CN101760013A - 无卤玻纤增强尼龙6材料及其制作工艺 - Google Patents

无卤玻纤增强尼龙6材料及其制作工艺 Download PDF

Info

Publication number
CN101760013A
CN101760013A CN200910212426A CN200910212426A CN101760013A CN 101760013 A CN101760013 A CN 101760013A CN 200910212426 A CN200910212426 A CN 200910212426A CN 200910212426 A CN200910212426 A CN 200910212426A CN 101760013 A CN101760013 A CN 101760013A
Authority
CN
China
Prior art keywords
glass fiber
free glass
halogen
nylon
fiber reinforced
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN200910212426A
Other languages
English (en)
Inventor
孙平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU CITY KECHUANG POLYMER CO Ltd
Original Assignee
SUZHOU CITY KECHUANG POLYMER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU CITY KECHUANG POLYMER CO Ltd filed Critical SUZHOU CITY KECHUANG POLYMER CO Ltd
Priority to CN200910212426A priority Critical patent/CN101760013A/zh
Publication of CN101760013A publication Critical patent/CN101760013A/zh
Pending legal-status Critical Current

Abstract

本发明涉及一种有机高分子复合材料,更具体地说,是涉及一种无卤玻纤增强尼龙6材料及其制备方法,是由以下成分按重量比组成,尼龙6:38.5-95%,无碱玻纤:5-60%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0,其他助剂:1.3-5.5,本发明的一种无卤玻纤增强尼龙6材料,性能与未改良的同类材料相比,冲击较高,脆性不明显,尤其是在零下低温环境时,克服了同类材料偏脆的缺点,并且生产采购方便,同时也符合其它所有的环保要求,这样全面提高了产品竞争力。

Description

无卤玻纤增强尼龙6材料及其制作工艺
技术领域
本发明涉及一种有机高分子复合材料,更具体地说,是涉及一种无卤玻纤增强尼龙6材料及其制备方法。
背景技术
目前,国际上用塑料替代天然材料的应用不断扩大,世界各地的科学家通过各种试验,积极寻找新的高性能热塑性塑料来替代金属与木材,而这也成为企业争取更多户和扩大市场份额的重要组成部分。
高温塑料的发展使工农业和民用设施更加的微型化轻量化和动力强劲化成为可能。耐高温塑料可以为某些部件带来更高的耐温性能,或是干脆替代了金属原材料来生产这些部件。新型设备的装置和组件同样也有用耐高温塑料代替金属和热固性材料的趋势。这些都将会加大对耐高温塑料材料的需求量,从而带动市场需求。
这些耐高温塑料材料可以耐180℃的持续高温,并且还能保持良好的尺寸稳定性。具有优异的长期和短期热性能,可以耐受无铅焊接过程中使用的红外(IR)回流炉所产生的高温,并在潮湿环境下提供相同的强度,卓越的耐化学性。
但是,目前市场中所有种类的耐高温塑料材料都有一个共同的缺点:冲击较低,脆性明显,尤其是在零下低温环境时,更加偏脆。这个缺点较大限制了高温塑料替代金属和木材的应用范围。而这些正是本发明要解决的问题。
本发明的系列产品充分符合欧盟“废旧电子电气设备”(WEEE)和“有害物质限用指令”(RoHS)法规及其他环保规定,对环保要求严格的应用领域都能使用。
发明内容
本发明的目的在于有效的克服了现有技术的缺陷,提供一种改良型的无卤玻纤增强尼龙6材料。
本发明提供的技术方案如下:无卤玻纤增强尼龙6材料,是由以下成分按重量比组成,尼龙6:38.5-95%,无碱玻纤:5-60%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0,其他助剂:1.3-5.5。
本发明所述的无卤玻纤增强尼龙6材料的制备方法,包括如下步骤:先将尼龙6、环保玻纤、热稳定剂、玻纤处理剂、其他助剂按照比例称量后在混料机中低速混合10分钟,自然放置12小时后再经双螺杆挤出机在中等强度剪切的螺杆组合情况下由侧面加入环保玻纤进行混炼挤出,水冷拉条切粒再经过筛分脱水制得一种无卤玻纤增强尼龙6材料。
本发明有效的克服了现有尼龙材料的缺陷,具有以下优点:
本发明的一种无卤玻纤增强尼龙6材料,性能与未改良的同类材料相比,冲击较高,脆性不明显,尤其是在零下低温环境时,克服了同类材料偏脆的缺点,并且生产采购方便,同时也符合其它所有的环保要求,这样全面提高了产品竞争力。
具体实施方式
以下是本发明所述的无卤玻纤增强尼龙6原料的实施例,并不因此限定本发明的保护范围。
实施例一,提供一种无卤玻纤增强尼龙6原料,由以下成分按重量比组成,尼龙6:65%,环保玻纤:30%;热稳定剂:1.5%,玻纤处理剂:1.0%,其他助剂:2.5%;
先将尼龙6、热稳定剂、玻纤处理剂、其他助剂按照比例称量后在混料机中低速混合10分钟,混料机采用低速混合,不锈钢材质,搅拌叶应与筒壁间隙小于0.5厘米,原辅料混合效果应目视各种粒子和粉末基本均匀,没有明显团块或集聚,然后自然放置12小时使其反应充分后再使用;双螺杆挤出机使用36长径比,中等强度剪切;环保玻纤由侧面按比例加入;保持真空状态和270度条件混炼挤出;采用水冷拉条切粒方式,经过筛分脱水即制得无卤玻纤增强尼龙6材料。

Claims (2)

1.一种无卤玻纤增强尼龙6材料,其特征在于:是由以下成分按重量比组成,尼龙6:38.5-95%,无碱玻纤:5-60%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0,其他助剂:1.3-5.5。
2.一种制备无卤玻纤增强尼龙6材料的方法,其特征在于:包括如下步骤:先将尼龙6、环保玻纤、热稳定剂、玻纤处理剂、其他助剂按照比例称量后在混料机中低速混合10分钟,自然放置12小时后再经双螺杆挤出机在中等强度剪切的螺杆组合情况下由侧面加入环保玻纤进行混炼挤出,水冷拉条切粒再经过筛分脱水制得一种无卤玻纤增强尼龙6材料。
CN200910212426A 2009-11-03 2009-11-03 无卤玻纤增强尼龙6材料及其制作工艺 Pending CN101760013A (zh)