CN101710535B - 电抗器用磁环的制备方法 - Google Patents

电抗器用磁环的制备方法 Download PDF

Info

Publication number
CN101710535B
CN101710535B CN200910117722A CN200910117722A CN101710535B CN 101710535 B CN101710535 B CN 101710535B CN 200910117722 A CN200910117722 A CN 200910117722A CN 200910117722 A CN200910117722 A CN 200910117722A CN 101710535 B CN101710535 B CN 101710535B
Authority
CN
China
Prior art keywords
reactor
magnetic ring
ring
mixture
semi
Prior art date
Legal status (The legal status is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the status listed.)
Expired - Fee Related
Application number
CN200910117722A
Other languages
English (en)
Other versions
CN101710535A (zh
Inventor
焦海波
Current Assignee (The listed assignees may be inaccurate. Google has not performed a legal analysis and makes no representation or warranty as to the accuracy of the list.)
NINGXIA YINLI ELECTRICAL CO., LTD.
Original Assignee
焦海波
Priority date (The priority date is an assumption and is not a legal conclusion. Google has not performed a legal analysis and makes no representation as to the accuracy of the date listed.)
Filing date
Publication date
Application filed by 焦海波 filed Critical 焦海波
Priority to CN200910117722A priority Critical patent/CN101710535B/zh
Publication of CN101710535A publication Critical patent/CN101710535A/zh
Application granted granted Critical
Publication of CN101710535B publication Critical patent/CN101710535B/zh
Expired - Fee Related legal-status Critical Current
Anticipated expiration legal-status Critical

Abstract

本发明涉及电抗器,尤其是电抗器用磁环的制备方法,其特点是,包括如下步骤:a、将软磁粉未与环氧树脂胶按4∶1的重量比混合成混合物;b、将混合物搅拌均匀;c、将搅拌均匀的混合物放入成型模具中,在压力机上压制成型;d、将成型后的磁环(1)连同成型模具一起放入烘箱,在温度120-130℃下连续烘干3-4小时,然后控制温度在1-1.5小时内均匀下降至常温;e、取出磁环(1)后脱模即可。本发明方法处理后,磁环的表面光滑、无气泡、可减少磁环的破裂,该磁环应用在电抗器上,可提高电抗器的铁心抗饱性能,增强屏蔽,从而符合技术指标的要求,提高电抗器的使用性能。

Description

电抗器用磁环的制备方法
技术领域
本发明涉及电抗器,尤其是电抗器用磁环的制备方法。
背景技术
随着经济的发展,电抗器在各个领域的应用已日趋广泛,电抗器具有滤波、整流、保护电路等作用,它能够维护电路正常稳定的工作。尤其是一些有特殊用途的电抗器对磁导率、屏蔽、抗铁心饱和都有较高的技术要求。为了避免铁心饱和,需要在铁心上开气隙,而气隙附近会有磁场扩散现象,扩散的磁场会产生附加的损耗,特别是在单个气隙尺寸较大的时候,会在气隙附近的铁心和绕组上产生非常严重的附加损耗。如果不加限制,这种附加损耗会使得电抗器的损耗增加一倍以上。为了减少这种不必要的附加损耗,在制造工艺上往往需要增加气隙的数量,减小单个气隙的尺寸,这样就会影响电抗器的外形。
发明内容
本发明的目的是提供一种电抗器用磁环的制备方法,带有该磁环的电抗器屏蔽作用良好、抗铁心饱和,并且具有较低的磁导率。
为实现上述目的,本发明采用的技术方案是:
一种电抗器用磁环的制备方法,其特别之处在于,包括如下步骤:
a、将软磁粉末与环氧树脂胶按4︰1的重量比混合成混合物;
b、将混合物搅拌均匀;
c、将搅拌均匀的混合物放入成型模具中,在压力机上压制成型;
d、将成型后的磁环连同成型模具一起放入烘箱,在温度120-130℃下连续烘干3-4小时,然后控制温度在1-1.5小时内均匀下降至常温;
e、取出磁环后脱模即可。
其中步骤a中软磁粉末为粒度20-40 μm的铁氧体粉末或粒度20-40μm的铁硅铝粉末。
步骤b中将混合物放入搅拌机搅拌30-35分钟。
本发明方法是为特殊用途的电抗器提供一种新型磁环的制作工艺,不仅能够克服电抗器制作过程中存在的技术缺陷,而且对电抗器有良好的屏蔽作用、抗铁心饱和及较低的磁导率。经实验证明,用本方法处理后,磁环的表面光滑、无气泡、可减少磁环的破裂,该磁环应用在电抗器上,可提高电抗器的铁心抗饱性能,增强屏蔽,从而符合技术指标的要求,提高电抗器的使用性能。
附图说明
附图l为本发明方法制备的磁环(1)(半个)的结构示意图;
附图2为带有磁环(1)的电抗器。
具体实施方式
如图l、2所示,带有磁环l的电抗器,包括由绕组2和铁心3组成的本体,以及安装在本体上的接线端子4,在本体外套装有磁环l,该磁环l由两个相同的半环组成,每个半环均为只有一端封闭的管状,该两个半环分别与铁心3的两端接触。另外在每个半环上均开有供接线端子4伸出的槽,每个半环的侧面和底面相交处均倒角。
实施例l
a、将粒度20μm的铁氧体粉末与环氧树脂胶(具体选用天津继泰亿丰公司,型号TJH-5217A)按4︰1的重量比混合成混合物;
b、将混合物放入搅拌机搅拌32分钟以搅拌均匀;
c、将搅拌均匀的混合物放入成型模具中,在压力机上压制成型;
d、将成型后的磁环(1)连同成型模具一起放入烘箱,在温度125℃下连续烘干3.5小时,然后控制温度在1.2小时内均匀下降至常温;
e、取出磁环(1)后脱模即可。
实施例2
a、将粒度30μm的铁硅铝粉末与环氧树脂胶(具体选用天津继泰亿丰公司,型号TJH-5217A)按4︰1的重量比混合成混合物;
b、将混合物放入搅拌机搅拌30分钟以搅拌均匀;
c、将搅拌均匀的混合物放入成型模具中,在压力机上压制成型;
d、将成型后的磁环(1)连同成型模具一起放入烘箱,在温度120℃下连续烘干3小时,然后控制温度在1.5小时内均匀下降至常温;
e、取出磁环(1)后脱模即可。

Claims (2)

1.一种电抗器用磁环的制备方法,其特征在于,所述的磁环(1)由两个相同的半环组成,每个半环均为只有一端封闭的管状,每个半环上均开有供接线端子(4)伸出的槽,每个半环的侧面和底面相交处均倒角;
采用如下步骤制备:
a、将软磁粉末与环氧树脂胶按4∶1的重量比混合成混合物;
b、将混合物搅拌均匀;
c、将搅拌均匀的混合物放入成型模具中,在压力机上压制成型;
d、将成型后的磁环(1)连同成型模具一起放入烘箱,在温度120-130℃下连续烘干3-4小时,然后控制温度在1-1.5小时内均匀下降至常温;
e、取出磁环(1)后脱模即可;
其中步骤a中软磁粉末为粒度20-40μm的铁氧体粉末或粒度20-40μm铁硅铝粉末。
2.如权利要求1所述的电抗器用磁环的制备方法,其特征在于:
步骤b中将混合物放入搅拌机搅拌30-35分钟。
CN200910117722A 2009-12-15 2009-12-15 电抗器用磁环的制备方法 Expired - Fee Related CN101710535B (zh)