CN101759392A - 水泥砂浆塑化粉 - Google Patents
水泥砂浆塑化粉 Download PDFInfo
- Publication number
- CN101759392A CN101759392A CN200910227543A CN200910227543A CN101759392A CN 101759392 A CN101759392 A CN 101759392A CN 200910227543 A CN200910227543 A CN 200910227543A CN 200910227543 A CN200910227543 A CN 200910227543A CN 101759392 A CN101759392 A CN 101759392A
- Authority
- CN
- China
- Prior art keywords
- parts
- cement mortar
- powder
- mortar
- present
- Prior art date
- Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
- Pending
Abstract
本发明公开了一种水泥砂浆塑化粉,由如下原料混配而成:按重量份计,970份高岭土粉,15份AOS,3份HPMC,两份CMS,10份木钠;具有减水、引气、增稠、保水、增塑功能,加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度。
Description
技术领域
本发明涉及建筑材料技术领域,尤其是涉及一种水泥砂浆塑化粉。
背景技术
随着石灰石资源的短缺和烧制石灰企业的减少,建筑行业使用的混和砂浆逐渐被水泥砂浆所取代。为了提高砂浆的稠度、保水率和工作度,社会上流传使用一种叫微沫剂的产品。微沫剂是一种水性物质,加入水泥量的万分之几,其使用很不好掌握且性能受到局限,重大建筑早已禁止使用。
发明内容
有鉴于此,本发明的目的在于提供一种水泥砂浆塑化粉,具有减水、引气、增稠、保水、增塑功能,加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度。
为达到上述目的,本发明采用以下技术方案:
由如下原料混配而成:按重量份计,970份高岭土粉,15份AOS,3份HPMC,两份CMS,10份木钠。
本发明的有益效果是:
本发明利用微晶高岭土粉作载体,加入一种表面活性剂和保水剂,制造出一种各项性能优越的砂浆塑化粉。本发明选择的高岭土是一种特殊的微晶高岭土磨制的矿粉,具有遇水水化的性能,可以保水增稠、可以增加砂浆强度;选择的表面活性剂为新型阴离子表面活性剂,名称:AOS(α-烯基磺酸钠);选择的保水助剂为HPMC(羟丙级甲级纤维素)和CMS(羧甲基淀粉醚);木钠为一般减水剂,具有减水增稠功能。
本发明的其他优点、目标和特征在某种程度上将在随后的说明书中进行阐述,并且在某种程度上,基于对下文的考察研究对本领域技术人员而言将是显而易见的,或者可以从本发明的实践中得到教导。
具体实施方式
下面结合实施例对本发明作进一步描述。
本实施例的水泥砂浆塑化粉制作简单,生产只用一台粉体混合机,即可生产出合格的产品。本实施例的水泥砂浆塑化粉由如下原料混配而成:按重量份计,970份高岭土粉,15份AOS,3份HPMC,两份CMS,10份木钠。将原料分别称重计量,计量误差不超过±1%,然后投入粉体混合机中混合均匀即成。大量试验表明本实施例的水泥砂浆塑化粉可完全替代建筑砂浆所用石灰膏,具有减水、引气、增稠、保水、增塑功能,加入水泥砂浆中可减少泌水率、提高和易性、增加抗渗性和砂浆强度。具体讲本发明的产品具有如下优点:
1.产品形状:在水中不产生盐析与凝聚,掺入本塑化粉的水泥砂浆具有很好的保水性,可有效防止泌水离析并提高砂浆和易性及工作度。
2.物理指标:含水率<5%;10%水溶液起泡高度大于50mm;稳定时间大于2小时;
3.使用性能:本发明产品掺入水泥量的1%,比之同标号、同灰砂比的水泥砂浆,含气量大于3-5%;凝结时间之差,±90分钟;抗压强度比,28天强度大于或等于100%;泌水率比<50%。
4.本发明的产品可替代水泥砂浆常用的石灰膏和微沫剂,使用方便,容易掌握且节约成本。
Claims (1)
1.水泥砂浆塑化粉,其特征在于,由如下原料混配而成:按重量份计,970份高岭土粉,15份AOS,3份HPMC,两份CMS,10份木钠。