Prior art keywords
temperature nylon
temperature
fiber
glass
nylon
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Pending
Application number
CN200910212445A
Other languages
English (en)
Inventor
孙平
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
SUZHOU CITY KECHUANG POLYMER CO Ltd
Original Assignee
SUZHOU CITY KECHUANG POLYMER CO Ltd
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by SUZHOU CITY KECHUANG POLYMER CO Ltd filed Critical SUZHOU CITY KECHUANG POLYMER CO Ltd
Priority to CN200910212445A priority Critical patent/CN101760006A/zh
Publication of CN101760006A publication Critical patent/CN101760006A/zh
Pending legal-status Critical Current

Links

Landscapes

  • Compositions Of Macromolecular Compounds (AREA)
  • Reinforced Plastic Materials (AREA)

Abstract

本发明涉及一种有机高分子复合材料,更具体地说,是涉及一种不露纤的玻纤增强高温尼龙及其制备方法,是由以下成分按重量比组成,高温尼龙:45.5-95%,无碱玻纤:5-55%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0%,其他助剂:1.3-5.5%,本发明的一种不露纤的玻纤增强高温尼龙及其制作工艺,具有优异的长期和短期热性能,耐高温,具有优异的机械强度,并在潮湿环境下提供相同的强度和韧性,卓越的耐化学性,尺寸稳定性,优异的电特性以及良好的外观。

Description

不露纤的玻纤增强高温尼龙及其制作工艺
技术领域
本发明涉及一种有机高分子复合材料,更具体地说,是涉及一种不露纤的玻纤增强高温尼龙原料。本发明还涉及制作这种高温尼龙原料的方法
背景技术
目前,国际上用塑料替代工业中金属的应用不断扩大,增强高温尼龙的发展使此速度和范围更加广泛。耐高温尼龙可以为很多部件带来更高的耐温性能。这种材料可以耐180℃的持续高温,并且还能保持良好的尺寸稳定性。具有优异的长期和短期热性能,可以耐受无铅焊接过程中使用的红外(IR)回流炉所产生的高温,具有优异的机械强度,并在潮湿环境下提供相同的强度和韧性,卓越的耐化学性,尺寸稳定性,优异的电特性,良好的外观。
新设计发明的许多电机和会发热部件的罩壳组件同样也有用耐高温尼龙代替金属和热固性材料的趋势。这些都将会加大对这种耐高温尼龙材料的需求量,从而带动尼龙市场需求。但是暴露在外面的看得见的部件比隐蔽在里面的部件又多了一个很难达到的要求,那就是外观美观------要求在耐受高温以及高强度的同时,外观上没有瑕疵。
该系列产品市场目前基本还是空白,这些正是本发明要解决的问题。
本发明的系列产品充分符合欧盟“废旧电子电气设备”(WEEE)和“有害物质限用指令”(RoHS)法规及其他环保规定,要求严格的应用领域都能使用。
发明内容
本发明的目的在于有效的克服了现有耐高温尼龙的缺陷,提供一种外观与未改良同类差不多但性能可比改良后的同类材料的不露纤的玻纤增强绿色环保高温尼龙原料。
本发明提供的技术方案如下:高温尼龙:45.5-95%,无碱玻纤:5-55%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0%,其他助剂:1.3-5.5%;
本发明所述的不露纤的玻纤增强高温尼龙的制备方法,包括如下步骤:先将高温尼龙粒子用100度的温度烘烤3-4小时,然后及时与玻纤处理剂按比例混合,50度恒温放置12小时后再与热稳定剂、、成核剂、其他助剂按照比例称量后在混料机中低速混合10分钟,经双螺杆挤出机在中等强度剪切的螺杆组合情况下由侧面按比例加入无碱玻纤,在真空状态下,用340度混炼挤出,水冷拉条切粒经过筛分脱水制得不露纤的玻纤增强绿色环保高温尼龙材料。
本发明有效的克服了现有耐高温尼龙的缺陷,具有以下优点:
本发明一种不露纤的玻纤增强高温尼龙具有优异的长期和短期热性能,可以耐受无铅焊接过程中使用的红外(IR)回流炉所产生的高温,具有优异的机械强度,并在潮湿环境下提供相同的强度和韧性,卓越的耐化学性,尺寸稳定性,优异的电特性以及良好的外观,并且生产采购方便,改变了用户设计产品时性能与外观二者只能选其一的状况,同时也符合所有的环保要求,这样全面提高了产品竞争力。
具体实施方式
以下是本发明所述的不露纤的玻纤增强高温尼龙的实施例,并不因此限定本发明的保护范围。
实施例一,提供一种不露纤的玻纤增强高温尼龙原料,由以下成分按重量比组成,高温尼龙:65%,无碱玻纤:30%;热稳定剂:0.8%,玻纤处理剂:1.0%,染料色粉:0.7%,其他助剂:2.5%;
先将高温尼龙粒子用100度的温度烘烤3-4小时,然后与玻纤处理剂按比例混合后在50度恒温条件下放置12小时,再及时与热稳定剂、、染料色粉及其他助剂按照比例称量后在混料机中低速混合10分钟,混料机采用低速混合,不锈钢材质,搅拌叶应与筒壁间隙小于0.5厘米,原辅料混合效果应目视各种粒子和粉末基本均匀,没有明显团块或集聚,然后及时进行混炼挤出;双螺杆挤出机使用积木式平行同向,40长径比,中等强度剪切;无卤无碱玻纤由侧面按比例加入;保持真空状态和340度条件混炼挤出;采用水冷拉条切粒方式,经过筛分脱水即制得不露纤的玻纤增强高温尼龙材料。

