锭的热工设备,炉内耐火材料主要由炉顶、炉墙、炉底及水冷梁滑轨系统四部分组成,还有空气预热装置、烟道和烟囱等附属设施。推钢式或步进式加热炉水冷梁内芯一般为厚壁无缝钢管,钢管外表面支设Y型锚固件,钢管外覆盖一层陶瓷纤维,外层采用耐火浇注料浇注成型。
加热炉工作过程中,水冷梁外层耐火浇注料由于受机械振动、温度梯度大、急冷急热及长时间的热疲劳的影响,经常会出现开裂、剥落等现象,严重影响加热炉的正常工作,并给安全生产带来隐患。水冷梁柱的损坏是加热炉最常见最频繁的故障,故一般在加热炉年修或定修时都会对水冷梁柱钢管及其外层耐火材料进行维修。
传统的水冷梁柱的耐火外壁维修主要是采用浇注的方法,通常的工序如下:拆除受损的外层耐火材料→拆除受损的耐火陶瓷纤维→拆除受损的Y型锚固件→有选择性地更换内芯钢管→更换损坏的Y型锚固件→包裹耐火陶瓷纤维→支设外模→浇注成型→自然养生→脱模→局部修整→烘烤。由于该维修方法工序复杂,一般至少需要七天以上时间才能完成全部工作,维修周期特别受浇注料施工周期影响,浇注需要4-5天,且需支模板,操作不便,工作效率低下,严重影响了钢厂的经济效益。
发明内容
本发明旨在解决现有技术的缺陷,提供一种加热炉水冷梁快速维修方法。本发明充分利用喷涂工艺对耐火材料维修,不需要支模板,大大缩短施工时间,提高施工效率,减少对钢铁企业的影响。
本发明是这样实现的:一种加热炉水冷梁快速维修方法,其特征在于:所述发明方法包括如下步骤:拆除耐火材料的受损外层步骤、拆除受损的耐火陶瓷纤维步骤、拆除受损的Y型锚固件步骤、有选择性地更换内芯钢管步骤、更换损坏的Y型锚固件步骤、包裹耐火陶瓷纤维步骤、利用喷涂机向水冷梁喷涂耐火材料步骤、局部修整步骤和烘烤步骤。
所述的加热炉水冷梁快速维修方法,利用喷涂机向水冷梁喷涂耐火材料步骤,包括将喷涂料装入喷涂机内,通过料管,利用压缩空气将喷涂料吹至喷枪枪头,同时在枪头加入水,喷至加热炉的水冷梁柱。
所述的加热炉水冷梁快速维修方法,利用喷涂机向水冷梁喷涂耐火材料步骤中所述的加水量为8~10%。
所述的加热炉水冷梁快速维修方法,利用喷涂机向水冷梁喷涂耐火材料步骤中,喷涂距离为800~900mm,喷涂角度为80°~100°。
采用本发明的喷涂施工的方法,修复水冷梁外层耐火材料,仅用三天时间就能完成原来一周才能完成的工作,无需支模板,可以大大节省人力、物力,减少对钢铁企业的影响。
具体实施方式
一种加热炉水冷梁快速维修方法,所述维修方法包括如下步骤:拆除耐火材料的受损外层步骤、拆除受损的耐火陶瓷纤维步骤、拆除受损的Y型锚固件步骤、有选择性地更换内芯钢管步骤、更换损坏的Y型锚固件步骤、包裹耐火陶瓷纤维步骤、利用喷涂机向水冷梁喷涂耐火材料步骤、局部修整步骤和烘烤步骤。
所述的加热炉水冷梁快速维修方法:所述利用喷涂机向水冷梁喷涂耐火材料步骤,包括将喷涂料装入喷涂机内,通过料管,利用压缩空气将喷涂料吹至喷枪枪头,同时在枪头加入水,喷至加热炉的水冷梁柱。所述的加水量为8~10%,喷涂距离800~900mm,喷涂角度为80°~100°。
Claims (4)
1.一种加热炉水冷梁快速维修方法,其特征在于:所述维修方法包括如下步骤:拆除耐火材料的受损外层步骤、拆除受损的耐火陶瓷纤维步骤、拆除受损的Y型锚固件步骤、有选择性地更换内芯钢管步骤、更换损坏的Y型锚固件步骤、包裹耐火陶瓷纤维步骤、利用喷涂机向水冷梁喷涂耐火材料步骤、局部修整步骤和烘烤步骤。
2.根据权利要求1所述的加热炉水冷梁快速维修方法,其特征在于:所述利用喷涂机向水冷梁喷涂耐火材料步骤,包括将喷涂料装入喷涂机内,通过料管,利用压缩空气将喷涂料吹至喷枪枪头,同时在枪头加入水,喷至加热炉的水冷梁柱。
3.根据权利要求2所述的加热炉水冷梁快速维修方法,其特征在于:所述利用喷涂机向水冷梁喷涂耐火材料步骤中所述的加水量为8~10%。
4.根据权利要求1或2所述的加热炉水冷梁快速维修方法,其特征在于:所述利用喷涂机向水冷梁喷涂耐火材料步骤中,喷涂距离为800~900mm,喷涂角度为80°~100°。