Claims (2)

1.一种不露纤的玻纤增强高温尼龙,其特征在于:是由以下成分按重量比组成,高温尼龙:45.5-95%,无碱玻纤:5-55%;热稳定剂:0.1-3.0%,玻纤处理剂:0.1-3.0%,其他助剂:1.3-5.5%。
2.一种制备不露纤的玻纤增强高温尼龙的方法,其特征在于:包括如下步骤:先将高温尼龙粒子用100度的温度烘烤3-4小时,然后与玻纤处理剂按比例混合后在50度恒温条件下放置12小时,再及时与成核剂、热稳定剂、其他助剂按照比例称量后在混料机中低速混合10分钟,再及时经双螺杆挤出机在中等强度剪切的螺杆组合情况下由侧面加入无卤无碱玻纤进行混炼挤出,水冷拉条切粒再经过筛分脱水制得一种不露纤的玻纤增强高温尼龙材料。
CN200910212445A 2009-11-03 2009-11-03 不露纤的玻纤增强高温尼龙及其制作工艺 Pending CN101760006A (zh)

Priority Applications (1)

Application Number Priority Date Filing Date Title
CN200910212445A CN101760006A (zh) 2009-11-03 2009-11-03 不露纤的玻纤增强高温尼龙及其制作工艺

Applications Claiming Priority (1)

Application Number Priority Date Filing Date Title
CN200910212445A CN101760006A (zh) 2009-11-03 2009-11-03 不露纤的玻纤增强高温尼龙及其制作工艺

Publications (1)

Publication Number Publication Date
CN101760006A true CN101760006A (zh) 2010-06-30

Family

ID=42491392

Family Applications (1)

Application Number Title Priority Date Filing Date
CN200910212445A Pending CN101760006A (zh) 2009-11-03 2009-11-03 不露纤的玻纤增强高温尼龙及其制作工艺

Country Status (1)

Country Link
CN (1) CN101760006A (zh)

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102888093A (zh) * 2012-11-05 2013-01-23 科创聚合物(苏州)有限公司 不露纤的玻纤增强高温尼原料及其制作工艺
CN102888108A (zh) * 2012-11-05 2013-01-23 科创聚合物(苏州)有限公司 不露纤的玻纤有机增强尼龙66制作工艺

Cited By (2)

* Cited by examiner, † Cited by third party
Publication number Priority date Publication date Assignee Title
CN102888093A (zh) * 2012-11-05 2013-01-23 科创聚合物(苏州)有限公司 不露纤的玻纤增强高温尼原料及其制作工艺
CN102888108A (zh) * 2012-11-05 2013-01-23 科创聚合物(苏州)有限公司 不露纤的玻纤有机增强尼龙66制作工艺

Similar Documents

Publication Publication Date Title
CN101831136A (zh) 一种高强度高韧性阻燃abs复合材料及其制备方法
CN105348796A (zh) 碳纤维增强聚苯硫醚复合材料及其制备方法
CN108102311A (zh) 一种低介电pbt/petg合金纳米注塑复合材料及其制备方法和应用
CN101760006A (zh) 不露纤的玻纤增强高温尼龙及其制作工艺
CN103333474B (zh) 一种高性能抗静电pc/abs合金及其制备方法和应用
CN101704996A (zh) 无卤高光泽防翘曲变形填充高温尼龙及其制作工艺
CN101760013A (zh) 无卤玻纤增强尼龙6材料及其制作工艺
CN101709145A (zh) 无卤玻纤增强尼龙66材料及其制作工艺
CN101654552A (zh) 无卤增强高温尼龙及其制作工艺
CN101760024A (zh) 高光洁耐乙二醇复合增强尼龙66及其制作工艺
CN102888093A (zh) 不露纤的玻纤增强高温尼原料及其制作工艺
CN101704997A (zh) 无卤防翘曲变形增强高温尼龙及其制作工艺
CN101709144A (zh) 无卤高温尼龙及其制作工艺
CN101654553A (zh) 无卤阻燃增强绿色环保高温尼龙及其制作工艺
CN101724262A (zh) 无卤增强尼龙及其制作工艺
CN101955651A (zh) 绿色环保耐寒柔性耐高温尼龙材料
CN101955637A (zh) 不露纤的玻纤增强绿色环保pbt材料
CN101974223A (zh) 风叶专用增强尼龙材料
CN102964811A (zh) 高光泽阻燃高温尼龙及其制作工艺
CN101717576A (zh) 自润滑耐磨注塑级石墨填充高温尼龙及其制作工艺
CN101717574A (zh) 无卤尼龙及其制作工艺
CN101717575A (zh) 环保耐寒增韧高温尼龙材料及其制作工艺
CN101792594A (zh) 自润滑耐磨注塑级二硫化钼填充高温尼龙及其制作工艺
CN101760007A (zh) 无卤防翘曲变形高光泽阻燃高温尼龙及其制作工艺
CN102898821A (zh) 注塑级石墨填充高温尼龙及其制作工艺

Legal Events

Date Code Title Description
C06 Publication
PB01 Publication
C10 Entry into substantive examination
SE01 Entry into force of request for substantive examination
C02 Deemed withdrawal of patent application after publication (patent law 2001)
WD01 Invention patent application deemed withdrawn after publication

Open date: 20100630